Painting & Coating Industry (PCI) logo Powder coating summit logo
search
cart
facebook twitter linkedin youtube
  • Sign In
  • Create Account
  • Sign Out
  • My Account
Painting & Coating Industry (PCI) logo Powder coating summit logo
  • NEWS
    • Latest News
    • Market Trends & Reports
    • Finishing News
    • Price Alerts
    • Subscribe to Newsletters
    • Global Top 10/ PCI 25
    • Weekly Featured Article
    • COATLE Word Game
  • PRODUCTS
    • Product News
    • Featured Products
    • Must See Products and Services
  • MATERIALS
    • Additives
    • Resins/Polymers
    • Pigments
    • Equipment
    • Distributors
  • TECHNOLOGIES
    • Adhesives
    • Architectural Coatings
    • Finishing Articles
    • Finishing Technologies
    • Finishing Equipment
    • Industrial Coatings
    • Nanotechnology
    • Powder Coatings
    • Solventborne
    • Special Purpose Coatings
    • Sustainability
    • UV Coatings
    • Waterborne
  • RESOURCES
    • Columns
      • Did you know?
      • Distribution Dive
      • Formulating With Mike
      • Innovation Insights
      • Powder Coating Perspectives
      • TiO2 Insider
    • Blogs
      • Editor's Viewpoint
      • Industry Insights
    • Coatings Supplier Handbook
    • Podcasts and Videos
      • COAT-IT! Podcast
      • Videos/PCI TV
    • PCI Store
    • Classifieds
    • eBooks
    • Sponsor Insights
    • White Papers
    • COATLE Word Game
  • EVENTS
    • Coatings Trends & Technologies Summit
    • Paint and Coatings Academy
    • Webinars
    • Calendar of Events
    • Lifetime Achievement Award
  • DIRECTORIES
    • Buyer's Guide
    • Equipment Directory
    • Materials Directory
  • EMAGAZINE
    • Current Issue
    • eMagazine Archive
    • China Issue Archive
    • Editorial Advisory Board
  • CONTACT
    • Contact Us
    • Advertise
    • Subscribe to eMagazine
    • Subscribe to Newsletters
  • SIGN UP!
Home » Topics » Featured Stories

Featured Stories
Featured Stories RSS Feed RSS

akzonobel

AkzoNobel Discusses Environment-Friendly Technologies and Sustainability

April 1, 2015
No Comments

Reducing energy and waste across the value chain, together with limiting raw material usage in coating formulas will become increasingly important aspects of product formulation strategies as materials become scarcer.


Read More
taminco

Waterborne Polyurethane Dispersions with New Sustainable Solvent

Mike Schmidt
April 1, 2015
No Comments

This new product is an innovative, next-generation sustainable solvent with excellent performance in a wide variety of waterborne PUD applications.


Read More
dow feature

An Exclusive Look Inside DCM’s Lab

Kristin Johansson
April 1, 2015
No Comments

A variety of technologies are under development, including waterborne polyolefin and alkyd dispersions, acrylic coatings for metal, isocyanate-free polyurethane coatings and BPA-free can coatings.


Read More

The Next Step in Wood Coatings

Silane/Urethane-Hybrid Crosslinkers for Multifunctional, Scratch-Resistant Coatings
March 1, 2015
No Comments

The VESTANAT EP-M range is a family of silane/urethane- hybrid crosslinkers that generates multifunctional, scratch-resistant coatings applicable on a variety of substrates.


Read More
lubrizol

Next-Generation Matting Agents for UV Coatings

March 1, 2015
No Comments

The alternative matting agents discussed in this article offer a first step to developing new ways of controlling the light scattering properties of radiation-curable coatings.


Read More
allnex

Color-Changing Resin Technology

March 1, 2015
No Comments

These new blue-colored resins have been designed with input from formulators, equipment manufacturers and coating applicators, and as a result meet the needs of this sector for increased ease of application combined with high-performance properties.


Read More
basf

Waterborne UVA/HALS Blend

for High-Performance Clear and Pigmented Coatings
March 1, 2015
3 Comments

A novel water-dispersible blend combining a high-performance UV absorber with a non-reacting HALS was designed to fulfill the requirements for long-term weather resistance in exterior deco, decking and joinery markets.


Read More
dow chemical

Spray Urethane Coatings

with Hydrophobic Polyols
March 1, 2015
No Comments

VORASTAR 7000 hybrid polyurea coatings exhibit excellent adhesion to steel and adhesion retention after longtermimmersion testing.


Read More
New Development in Penniman Red Production

A New Development in Penniman Red Production

A Solution for Nitrous Oxide Emissions
February 6, 2015
No Comments

The innovative Penniman red process sets new standards in the iron oxide industry due to its very low NOx and nitrous oxide emissions made possible by comprehensive waste gas and wastewater cleaning.


Read More

A Review of Global Supply and Demand for Titanium Dioxide

Ed Barlow
February 6, 2015
No Comments

We see a stabilizing of TiO2 supply, which will most likely lead to very modest price growth.


Read More
Previous 1 2 … 35 36 37 38 39 40 41 42 43 … 157 158 Next
Manage My Account
  • eMagazine
  • Newsletters
  • Online Registration
  • Subscription Customer Service

More Videos

Sponsored Content

Sponsored Content is a special paid section where industry companies provide high quality, objective, non-commercial content around topics of interest to the PCI audience. All Sponsored Content is supplied by the advertising company and any opinions expressed in this article are those of the author and not necessarily reflect the views of PCI or its parent company, BNP Media. Interested in participating in our Sponsored Content section? Contact your local rep!

close
  • wooden kitchen set and shelving
    Sponsored bySirca North America

    Leveraging Coatings to Meet ESG Goals in Manufacturing

  • man woodworking in workshop
    Sponsored byGemini Industries, Inc.

    Waterborne Coatings Aren't the Future -- They're the New Performance Benchmark

Popular Stories

Akzo, SW, Nippon Logos

AkzoNobel Rejects Cash Offer From Nippon Paint, Sherwin-Williams

BASF SE Logo

BASF Announces Strategic Business Sale

AkzoSWNipponEndTalks

Nippon Paint, Sherwin-Williams End AkzoNobel Pursuit

POB-Point-and-Shoot

PCI Buyers Guide

Submit a Request for Proposal (RFP) to suppliers of your choice with details on what you need with a click of a button

Start your RFP

Browse our Buyers Guide for manufacturers and distributors of all types of coatings products and much more!

Find Suppliers

Events

September 4, 2025

N-Butylpyrrolidone (NBP) as a Green Solvent to Replace N-Methylpyrrolidone (NMP) in Industrial Coating Applications

ON DEMAND: EPA published a regulation proposal around N-methylpyrrolidone (NMP) in June 2024 to ban or limit NMP in many applications, such as paints and coatings and their removers. N-butylpyrrolidone (NBP) is a powerful and versatile solvent for a variety of industries looking for alternatives to substance of very high concern (SVHC)-listed solvents.

September 15, 2026

Coatings Trends & Technologies Summit

The Coatings Trends & Technologies (CTT) Summit is an annual conference for both liquid and powder coatings formulators and manufacturers to discuss innovations in coatings technology. This event combines high-quality technical presentations, a resource-rich exhibit hall, and dedicated networking opportunities to connect scientific minds, foster innovation, and cultivate game-changing new ideas!

View All Submit An Event

Poll

Longest-running laboratory experiment

What is the longest-running laboratory experiment?
View Results Poll Archive

Products

Automotive Paints and Coatings, 2nd Edition

Now in its second edition and still the only book of its kind, this is an authoritative treatment of all stages of the coating process.

See More Products
Inside the AI Shift in Coatings - See the article now

Keep the info flowing with our eNewsletters!

Get the latest industry updates tailored your way.

JOIN TODAY!
  • RESOURCES
    • Advertise
    • Contact Us
    • Directories
    • Store
    • Want More
    • Manufacturing Division
  • SIGN UP TODAY
    • Create Account
    • eMagazine
    • Newsletters
    • Customer Service
    • Manage Preferences
  • SERVICES
    • Marketing Services
    • Reprints
    • Market Research
    • List Rental
    • Survey & Sample
  • STAY CONNECTED
    • LinkedIn
    • Facebook
    • Youtube
    • X (Twitter)
  • PRIVACY
    • PRIVACY POLICY
    • TERMS & CONDITIONS
    • DO NOT SELL MY PERSONAL INFORMATION
    • PRIVACY REQUEST
    • ACCESSIBILITY

Copyright ©2026. All Rights Reserved BNP Media, Inc. and BNP Media II, LLC.

Design, CMS, Hosting & Web Development :: ePublishing