Painting & Coating Industry (PCI) logo Powder coating summit logo
search
cart
facebook twitter linkedin youtube
  • Sign In
  • Join Today
  • Sign Out
  • My Account
Painting & Coating Industry (PCI) logo Powder coating summit logo
  • NEWS
    • Latest News
    • PCI News Now
    • Market Trends & Reports
    • Finishing News
    • Price Alerts
    • Global Top 10/ PCI 25
  • PRODUCTS
    • Product News
    • Featured Products
    • Must See Products and Services
  • MATERIALS
    • Additives
    • Resins/Polymers
    • Pigments
    • Equipment
    • Distributors
  • TECHNOLOGIES
    • Adhesives
    • Architectural Coatings
    • Finishing Articles
    • Finishing Technologies
    • Finishing Equipment
    • Industrial Coatings
    • Nanotechnology
    • Powder Coatings
    • Solventborne
    • Special Purpose Coatings
    • Sustainability
    • UV Coatings
    • Waterborne
  • EVENTS
    • Coatings Trends & Technologies Summit
    • Paint and Coatings Academy
    • Webinars
    • Calendar of Events
    • Lifetime Achievement Award
  • DIRECTORIES
    • Buyer's Guide
    • Equipment Directory
    • Materials Directory
  • RESOURCES
    • Columns
      • Did you know?
      • Distribution Dive
      • Formulating With Mike
      • Innovation Insights
      • Powder Coating Perspectives
      • TiO2 Insider
    • Blogs
      • Editor's Viewpoint
      • Industry Insights
    • Coatings Supplier Handbook
    • COAT-IT! Podcast
    • Videos
    • PCI Store
    • eBooks
    • Sponsor Insights
  • EMAGAZINE
    • eMagazine
    • Archive Issues
    • Editorial Advisory Board
    • CONTACT
    • Advertise
  • JOIN!
Home » Topics » Paint and Coatings Additives

Paint and Coatings Additives
Paint and Coatings Additives RSS Feed RSS

comparison between market standard thickeners and the new byk thickeners

New Non-Dusting Associative Thickeners from BYK

January 30, 2023
No Comments

The thickeners are supplied as flakes that do not tend to form dust, and yet are easy to incorporate into the millbase or into the letdown as well as a solution into the formulation.


Read More
GettyImages-530583272.jpg

Hygienic Coatings Prevent the Spread of Bacteria Safely

Teknos
January 27, 2023
No Comments

Teknos developed hygienic coatings for use in public spaces where there is a lot of movement, and infections spread easily. Study results confirm that these coatings are both safe and effective.


Read More
image of byk's production site in shanghai

BYK Completes Production Expansion in Shanghai

January 25, 2023
No Comments

Coatings additives supplier BYK has completed the expansion of its Shanghai integrated site, its second production facility in China following BYK Tongling. The site is designed for an annual capacity of 4,750 tons. 


Read More
Lead Image.png

Waterborne Conductive Primer/Adhesion Promoter with Graphene Nanotubes

Shows Sustainable Approach in Auto Industry
OCSiAl
January 9, 2023
One Comment

The new light-grey primer provides stable surface resistivity, strongly improving the adhesion between primer and base/clear coat on TPO car parts. A colloidal suspension of powder in water can be sprayed with standard liquid equipment devices while performing like a powder coating. 


Read More
GettyImages-1282726737.jpg

A Better Synthetic Rutile is Coming Soon

Taso Arima
December 28, 2022
No Comments

One metals technology company is commercializing innovative titanium mineral-enrichment technologies that upgrade ilmenite minerals into a high-grade TiO2 synthetic rutile product, with fewer carbon emissions than current industry processes.



Read More
pci1222-Songwon-471967941-1170.jpg

Stabilizer Solutions: Methods to Improve Resistance of BPA/BPF-Based Epoxy Resins to Light and Heat Damage

Sangjoon Park Benno Blickenstorfer Rosanna Telesca
December 20, 2022
One Comment

Epoxy resins are widely used in coatings thanks to their excellent adhesion to materials and their durability. However, epoxy resins typically contain aromatic groups with strong absorption in the UV range. This makes epoxy structures vulnerable to UV degradation. The performance of one company’s stabilizers in a typical commercial epoxy resin with hardeners are tested and reviewed in this article.


Read More
pci1222-Borregaard-1323677055-2.jpg

Novel Bio-Based Additives for Water-Based Coatings

Harrison Christopher Gallantree-Smith Ross J. Ellis Linn K. Larsson Anne Opstad Otto Soidinsalo
December 14, 2022
No Comments

Today, many coatings producers are increasingly focusing their production towards water-based coatings and are moving away from solvent-based formulations. This is to reduce the VOC content of their formulations, not only to make it friendlier for the end-user, but also to improve the sustainability impact on the environment by reducing their CO2 footprint. 


Read More
pci0222-Concentrol-484554988-1170.jpg

New Range of Ecological Anti-Foaming Agents

Josep Nadal Lorenzo Rico
December 13, 2022
No Comments

Anti-foam products allow controlling the presence of unwanted foam in different processes, including the manufacture and application of paints. A new range of mineral oil-free anti-foams have been designed, which are not harmful to humans or the environment due to their low or no toxicity, and include enhanced bio-degradability of the raw materials.


Read More
pco0922-OCSiAl-1137617582-1170.jpg

Exploring the Ability of Graphene Nanotubes to Enhance Coating Safety, Durability, and Performance

Ian Fellows
September 21, 2022
No Comments

The specific properties of graphene nanotubes that enable them to enhance different types of industrial coatings are explored.


Read More
pci0922-Spektrochem-1388358881-1170.jpg

Best Practices for Selecting Rheological Additives in Latex Paints and the Interpretation of their Effectiveness

Artur Palasz
September 19, 2022
No Comments

Best practices when selecting rheological additives are discussed in this article. The article explains that properly prepared technical materials are the basis for a quick and efficient start of tests and drawing conclusions based on repeated case studies in specific paint manufacturer formulations.


Read More
Previous 1 2 … 18 19 20 21 22 23 24 25 26 … 52 53 Next
Manage My Account
  • Join Paint & Coatings Industry
  • Manage My Preferences
  • Customer Service

More Videos

Popular Stories

industry news

Dozens Treated After Toledo Chemical Release

Mergers and aquisitions

Evonik Holds Off on BASF Takeover Talks

AkzoNobel Axalta

EU Clears $25B Akzo-Axalta Merger with One Big Condition

Events

November 19, 2026

Reformulating Paints with AI: Turn Change into a Competitive Advantage

Join industry leaders and experts for real case studies showing how AI helps R&D teams use existing paint formulation and test data to evaluate alternatives, predict trade-offs, and prioritize experiments.

December 10, 2026

PC Academy: Waterborne Polymers and Film Formation

The trend towards waterborne polymers in the paint and coatings industry is clear; highlighting their environmentally friendly nature, regulatory considerations, growing market demand, and meeting sustainability goals.

View All Submit An Event

Products

Powder Coatings - Foundation for the Novice Formulator (ebook)

Powder Coatings - Foundation for the Novice Formulator (ebook)

See More Products
PCI news now promo ad

Keep the info flowing with our eNewsletters!

Get the latest industry updates tailored your way.

JOIN TODAY!
  • RESOURCES
    • Advertise
    • Contact Us
    • Directories
    • Store
    • Manufacturing Division
  • JOIN TODAY
    • Create Account
    • eMagazine
    • Newsletters
    • Customer Service
    • Manage Preferences
  • SERVICES
    • Marketing Services
    • Reprints
    • Market Research
    • List Rental
    • Survey & Sample
  • STAY CONNECTED
    • LinkedIn
    • Facebook
    • Youtube
    • X (Twitter)
  • PRIVACY
    • PRIVACY POLICY
    • TERMS & CONDITIONS
    • DO NOT SELL MY PERSONAL INFORMATION
    • PRIVACY REQUEST
    • ACCESSIBILITY

Copyright ©2026. All Rights Reserved BNP Media, Inc. and BNP Media II, LLC.

Design, CMS, Hosting & Web Development :: ePublishing