Painting & Coating Industry (PCI) logo Powder coating summit logo
search
cart
facebook twitter linkedin youtube
  • Sign In
  • Create Account
  • Sign Out
  • My Account
Painting & Coating Industry (PCI) logo Powder coating summit logo
  • NEWS
    • Latest News
    • PCI News Now
    • Market Trends & Reports
    • Finishing News
    • Price Alerts
    • Global Top 10/ PCI 25
  • PRODUCTS
    • Product News
    • Featured Products
    • Must See Products and Services
  • MATERIALS
    • Additives
    • Resins/Polymers
    • Pigments
    • Equipment
    • Distributors
  • TECHNOLOGIES
    • Adhesives
    • Architectural Coatings
    • Finishing Articles
    • Finishing Technologies
    • Finishing Equipment
    • Industrial Coatings
    • Nanotechnology
    • Powder Coatings
    • Solventborne
    • Special Purpose Coatings
    • Sustainability
    • UV Coatings
    • Waterborne
  • EVENTS
    • Coatings Trends & Technologies Summit
    • Paint and Coatings Academy
    • Webinars
    • Calendar of Events
    • Lifetime Achievement Award
  • DIRECTORIES
    • Buyer's Guide
    • Equipment Directory
    • Materials Directory
  • RESOURCES
    • Columns
      • Did you know?
      • Distribution Dive
      • Formulating With Mike
      • Innovation Insights
      • Powder Coating Perspectives
      • TiO2 Insider
    • Blogs
      • Editor's Viewpoint
      • Industry Insights
    • Coatings Supplier Handbook
    • COAT-IT! Podcast
    • Videos
    • PCI Store
    • eBooks
    • Sponsor Insights
  • EMAGAZINE
    • eMagazine
    • Archive Issues
    • Editorial Advisory Board
    • CONTACT
    • Advertise
  • SIGN UP!
Home » Topics » Industrial Coatings

Industrial Coatings
Industrial Coatings RSS Feed RSS

Solvent-Based Polyurethane

December 3, 2012
No Comments
Acrolon Ultra is a high-gloss, solvent-based acrylic polyurethane providing long-term UV protection for high-profile structures where high durability is required.


Read More

Anticorrosion Coating

December 3, 2012
No Comments
NANOMYTE® TC‐3001is a new flexible coating specifically designed to protect oxidizing steel and aluminum exposed to corrosive chemicals or harsh environmental conditions.


Read More

Interior/Exterior, High-Performance Coatings

December 3, 2012
No Comments
Ultrashield is a new line of interior/exterior, high-performance coatings.


Read More

Teflon® Powder Coatings

December 3, 2012
No Comments
A full line of Teflon® powder coatings that are electro-statically applied to pumps, mixers, tanks, valves, and other components is available.


Read More

Lactides

December 3, 2012
No Comments
PURALACT® special-grade lactides provide reduced resin viscosity, allowing for coatings formulations with higher solid content, lower VOCs and improved ease-of-use.


Read More

Durable, Multi-Purpose Protective Coatings

William R. Schaeffer
November 1, 2012
No Comments
This article reports on the performance results of acrylated monomers and oligomers when subjected to typical end-use tests designed to measure the flexibility and adhesion characteristics of coatings.


Read More

A Powerful Ingredient at the Heart of “Green” Transformation

Brian Pickett
November 1, 2012
No Comments
We are used to the fact that technology lies at the heart of many modern innovative solutions, and the coatings industry is no exception to this fact.


Read More

High-Performance Carbon Black Pigment Advances Meet Emerging Needs

Thomas Papasso
October 1, 2012
No Comments
Performance requirements for carbon black pigments are increasingly important in the development of advanced coating, ink and polymer formulations as the need for more eco-friendly products grows.


Read More

Waterborne Epoxy Zinc-Rich Primers: There Are Viable Options

Françoise Heine Pascale Bouuaert Nathalie Wauters Jim Elmore Bedri Erdem Derek Crawford
September 4, 2012
No Comments
With stringent environmental and health regulations, waterborne coatings are increasingly replacing solventborne paints.


Read More

Corrosion-Resistant Nanocomposite Coating for Metal Structures

Dr. Jiong Liu Dr. Robert Lezzi
September 4, 2012
No Comments
Grit blasting of metal surfaces, a routine surface preparation technique prior to painting, is expensive, labor-intensive, time-consuming, and generates a large amount of hazardous, powdery waste


Read More
Previous 1 2 … 87 88 89 90 91 92 93 94 95 … 98 99 Next
Manage My Account
  • eMagazine
  • Newsletters
  • Online Registration
  • Subscription Customer Service

More Videos

Popular Stories

industry news

Dozens Treated After Toledo Chemical Release

AkzoNobel, Nippon

AkzoNobel to Sell Southeast Asia Decorative Paints Business to Nippon Paint for $1.35 Billion

Mergers and aquisitions

Evonik Declines BASF Negotiations

Events

November 5, 2026

Advancing Polyester Powder Coatings: Breakthroughs in Flexibility and Low-Cure Performance

Join us to learn how to improve coating durability while keeping your manufacturing process efficient. Explore the latest advancements in polyester powder coating technology.

November 12, 2026

Premium Leveling, Broad Compatibility: A Cost-Effective Flow and Leveling Additive

This new workhorse additive is recommended in all types of coatings. This highly compatible, 100% active siloxane product prevents defects and maintains good defoamer synergy.

View All Submit An Event
PCI news now promo ad

Keep the info flowing with our eNewsletters!

Get the latest industry updates tailored your way.

JOIN TODAY!
  • RESOURCES
    • Advertise
    • Contact Us
    • Directories
    • Store
    • Want More
    • Manufacturing Division
  • SIGN UP TODAY
    • Create Account
    • eMagazine
    • Newsletters
    • Customer Service
    • Manage Preferences
  • SERVICES
    • Marketing Services
    • Reprints
    • Market Research
    • List Rental
    • Survey & Sample
  • STAY CONNECTED
    • LinkedIn
    • Facebook
    • Youtube
    • X (Twitter)
  • PRIVACY
    • PRIVACY POLICY
    • TERMS & CONDITIONS
    • DO NOT SELL MY PERSONAL INFORMATION
    • PRIVACY REQUEST
    • ACCESSIBILITY

Copyright ©2026. All Rights Reserved BNP Media, Inc. and BNP Media II, LLC.

Design, CMS, Hosting & Web Development :: ePublishing