Painting & Coating Industry (PCI) logo Powder coating summit logo
search
cart
facebook twitter linkedin youtube
  • Sign In
  • Join Today
  • Sign Out
  • My Account
Painting & Coating Industry (PCI) logo Powder coating summit logo
  • NEWS
    • Latest News
    • PCI News Now
    • Market Trends & Reports
    • Finishing News
    • Price Alerts
    • Global Top 10/ PCI 25
  • PRODUCTS
    • Product News
    • Featured Products
    • Must See Products and Services
  • MATERIALS
    • Additives
    • Resins/Polymers
    • Pigments
    • Equipment
    • Distributors
  • TECHNOLOGIES
    • Adhesives
    • Architectural Coatings
    • Finishing Articles
    • Finishing Technologies
    • Finishing Equipment
    • Industrial Coatings
    • Nanotechnology
    • Powder Coatings
    • Solventborne
    • Special Purpose Coatings
    • Sustainability
    • UV Coatings
    • Waterborne
  • EVENTS
    • Coatings Trends & Technologies Summit
    • Paint and Coatings Academy
    • Webinars
    • Calendar of Events
    • Lifetime Achievement Award
  • DIRECTORIES
    • Buyer's Guide
    • Equipment Directory
    • Materials Directory
  • RESOURCES
    • Columns
      • Did you know?
      • Distribution Dive
      • Formulating With Mike
      • Innovation Insights
      • Powder Coating Perspectives
      • TiO2 Insider
    • Blogs
      • Editor's Viewpoint
      • Industry Insights
    • Coatings Supplier Handbook
    • COAT-IT! Podcast
    • Videos
    • PCI Store
    • eBooks
    • Sponsor Insights
  • EMAGAZINE
    • eMagazine
    • Archive Issues
    • Editorial Advisory Board
    • CONTACT
    • Advertise
  • JOIN!
Home » Topics » Waterborne Coatings

Waterborne Coatings
Waterborne Coatings RSS Feed RSS

Hexigone Lead Image.png

6,000 Hours of Real-World Anticorrosion Coastal Testing

Hexigone Inhibitors Ltd
January 24, 2025
No Comments

A cutting-edge anticorrosion additive endured 6,000 hours of real-world coastal testing—revealing surprising results, including the standout performance of waterborne acrylic coatings in marine environments.


Read More
chart with falling and rising columns and line

Coatings Additives Market Report

Eco-Friendly Solutions and Global Demand Fuel Growth
Priyanka Tiwari
December 8, 2024
No Comments

The coating additives market is set to expand due to increasing demand for waterborne products, bio-based solutions and corrosion protection across key industries.


Read More
paint roller in tray with white paint

Integrating Reactive Surfactants to Improve Water Resistance in Coatings

Reactive or Proactive?
Indorama Ventures
December 8, 2024
No Comments

Innovative reactive surfactants enhance water resistance and stability in waterborne coatings, marking a significant technological advancement in emulsion polymerization.


Read More
Japanese boho beige interior with armchair and commode background. Light modern natural Australian living room.

Shortcut to a Natural Look—Inherently Matte Acrylic

A water-based acrylic polymer technology delivers high transparency and low gloss, preserving a substrate’s natural look, while enhancing scratch and stain resistance, and long-term durability.
Fabian Gyger, Michael Lucas Benjamin van den Boom Kim Öhlenschläger Kaitlyn Funk
October 10, 2024
No Comments

In the realm of wood coatings, achieving a "natural look" has become a hallmark of modern design. To accomplish this, not only is low gloss required but also high transparency to preserve the vibrant colors of the wood.


Read More
sun rising over field of crops

Development of More-Sustainable Water-Based DTM Coatings, Part II

Soy-Alkyd Dispersion Paints
Debora L. Hense-Hric Kris Weigal
September 13, 2024
One Comment

The objective of this collaboration was to showcase the performance of sustainable, soy-based coating materials in real-world formulations, comparing them to benchmarks derived from petroleum-based counterparts. Part II of this series focuses on soy-alkyd dispersion paint. 


Read More
digital close up of molecules

Substituted Styrenic Monomers

Improving Waterborne Coating Performance
Pavel Ilmenev Ph.D.
August 5, 2024
4 Comments

When comparing the performance of polymer emulsions made with substituted styrene versus conventional styrene in direct-to-metal, wood coatings, concrete sealer, and FR/intumescent coating applications, the results demonstrate improved performance properties when the substitute is utilized.


Read More
Wooden cuisine cabinet with clean dishes. Scandinavian style kitchen interior. Organization of storage in kitchen. Different kind of cookware and ceramic plates on tabletop. Cleaning at kitchen

Debunking Myths About Waterborne Coatings

Kevin O’Neill
July 12, 2024
No Comments

Waterborne coatings have well-known benefits including a far-lower VOC-emissions profile, and lower inherent flammability, which make them generally safer to store and handle. There are still some common misperceptions around waterborne coatings, slowing their use. This article debunks a few of the most common myths.


Read More
GettyImages-1253477339-1170.jpg

Shortcut to a Natural Look

Inherently Matte Acrylic
Fabian Gyger, Kim Öhlenschläger Kaitlyn Funk Michael Lucas Benjamin van den Boom
July 9, 2024
No Comments

A coating with low gloss and high transparency is the basis for a matte finish, without affecting the color strength and thus, leading to a very natural wood look even with dark tones. The work presented here outlines the development and application data of an inherently matte, waterborne acrylic polymer. 


Read More
Empty interior in an elegan new house with wood floor

New Silicone-Free Super-Wetting Surfactants for Waterborne Coatings

Hilbert Esselbrugge
June 14, 2024
No Comments

A new wetting agent enhances wetting behavior, particularly in wood coatings. The innovative approach is based on a comparative evaluation of silicone-free and silicone-based surfactants, focusing on surface tension and contact angle.


Read More
Five paint cans - yellow, orange, white with paint samplers on white background

Phyllosilicate Clay Thickeners for Latex Paints

Winner of the PCI Award for Technical Excellence at the Waterborne Symposium
Artur Palasz
June 12, 2024
One Comment

This article discusses the basic characteristics of phyllosilicate thickeners, and provides an introduction to understanding their performance in formulations in order to use them to build the rheological properties of latex paints.


Read More
Previous 1 2 3 4 5 6 7 8 9 10 11 … 23 24 Next
Manage My Account
  • Join Paint & Coatings Industry
  • Manage My Preferences
  • Customer Service

More Videos

Popular Stories

industry news

Dozens Treated After Toledo Chemical Release

Mergers and aquisitions

Evonik Holds Off on BASF Takeover Talks

Lincoln Memorial Pool Coating

Inspection Report Finds at Least 85 Reflecting Pool Liner Failure Locations

Events

November 11, 2026

ChinaCoat

CHINACOAT2026 returns to Guangzhou this year. Welcome to exhibit, visit and join the annual industry gathering!

November 12, 2026

Premium Leveling, Broad Compatibility: A Cost-Effective Flow and Leveling Additive

This new workhorse additive is recommended in all types of coatings. This highly compatible, 100% active siloxane product prevents defects and maintains good defoamer synergy.

View All Submit An Event

Products

Powder Coatings - Foundation for the Novice Formulator (ebook)

Powder Coatings - Foundation for the Novice Formulator (ebook)

See More Products
PCI news now promo ad

Keep the info flowing with our eNewsletters!

Get the latest industry updates tailored your way.

JOIN TODAY!
  • RESOURCES
    • Advertise
    • Contact Us
    • Directories
    • Store
    • Manufacturing Division
  • JOIN TODAY
    • Create Account
    • eMagazine
    • Newsletters
    • Customer Service
    • Manage Preferences
  • SERVICES
    • Marketing Services
    • Reprints
    • Market Research
    • List Rental
    • Survey & Sample
  • STAY CONNECTED
    • LinkedIn
    • Facebook
    • Youtube
    • X (Twitter)
  • PRIVACY
    • PRIVACY POLICY
    • TERMS & CONDITIONS
    • DO NOT SELL MY PERSONAL INFORMATION
    • PRIVACY REQUEST
    • ACCESSIBILITY

Copyright ©2026. All Rights Reserved BNP Media, Inc. and BNP Media II, LLC.

Design, CMS, Hosting & Web Development :: ePublishing