Painting & Coating Industry (PCI) logo Powder coating summit logo
search
cart
facebook twitter linkedin youtube
  • Sign In
  • Create Account
  • Sign Out
  • My Account
Painting & Coating Industry (PCI) logo Powder coating summit logo
  • NEWS
    • Latest News
    • Market Trends & Reports
    • Finishing News
    • Price Alerts
    • Global Top 10/ PCI 25
  • PRODUCTS
    • Product News
    • Featured Products
    • Must See Products and Services
  • MATERIALS
    • Additives
    • Resins/Polymers
    • Pigments
    • Equipment
    • Distributors
  • TECHNOLOGIES
    • Adhesives
    • Architectural Coatings
    • Finishing Articles
    • Finishing Technologies
    • Finishing Equipment
    • Industrial Coatings
    • Nanotechnology
    • Powder Coatings
    • Solventborne
    • Special Purpose Coatings
    • Sustainability
    • UV Coatings
    • Waterborne
  • EVENTS
    • Coatings Trends & Technologies Summit
    • Paint and Coatings Academy
    • Webinars
    • Calendar of Events
    • Lifetime Achievement Award
  • DIRECTORIES
    • Buyer's Guide
    • Equipment Directory
    • Materials Directory
  • RESOURCES
    • Columns
      • Did you know?
      • Distribution Dive
      • Formulating With Mike
      • Innovation Insights
      • Powder Coating Perspectives
      • TiO2 Insider
    • Blogs
      • Editor's Viewpoint
      • Industry Insights
    • Coatings Supplier Handbook
    • COAT-IT! Podcast
    • Videos
    • PCI Store
    • eBooks
    • Sponsor Insights
  • EMAGAZINE
    • eMagazine
    • Archive Issues
    • Editorial Advisory Board
    • CONTACT
    • Advertise
  • SIGN UP!
Home » Topics » FT Archives

FT Archives
FT Archives RSS Feed RSS

One-Step Metal Pretreatment

Mary Carpenter
July 1, 2007
No Comments
Metal preparation is in many ways a dirty business. Improvements have been made in the painting phase of the operation, including a general switch to high-solids liquids and powder coatings. But pretreatment has not changed much in many years. However, starting in 2000, a different kind of pretreatment was introduced in North America. This single-stage organic phosphating system is reducing the cost and environmental impact of pretreating metal substrates.
Read More

Extending the Life of Bell Cups

July 1, 2007
No Comments
In a typical automotive plant, bell cups must be replaced every three to four months. As a result, an automotive plant using 50 rotary bell atomizers might incur replacement costs for bell cups totaling approximately $300,000 per year. An advanced coating technology can extend the life of paint bell cups and offer a dramatic cost savings for rotary paint atomizer users.
Read More

Advanced Finishes for Farm Equipment

Linda Cassil
July 1, 2007
No Comments
As agricultural equipment has advanced, coating technology for this demanding market has improved along with it. With modern polyurethane and powder coating formulations, today’s farm equipment manufacturers can achieve durable, high-quality, cost-effective finishes on a range of substrates.
Read More

Cost-Effective Conductivity

Jill Simpson, Ph.D Patrick Kinlen Ph.D.
July 1, 2007
No Comments
New coatings based on a conductive polymer known as soluble doped polyaniline can offer a significant improvement in functionality and ease of application over current capacitor coating technologies. The new coatings provide the same benefits as traditional conductive polymer-based coatings but with significantly less manufacturing time, as well as other enhanced attributes.
Read More

A Virtual Approach to Applicator Training

Joe Bolick
July 1, 2007
No Comments
Proper hands-on training can produce immediate and long-term results in areas such as material conservation, waste and air emission reduction, reduced rework, and better finish quality. However, a significant drawback of traditional hands-on training has been the time and materials required to perform this task properly. A virtual reality training tool can provide paint and powder applicators with the benefits of hands-on training while eliminating the time and material requirements.
Read More

A Double-Duty Cure

Douglas Larsen
July 1, 2007
No Comments
Have you ever wondered whether your curing ovens could make better use of all those British thermal units before venting the waste heat? With heat-activated structural epoxy adhesive tapes, they can. These tapes can combine components into assemblies, replace unsightly welds or rivets, join dissimilar metals without the threat of corrosion and provide local stiffening, all while being cured in an existing electrocoat (e-coat) or powder coat oven cure process.
Read More

Rohm and Haas to Invest $60 Million in Anti-Reflective Coatings - Posted 6/27/07

June 27, 2007
No Comments
Rohm and Haas Electronic Materials will invest $60 million in leading-edge lithography equipment to support its extensive research and development of advanced 193 nanometer (nm) photoresist and anti-reflective coatings used in the manufacture of semiconductor devices.
Read More

SPI Achieves ISO 9001:2000 Certification - Posted 6/27/07

June 27, 2007
No Comments
Specialty Products, Inc. (SPI) was recognized to be in compliance with the quality management standards required for ISO 9001:2000 certification by AIB-Vincotte USA, on May 17, 2007.
Read More

Industrial Nanotech Supplies Coatings to Latin American Brewery - Posted 6/27/07

June 27, 2007
One Comment
Industrial Nanotech, Inc., a nanotechnology firm, is working with AmBev to incorporate its Nansulate line of industrial coatings into the company’s plant maintenance program through the company's manufacturer's representative in Brazil. AmBev is the largest private producer of consumer goods in Brazil, the biggest brewery in Latin America, and has operations in 14 countries in the Americas.
Read More

Basell to Acquire Huntsman - Posted 6/27/07

June 27, 2007
No Comments
Basell, a global leader in polyolefin technology, production and marketing, and Huntsman Corp., one of the world’s largest manufacturers and marketers of differentiated chemicals and pigments, have signed a definitive agreement pursuant to which Basell will acquire Huntsman in a transaction valued at approximately $9.6 billion.
Read More
Previous 1 2 … 80 81 82 83 84 85 86 87 88 … 231 232 Next
Manage My Account
  • eMagazine
  • Newsletters
  • Online Registration
  • Subscription Customer Service

More Videos

Popular Stories

Breaking News

Yenkin-Majestic Pleads Guilty in Fatal Resin Plant Explosion Case

Evonik Logo

Evonik to Close Two German Sites

Mergers-and-Company-Strategies.jpg

BASF Confirms Exploratory Talks on Potential Evonik Takeover

Webinar custom content box

Events

October 8, 2026

AI-Powered Reformulation: Finding PFAS-Free, Lower-VOC Formulations Faster

In this webinar, we will use case studies from industry to illustrate how AI can be used to identify PFAS-free formulations and select surfactant blends for water-based products.

January 1, 2030

Webinar Sponsorship Information

For webinar sponsorship information, visit www.bnpevents.com/webinars or email webinars@bnpmedia.com.

View All Submit An Event

Products

Advanced Coating Materials

Advanced Coating Materials

See More Products
Webinar custom content box

Keep the info flowing with our eNewsletters!

Get the latest industry updates tailored your way.

JOIN TODAY!
  • RESOURCES
    • Advertise
    • Contact Us
    • Directories
    • Store
    • Want More
    • Manufacturing Division
  • SIGN UP TODAY
    • Create Account
    • eMagazine
    • Newsletters
    • Customer Service
    • Manage Preferences
  • SERVICES
    • Marketing Services
    • Reprints
    • Market Research
    • List Rental
    • Survey & Sample
  • STAY CONNECTED
    • LinkedIn
    • Facebook
    • Youtube
    • X (Twitter)
  • PRIVACY
    • PRIVACY POLICY
    • TERMS & CONDITIONS
    • DO NOT SELL MY PERSONAL INFORMATION
    • PRIVACY REQUEST
    • ACCESSIBILITY

Copyright ©2026. All Rights Reserved BNP Media, Inc. and BNP Media II, LLC.

Design, CMS, Hosting & Web Development :: ePublishing