Painting & Coating Industry (PCI) logo Powder coating summit logo
search
cart
facebook twitter linkedin youtube
  • Sign In
  • Create Account
  • Sign Out
  • My Account
Painting & Coating Industry (PCI) logo Powder coating summit logo
  • NEWS
    • Latest News
    • Market Trends & Reports
    • Finishing News
    • Price Alerts
    • Global Top 10/ PCI 25
  • PRODUCTS
    • Product News
    • Featured Products
    • Must See Products and Services
  • MATERIALS
    • Additives
    • Resins/Polymers
    • Pigments
    • Equipment
    • Distributors
  • TECHNOLOGIES
    • Adhesives
    • Architectural Coatings
    • Finishing Articles
    • Finishing Technologies
    • Finishing Equipment
    • Industrial Coatings
    • Nanotechnology
    • Powder Coatings
    • Solventborne
    • Special Purpose Coatings
    • Sustainability
    • UV Coatings
    • Waterborne
  • EVENTS
    • Coatings Trends & Technologies Summit
    • Paint and Coatings Academy
    • Webinars
    • Calendar of Events
    • Lifetime Achievement Award
  • DIRECTORIES
    • Buyer's Guide
    • Equipment Directory
    • Materials Directory
  • RESOURCES
    • Columns
      • Did you know?
      • Distribution Dive
      • Formulating With Mike
      • Innovation Insights
      • Powder Coating Perspectives
      • TiO2 Insider
    • Blogs
      • Editor's Viewpoint
      • Industry Insights
    • Coatings Supplier Handbook
    • COAT-IT! Podcast
    • Videos
    • PCI Store
    • eBooks
    • Sponsor Insights
  • EMAGAZINE
    • eMagazine
    • Archive Issues
    • Editorial Advisory Board
    • CONTACT
    • Advertise
  • SIGN UP!
Home » Topics » Finishing Articles

Finishing Articles
Finishing Articles RSS Feed RSS

20221122-covestro-at-trustech-2022-pic.jpg

Pushing Boundaries in ID Document Innovations

February 9, 2023
No Comments

Covestro offers a comprehensive specialty films portfolio for producing highly secure ID documents, such as passports and e-ID cards. 


Read More
Lead Image.JPG

Selective Brush Plating: a Flexible, Automated Solution to Plating Challenges

SIFCO Applied Surface Concepts (SIFCO ASC)
February 2, 2023
No Comments

Innovation continues at a great pace in the area of plating automation. The latest development comes in the form of a fully portable automated electroplating system, able to be moved directly to a specific component for in situ plating. 



Read More
GettyImages-530583272.jpg

Hygienic Coatings Prevent the Spread of Bacteria Safely

Teknos
January 27, 2023
No Comments

Teknos developed hygienic coatings for use in public spaces where there is a lot of movement, and infections spread easily. Study results confirm that these coatings are both safe and effective.


Read More
Lead Image.jpeg

Industrial Safety: Preventing Slips and Falls Virtually Everywhere

Del Williams
January 20, 2023
2 Comments

A new category of durable, high-tech, all-epoxy coating is dramatically increasing traction and improving safety in a wide range of slip and fall prone areas such as production floors, warehouse space, loading docks, platforms, ramps, and more.



Read More
GettyImages-1214122572.jpg

Coatings are a Game Changer in Pest Control

Tony Gonzales
January 12, 2023
3 Comments

Pest control coatings are truly innovative. By targeting a crawling pest’s inability to climb a smooth surface, a physical barrier around a home can be created with a coating.



Read More
Singulus_colored_coatings.jpg

Sustainably and Economically Coating 3D Components with Titanium

Singulus Technologies
January 1, 2023
No Comments

Singulus Technologies has developed a new layer system with titanium for sustainable coatings with the DECOLINE II production line. The innovative coating process reduces the necessary production steps and is, therefore, significantly more economical. 


Read More
Lead Image.png

Next-Generation Powder Coatings Shift from Pre- to Post-Consumer Recycled Plastic Resins

Sherwin Williams
December 23, 2022
No Comments

A line of powder coatings from Sherwin-Williams are now formulated with trailblazing polyester resins comprised of 25 percent post-consumer recycled plastic (rPET).


Read More
Lead Image.jpg

How Are Electric Vehicle Battery Coatings Improving the Auto Industry?

Emily Newton
December 9, 2022
No Comments

Internal combustion engines (ICEs) are falling out of fashion to make way for battery electric vehicles (BEVs). Many components, including battery packs and power conversion parts, should have coatings to increase the car’s longevity, and to help with the issues BEV batteries bring. Creative solutions are coming out of the industry to help maintain BEVs for longer. 


Read More
Lead Image.jpg

WashU’s McKelvey Hall Receives Sustainability-Focused Redesign 

Tubelite Inc.
November 25, 2022
No Comments

Part of the largest capital project in Washington University’s (WashU’s) 125-year history, James M. McKelvey, Sr. Hall completes the final stage for the East End transformation of Danforth Campus in St. Louis, Missouri. Sustainability and occupant well-being were essential objectives for the university.


Read More
Lead Image.jpg

HMG Paints Assists with Iconic Aston Martin Conservation

HMG Paints
November 21, 2022
No Comments

Ecurie Bertelli, the pre-war Aston Martin specialist, and HMG Paints, a United Kingdom-based independent paint manufacturer, have combined their market leading knowledge for a one-of-a-kind project conserving a 1934 Aston Martin MKII. The team at HMG Paints developed a special stabilizing and sealing solution that allowed the team to seal the worn paintwork and prevent further degradation.


Read More
Previous 1 2 … 17 18 19 20 21 22 23 24 25 … 41 42 Next
Manage My Account
  • eMagazine
  • Newsletters
  • Online Registration
  • Subscription Customer Service

More Videos

Popular Stories

Evonik Logo

Evonik to Close Two German Sites

Mergers-and-Company-Strategies.jpg

BASF Confirms Exploratory Talks on Potential Evonik Takeover

Breaking News

Evonik Rejected €10.3 Billion BASF Offer, Reuters Reports

Webinar custom content box

Events

January 1, 2030

Webinar Sponsorship Information

For webinar sponsorship information, visit www.bnpevents.com/webinars or email webinars@bnpmedia.com.

View All Submit An Event

Products

Advanced Coating Materials

Advanced Coating Materials

See More Products
Webinar custom content box

Keep the info flowing with our eNewsletters!

Get the latest industry updates tailored your way.

JOIN TODAY!
  • RESOURCES
    • Advertise
    • Contact Us
    • Directories
    • Store
    • Want More
    • Manufacturing Division
  • SIGN UP TODAY
    • Create Account
    • eMagazine
    • Newsletters
    • Customer Service
    • Manage Preferences
  • SERVICES
    • Marketing Services
    • Reprints
    • Market Research
    • List Rental
    • Survey & Sample
  • STAY CONNECTED
    • LinkedIn
    • Facebook
    • Youtube
    • X (Twitter)
  • PRIVACY
    • PRIVACY POLICY
    • TERMS & CONDITIONS
    • DO NOT SELL MY PERSONAL INFORMATION
    • PRIVACY REQUEST
    • ACCESSIBILITY

Copyright ©2026. All Rights Reserved BNP Media, Inc. and BNP Media II, LLC.

Design, CMS, Hosting & Web Development :: ePublishing