Painting & Coating Industry (PCI) logo Powder coating summit logo
search
cart
facebook twitter linkedin youtube
  • Sign In
  • Create Account
  • Sign Out
  • My Account
Painting & Coating Industry (PCI) logo Powder coating summit logo
  • NEWS
    • Latest News
    • Market Trends & Reports
    • Finishing News
    • Price Alerts
    • Global Top 10/ PCI 25
  • PRODUCTS
    • Product News
    • Featured Products
    • Must See Products and Services
  • MATERIALS
    • Additives
    • Resins/Polymers
    • Pigments
    • Equipment
    • Distributors
  • TECHNOLOGIES
    • Adhesives
    • Architectural Coatings
    • Finishing Articles
    • Finishing Technologies
    • Finishing Equipment
    • Industrial Coatings
    • Nanotechnology
    • Powder Coatings
    • Solventborne
    • Special Purpose Coatings
    • Sustainability
    • UV Coatings
    • Waterborne
  • EVENTS
    • Coatings Trends & Technologies Summit
    • Paint and Coatings Academy
    • Webinars
    • Calendar of Events
    • Lifetime Achievement Award
  • DIRECTORIES
    • Buyer's Guide
    • Equipment Directory
    • Materials Directory
  • RESOURCES
    • Columns
      • Did you know?
      • Distribution Dive
      • Formulating With Mike
      • Innovation Insights
      • Powder Coating Perspectives
      • TiO2 Insider
    • Blogs
      • Editor's Viewpoint
      • Industry Insights
    • Coatings Supplier Handbook
    • COAT-IT! Podcast
    • Videos
    • PCI Store
    • eBooks
    • Sponsor Insights
  • EMAGAZINE
    • eMagazine
    • Archive Issues
    • Editorial Advisory Board
    • CONTACT
    • Advertise
  • SIGN UP!
Home » Topics » Finishing Articles

Finishing Articles
Finishing Articles RSS Feed RSS

Cortec Lead Image.jpg

Choosing the Best Paint for Metal

Cortec Corporation
July 24, 2023
No Comments

In addition to good adhesion and rust prevention, a metal coating must be equipped to meet force-dry, high-slip, or high-temp requirements in certain applications. To address these needs, one company offers two specialty versions of a high-performing, water-based, anti-corrosion coating for industrial applications.


Read More
PRAB Lead Image.jpg

New Dip-and-Spin Technologies Reduce Material and Labor Costs

Tim Hanna
July 24, 2023
No Comments

At a time when every drop of coating material and workforce resource is precious, cutting back on material waste and operational inefficiencies is vital to the continued success of any coating operation. New advancements in coating technologies make that possible.


Read More
PPG’s New Paint for a New Start Initiative Transforms Primary School in China.jpg

PPG’s New Paint for a New Start Initiative Transforms Primary School in China

July 17, 2023
No Comments

In the second year of New Paint for a New Start, PPG employees around the world are volunteering their time throughout the months of June, July and August to transform more than 25 schools.


Read More
pci0723-BenjaminMoore-FK_CT23_B03_RasperryBlush_RGB-1170.jpg

Leading a Business Through Challenging Times

Kristin Johansson Dan Calkins
July 17, 2023
One Comment

In an exclusive interview with PCI Magazine, Dan Calkins, Chairman and CEO of Benjamin Moore & Co., discusses leading his business through the extreme challenges of the last four years, and chasing the “new normal” in the paint and coatings industry.


Read More
GettyImages-1170x878-1270321679.jpg

How Can the Paint Industry Improve PSRA Compliance?

Emily Newton
July 14, 2023
No Comments

Product stewardship and regulatory affairs (PSRA) professionals handle the minimization of all negative environmental impacts, and follow the respective regulations for formulating, manufacturing, and distributing products responsibly. Here are some particular ways paint professionals can promote product stewardship and regulatory compliance within their industry. 


Read More
AmCoat Lead Image.jpg

Best in Class Means Best in Safety

Ceramic Elastomeric Coating Offers Class A Fire Rating
AmCoat Industrial
July 8, 2023
No Comments

With an increase in the number of wildfires since the late 1990s, it’s important to use fire-rated materials when building or renovating a home. One company shares steps taken over the last 25 years to ensure its high-performance products are as safe as they possibly can be.


Read More
GettyImages-1450272068.jpg

Solar Glass Coatings Enhance Electricity Production

Strategic Market Research
July 3, 2023
No Comments

The United States has increased the use of solar and wind power for electricity production. The U.S. Department of Energy claims that preserving your panels' surface with a glass coating can boost the photoelectric effect by up to 3-6%, therefore boosting potential demand in the glass coatings market. 


Read More
Dunn-Edwards Announces 2024 Color + Design Trends To Watch.jpg

Dunn-Edwards Announces 2024 Color + Design Trends To Watch

June 26, 2023
No Comments

Four expert-selected color palettes explore the journey of rediscovery and escapism through design. 


Read More
ION Science Lead Image.jpg

High-Performance Sensors Underpin the Quality of Occupational Safety Equipment

ION Science Ltd.
June 22, 2023
One Comment

Employers have a duty of care to protect the health, safety, and welfare of employees, so it is vitally important to keep workers’ occupational exposure to harmful gases within permissible limits. For this reason, providing highly accurate sensors that are reliable is a must. 


Read More
Wagner Lead Image.jpg

Resource-Saving Coating Technology for Rail Vehicle Wheels

Walther Spritz- und Lackiersysteme GmbH
June 20, 2023
No Comments

In order to adapt to the increasing demand in rail transport, a wheelset system production plant was modernized to include use of a highly efficient coating line that emphasizes sustainability and resource-saving production value. 


Read More
Previous 1 2 … 13 14 15 16 17 18 19 20 21 … 41 42 Next
Manage My Account
  • eMagazine
  • Newsletters
  • Online Registration
  • Subscription Customer Service

More Videos

Popular Stories

Evonik Logo

Evonik to Close Two German Sites

Mergers-and-Company-Strategies.jpg

BASF Confirms Exploratory Talks on Potential Evonik Takeover

Breaking News

Evonik Rejected €10.3 Billion BASF Offer, Reuters Reports

Webinar custom content box

Events

January 1, 2030

Webinar Sponsorship Information

For webinar sponsorship information, visit www.bnpevents.com/webinars or email webinars@bnpmedia.com.

View All Submit An Event

Products

Advanced Coating Materials

Advanced Coating Materials

See More Products
Webinar custom content box

Keep the info flowing with our eNewsletters!

Get the latest industry updates tailored your way.

JOIN TODAY!
  • RESOURCES
    • Advertise
    • Contact Us
    • Directories
    • Store
    • Want More
    • Manufacturing Division
  • SIGN UP TODAY
    • Create Account
    • eMagazine
    • Newsletters
    • Customer Service
    • Manage Preferences
  • SERVICES
    • Marketing Services
    • Reprints
    • Market Research
    • List Rental
    • Survey & Sample
  • STAY CONNECTED
    • LinkedIn
    • Facebook
    • Youtube
    • X (Twitter)
  • PRIVACY
    • PRIVACY POLICY
    • TERMS & CONDITIONS
    • DO NOT SELL MY PERSONAL INFORMATION
    • PRIVACY REQUEST
    • ACCESSIBILITY

Copyright ©2026. All Rights Reserved BNP Media, Inc. and BNP Media II, LLC.

Design, CMS, Hosting & Web Development :: ePublishing