Tnemec Co. Inc., a leading manufacturer of high-performance protective coatings, announced the launch of three low-VOC polyurethane coatings: Series 1094, Series 1095 and Series 1096 Endura-Shield.
Pison Stream Solutions' Defense Coatings business announced that its White Type III Topcoat powder coating meets the newest Type III military specification approval for CARC (chemical agent resistant coating) powder topcoats.
ALTANA announced that Tammo Boinowitz will become Managing Director of BYK-Chemie GmbH based in Wesel, Germany, as of Jan. 1, 2021, and after a two-month training and transitional phase, will also become the President of BYK.
Axalta Coating Systems Ltd. announced its financial results for the first quarter ended March 31, 2020, and provided an update regarding the impact of the COVID-19 pandemic on its business, employees, customers and shareholders as well as Axalta's current and planned management of such impacts.
The International Carbon Black Association (ICBA) recently awarded certificates of recognition to 14 plants and two R&D centers of Birla Carbon for achieving a level of safety performance above the industry average.