Painting & Coating Industry (PCI) logo Powder coating summit logo
search
cart
facebook twitter linkedin youtube
  • Sign In
  • Create Account
  • Sign Out
  • My Account
Painting & Coating Industry (PCI) logo Powder coating summit logo
  • NEWS
    • Latest News
    • Market Trends & Reports
    • Finishing News
    • Price Alerts
    • Subscribe to Newsletters
    • Global Top 10/ PCI 25
    • Weekly Featured Article
  • PRODUCTS
    • Product News
    • Featured Products
    • Must See Products and Services
  • MATERIALS
    • Additives
    • Resins/Polymers
    • Pigments
    • Equipment
    • Distributors
  • TECHNOLOGIES
    • Adhesives
    • Architectural Coatings
    • Finishing Articles
    • Finishing Technologies
    • Finishing Equipment
    • Industrial Coatings
    • Nanotechnology
    • Powder Coatings
    • Solventborne
    • Special Purpose Coatings
    • Sustainability
    • UV Coatings
    • Waterborne
  • RESOURCES
    • Columns
      • Did you know?
      • Distribution Dive
      • Formulating With Mike
      • Innovation Insights
      • Powder Coating Perspectives
      • TiO2 Insider
    • Blogs
      • Editor's Viewpoint
      • Industry Insights
    • Coatings Supplier Handbook
    • Podcasts and Videos
      • COAT-IT! Podcast
      • Videos/PCI TV
    • PCI Store
    • Classifieds
    • eBooks
    • Sponsor Insights
    • White Papers
    • COATLE Word Game
  • EVENTS
    • Coatings Trends & Technologies Summit
    • Paint and Coatings Academy
    • Webinars
    • Calendar of Events
    • Lifetime Achievement Award
  • DIRECTORIES
    • Buyer's Guide
    • Equipment Directory
    • Materials Directory
  • EMAGAZINE
    • Current Issue
    • eMagazine Archive
    • China Issue Archive
    • Editorial Advisory Board
  • CONTACT
    • Contact Us
    • Advertise
    • Subscribe to eMagazine
    • Subscribe to Newsletters
  • SIGN UP!
FT Archives

Green Workstations

December 1, 2006
An environmentally friendly wood coating is playing a key role in the design of one of the cleanest, greenest buildings on earth.

Built at a cost of $51 million (Australian) and brimming with technical innovations, the new 10-story Melbourne City Council building - known as CH2 - was recently awarded the first six star design rating from Autralia’s Green Building Council.

Sustainable technology had to be incorporated into every aspect of the design, including the building’s interior. Coatings and materials were chosen to help minimize indoor air pollution, and the building’s designers paid special attention to the furniture.

Like a lot of modern furniture, the workstations used by the 500-plus CH2 employees are made from medium density fiberboard (MDF). When the decision was made to use powder coatings on the workstation surfaces - a coating not traditionally used on wood products due to the heat involved during the curing process - the designers turned to Akzo Nobel’s new Interpon Woodcote TE product line, developed by the company’s Powder Coatings business.

“Woodcote TE is a specially formulated coating which is environmentally sound and introduces no harmful emissions during or after application,” explains Guy Vissel, Akzo Nobel’s Powder Coatings marketing manager in Australia. “We’ve been working on powder coatings for MDF for a number of years and have been able to draw on a lot of global expertise during the development of this new product line.”

The contract for the Melbourne building was the culmination of a project that involved Woodcote TE being used in the creation of a new powder coated MDF system called Opalz™. Devised by Powder Coatings’ customer Decorative Imaging, the resulting system involves the use of MDF panels supplied by Carter Holt Harvey, with a company called Formway Furniture using Opalz to produce the ergonomically designed workstations now found in CH2.

“The traditional coating for this type of application is solventborne polyurethane,” adds Vissel. “But Woodcote TE, which has been on the market for less than a year, now offers an attractive and durable surface finish with the added benefit of being perfectly suited to environmentally conscious design.”

For more information about the CH2 project or powder coatings for MDF, visit www.akzonobel.com.

Share This Story

Looking for a reprint of this article?
From high-res PDFs to custom plaques, order your copy today!

Recommended Content

JOIN TODAY
to unlock your recommendations.

Already have an account? Sign In

  • Double exposure of creative chemistry concept on laptop background, research and development concept

    Inside the AI Shift in Coatings

    Industry leaders share real-world examples of how AI is...
    Paint and Coatings Additives
    By: PCI Editorial Staff
  • Global Top 10 and PCI Logo

    2026 Global Top 10: Top Paint and Coatings Companies

    See how the world’s largest paint and coatings companies...
    Global Top 10 and PCI 25
    By: Courtney Bassett
  • The 2026 PCI 25

    2026 PCI 25: Top Paint and Coatings Companies

    See how North America's largest paint and coatings...
    Global Top 10 and PCI 25
    By: Courtney Bassett
You must login or register in order to post a comment.

Report Abusive Comment

Manage My Account
  • eMagazine
  • Newsletters
  • Online Registration
  • Subscription Customer Service

More Videos

Sponsored Content

Sponsored Content is a special paid section where industry companies provide high quality, objective, non-commercial content around topics of interest to the PCI audience. All Sponsored Content is supplied by the advertising company and any opinions expressed in this article are those of the author and not necessarily reflect the views of PCI or its parent company, BNP Media. Interested in participating in our Sponsored Content section? Contact your local rep!

close
  • wooden kitchen set and shelving
    Sponsored bySirca North America

    Leveraging Coatings to Meet ESG Goals in Manufacturing

  • man woodworking in workshop
    Sponsored byGemini Industries, Inc.

    Waterborne Coatings Aren't the Future -- They're the New Performance Benchmark

Popular Stories

The 2026 PCI 25

2026 PCI 25: Top Paint and Coatings Companies

USA election voters in red and blue to represent democrats and republicans

The AkzoNobel-Axalta Vote is Over. What Will Regulators Ask Next?

Global Top 10 and PCI Logo

2026 Global Top 10: Top Paint and Coatings Companies

The PCI 25 Annual Revenue Rankings

Events

September 4, 2025

N-Butylpyrrolidone (NBP) as a Green Solvent to Replace N-Methylpyrrolidone (NMP) in Industrial Coating Applications

ON DEMAND: EPA published a regulation proposal around N-methylpyrrolidone (NMP) in June 2024 to ban or limit NMP in many applications, such as paints and coatings and their removers. N-butylpyrrolidone (NBP) is a powerful and versatile solvent for a variety of industries looking for alternatives to substance of very high concern (SVHC)-listed solvents.

September 15, 2026

Coatings Trends & Technologies Summit

The Coatings Trends & Technologies (CTT) Summit is an annual conference for both liquid and powder coatings formulators and manufacturers to discuss innovations in coatings technology. This event combines high-quality technical presentations, a resource-rich exhibit hall, and dedicated networking opportunities to connect scientific minds, foster innovation, and cultivate game-changing new ideas!

View All Submit An Event

Poll

Longest-running laboratory experiment

What is the longest-running laboratory experiment?
View Results Poll Archive

Products

Advanced Coating Materials

Advanced Coating Materials

See More Products
PCI Coat It! Podcast

Related Articles

  • Former Chief of the World Green Building Council to Promote Green Building in Asia

    See More
  • Green Performance - More Valuable than Green Products

    See More
  • APEC Conference on Green Buildings and Green Growth Emphasizes Cooperation

    See More

Related Products

See More Products
  • Wood Coatings

  • 9780323355957.jpg

    Adhesives Technology Handbook, 3rd Edition

  • Handbook of Adhesives and Surface Preparation

See More Products
×

Keep the info flowing with our eNewsletters!

Get the latest industry updates tailored your way.

JOIN TODAY!
  • RESOURCES
    • Advertise
    • Contact Us
    • Directories
    • Store
    • Want More
    • Manufacturing Division
  • SIGN UP TODAY
    • Create Account
    • eMagazine
    • Newsletters
    • Customer Service
    • Manage Preferences
  • SERVICES
    • Marketing Services
    • Reprints
    • Market Research
    • List Rental
    • Survey & Sample
  • STAY CONNECTED
    • LinkedIn
    • Facebook
    • Youtube
    • X (Twitter)
  • PRIVACY
    • PRIVACY POLICY
    • TERMS & CONDITIONS
    • DO NOT SELL MY PERSONAL INFORMATION
    • PRIVACY REQUEST
    • ACCESSIBILITY

Copyright ©2026. All Rights Reserved BNP Media, Inc. and BNP Media II, LLC.

Design, CMS, Hosting & Web Development :: ePublishing