Painting & Coating Industry (PCI) logo Powder coating summit logo
search
cart
facebook twitter linkedin youtube
  • Sign In
  • Join Today
  • Sign Out
  • My Account
Painting & Coating Industry (PCI) logo Powder coating summit logo
  • NEWS
    • Latest News
    • PCI News Now
    • Market Trends & Reports
    • Finishing News
    • Price Alerts
    • Global Top 10/ PCI 25
  • PRODUCTS
    • Product News
    • Featured Products
    • Must See Products and Services
  • MATERIALS
    • Additives
    • Resins/Polymers
    • Pigments
    • Equipment
    • Distributors
  • TECHNOLOGIES
    • Adhesives
    • Architectural Coatings
    • Finishing Articles
    • Finishing Technologies
    • Finishing Equipment
    • Industrial Coatings
    • Nanotechnology
    • Powder Coatings
    • Solventborne
    • Special Purpose Coatings
    • Sustainability
    • UV Coatings
    • Waterborne
  • EVENTS
    • Coatings Trends & Technologies Summit
    • Paint and Coatings Academy
    • Webinars
    • Calendar of Events
    • Lifetime Achievement Award
  • DIRECTORIES
    • Buyer's Guide
    • Equipment Directory
    • Materials Directory
  • RESOURCES
    • Columns
      • Did you know?
      • Distribution Dive
      • Formulating With Mike
      • Innovation Insights
      • Powder Coating Perspectives
      • TiO2 Insider
    • Blogs
      • Editor's Viewpoint
      • Industry Insights
    • Coatings Supplier Handbook
    • COAT-IT! Podcast
    • Videos
    • PCI Store
    • eBooks
    • Sponsor Insights
  • EMAGAZINE
    • eMagazine
    • Archive Issues
    • Editorial Advisory Board
    • CONTACT
    • Advertise
  • JOIN!
Home » Keywords: » hardeners

Items Tagged with 'hardeners'

ARTICLES

Pflaumer logo

Pflaumer Brothers Targets Epoxy Flow and Finish With New Hardener

July 15, 2026
No Comments

The low-viscosity curing agent is designed for high-solids and solvent-free systems requiring medium cure, color stability and chemical resistance.


Read More
Pflaumer logo

Epoxy Co-Hardener and Accelerator for Ambient-Cure Systems

March 16, 2026
No Comments

This co-hardener and accelerator improves cure speed and control in ambient-cure epoxy systems for coatings, composites and electrical applications.


Read More
Novel Epoxy-Cure Hardener Sets New Industry Standard in Ultra-Fast Curing for Protective Coatings.jpg

Novel Epoxy-Cure Hardener Sets New Industry Standard in Ultra-Fast Curing for Protective Coatings

April 16, 2024
No Comments

The new high-functional aliphatic amine hardener is designed for plural component spray applications.


Read More
pci0623-Evonik-1372277590-1170.jpg

New Insights into Coating Additives to Improve Durability of Waterborne Coatings

Ali Javadi Jim Reader Maria Nargiello Marco Heuer Roger Reinartz
June 5, 2023
10 Comments

Abrasion is one of the most important defects that deteriorates the durability of coatings. The goal of the research presented in this article was to achieve a good understanding of the effects of coating additives on the abrasion resistance of waterborne coatings.


Read More
pci0423-Westlake-1164053857-1170.jpg

Lower Yellowing Epoxy System for Improved Sustainability of Concrete Coatings

Matthew Sumpter Mingbo He Dan Weinmann
April 6, 2023
No Comments

This article makes the case for a single coating layer system to replace two-coat systems for concrete coatings, claiming superior hardness and abrasion resistance as well as comparable adhesion to wet or dry concrete and equivalent chemical resistance.


Read More
ask-joe-powder-feature-1170.jpg

Ask Joe Powder: Is There Any Way to Reduce the Hardness of a Powder Coating?

Kevin Biller
March 21, 2023
One Comment

A reader from Vietnam asks Joe if there is a way to reduce the hardness of powder coatings. She is using a polyester resin for a powder coating with a pencil hardness of 3H. However, her customer requires 1H hardness.



Read More
evonik

Heat-Stable Hardener from Evonik

February 1, 2022
No Comments
TEGO Cure 100 hardener ensures that the coating cures at room temperature, eliminating the need for energy-intensive drying in the oven, while the surface is heat-stable up to 650 °C during application.
Read More

BASF Increases Production Capacity for Basonat Hardeners

May 15, 2016
No Comments

BASF is investing to expand its existing production facilities for Basonat® hardeners at its Ludwigshafen, Germany, site, significantly increasing its local production capacity.


Read More

Additives for Adhesives and Sealants

Incorez
June 1, 2013
No Comments
Incorez STP is a silane-terminated polyurethane prepolymer that can be formulated into sealants and adhesives, providing bubble-free films with good elastic properties.
Read More
advertisement

Polyisocyanate

January 4, 2012
No Comments
Easaqua™ X L 600 polyisocyanate provides easy dispersibility and improved humidity resistance in waterborne polyurethane coatings and further solutions for environmentally friendly coatings.


Read More
Manage My Account
  • Join Paint & Coatings Industry
  • Manage My Preferences
  • Customer Service

More Videos

Popular Stories

Mergers and aquisitions

BASF Ends Evonik Takeover Pursuit

Breaking News

H.B. Fuller to Close Seven Sites in Supply-Chain Overhaul

AkzoNobel Axalta

EU Clears $25B Akzo-Axalta Merger with One Big Condition

Events

December 2, 2026

Self-Activated Binder Technology: A New Path to Tin-Free Polyurethane Coatings

Through examples from protective and general industrial coating applications, attendees will learn how these innovative technologies can help maintain, and in some cases improve, coating performance while supporting safer, more sustainable formulations that align with evolving regulatory expectations

December 10, 2026

PC Academy: Waterborne Polymers and Film Formation

The trend towards waterborne polymers in the paint and coatings industry is clear; highlighting their environmentally friendly nature, regulatory considerations, growing market demand, and meeting sustainability goals.

View All Submit An Event

Products

Powder Coatings - Foundation for the Novice Formulator (ebook)

Powder Coatings - Foundation for the Novice Formulator (ebook)

See More Products
PCI news now promo ad

Keep the info flowing with our eNewsletters!

Get the latest industry updates tailored your way.

JOIN TODAY!
  • RESOURCES
    • Advertise
    • Contact Us
    • Directories
    • Store
    • Manufacturing Division
  • JOIN TODAY
    • Create Account
    • eMagazine
    • Newsletters
    • Customer Service
    • Manage Preferences
  • SERVICES
    • Marketing Services
    • Reprints
    • Market Research
    • List Rental
    • Survey & Sample
  • STAY CONNECTED
    • LinkedIn
    • Facebook
    • Youtube
    • X (Twitter)
  • PRIVACY
    • PRIVACY POLICY
    • TERMS & CONDITIONS
    • DO NOT SELL MY PERSONAL INFORMATION
    • PRIVACY REQUEST
    • ACCESSIBILITY

Copyright ©2026. All Rights Reserved BNP Media, Inc. and BNP Media II, LLC.

Design, CMS, Hosting & Web Development :: ePublishing