Painting & Coating Industry (PCI) logo Powder coating summit logo
search
cart
facebook twitter linkedin youtube
  • Sign In
  • Join Today
  • Sign Out
  • My Account
Painting & Coating Industry (PCI) logo Powder coating summit logo
  • NEWS
    • Latest News
    • PCI News Now
    • Market Trends & Reports
    • Finishing News
    • Price Alerts
    • Global Top 10/ PCI 25
  • PRODUCTS
    • Product News
    • Featured Products
    • Must See Products and Services
  • MATERIALS
    • Additives
    • Resins/Polymers
    • Pigments
    • Equipment
    • Distributors
  • TECHNOLOGIES
    • Adhesives
    • Architectural Coatings
    • Finishing Articles
    • Finishing Technologies
    • Finishing Equipment
    • Industrial Coatings
    • Nanotechnology
    • Powder Coatings
    • Solventborne
    • Special Purpose Coatings
    • Sustainability
    • UV Coatings
    • Waterborne
  • EVENTS
    • Coatings Trends & Technologies Summit
    • Paint and Coatings Academy
    • Webinars
    • Calendar of Events
    • Lifetime Achievement Award
  • DIRECTORIES
    • Buyer's Guide
    • Equipment Directory
    • Materials Directory
  • RESOURCES
    • Columns
      • Did you know?
      • Distribution Dive
      • Formulating With Mike
      • Innovation Insights
      • Powder Coating Perspectives
      • TiO2 Insider
    • Blogs
      • Editor's Viewpoint
      • Industry Insights
    • Coatings Supplier Handbook
    • COAT-IT! Podcast
    • Videos
    • PCI Store
    • eBooks
    • Sponsor Insights
  • EMAGAZINE
    • eMagazine
    • Archive Issues
    • Editorial Advisory Board
    • CONTACT
    • Advertise
  • JOIN!
Breaking NewsIndustry News

EPA Proposes Reporting and Record-Keeping Requirements on Nanoscale Materials

April 10, 2015

WASHINGTON D.C. – The U.S. Environmental Protection Agency (EPA) is proposing one-time reporting and recordkeeping requirements on nanoscale chemical substances in the marketplace.

“Nanotechnology holds great promise for improving products, from TVs and vehicles to batteries and solar panels,” said Jim Jones, EPA’s Assistant Administrator for Chemical Safety and Pollution Prevention. “We want to continue to facilitate the trend toward this important technology. Today’s action will ensure that EPA also has information on nano-sized versions of chemicals that are already in the marketplace.”

EPA currently reviews new chemical substances manufactured or processed as nanomaterials prior to introduction into the marketplace to ensure that they are safe. For the first time, the agency is proposing to use the Toxic Substances Control Act (TSCA) to collect existing exposure and health and safety information on chemicals currently in the marketplace when manufactured or processed as nanoscale materials. The proposal will require one-time reporting from companies that manufacture or process chemical substances as nanoscale materials.

The companies will notify EPA of certain information, including specific chemical identity; production volume; methods of manufacture including processing, use, exposure, and release information; and available health and safety data.

Nanoscale materials have special properties related to their small size such as greater strength and lighter weight, however, they may take on different properties than their conventionally sized counterpart. The proposal is not intended to conclude that nanoscale materials will cause harm to human health or the environment. Rather, EPA would use the information gathered to determine if any further action under the TSCA, including additional information collection, is needed.

The proposed reporting requirements are being issued under the authority of section 8(a) under TSCA. The agency is requesting public comment on the proposed reporting and record-keeping requirements 90 days from publication in the Federal Register. EPA also anticipates holding a public meeting during the comment period. The time and place of the meeting will be announced on EPA’s web page.

Additional information and a fact sheet on the specifics of the proposed rule and what constitutes a nanoscale chemical material can be found at www.epa.gov/oppt/nano.   

KEYWORDS: Environmental Protection Agency nanotechnology nanotechnology regulation

Share This Story

Looking for a reprint of this article?
From high-res PDFs to custom plaques, order your copy today!

Recommended Content

JOIN TODAY
to unlock your recommendations.

Already have an account? Sign In

  • Double exposure of creative chemistry concept on laptop background, research and development concept

    Inside the AI Shift in Coatings

    Industry leaders share real-world examples of how AI is...
    Paint and Coating Pigments
    By: PCI Editorial Staff
  • Global Top 10 and PCI Logo

    2026 Global Top 10: Top Paint and Coatings Companies

    See how the world’s largest paint and coatings companies...
    Global Top 10 and PCI 25
    By: Courtney Bassett
  • The 2026 PCI 25

    2026 PCI 25: Top Paint and Coatings Companies

    See how North America's largest paint and coatings...
    Global Top 10 and PCI 25
    By: Courtney Bassett
You must login or register in order to post a comment.

Report Abusive Comment

Manage My Account
  • Join Paint & Coatings Industry
  • Manage My Preferences
  • Customer Service

More Videos

Popular Stories

Mergers and aquisitions

BASF Ends Evonik Takeover Pursuit

Breaking News

H.B. Fuller to Close Seven Sites in Supply-Chain Overhaul

AkzoNobel Axalta

EU Clears $25B Akzo-Axalta Merger with One Big Condition

Events

December 2, 2026

Self-Activated Binder Technology: A New Path to Tin-Free Polyurethane Coatings

Through examples from protective and general industrial coating applications, attendees will learn how these innovative technologies can help maintain, and in some cases improve, coating performance while supporting safer, more sustainable formulations that align with evolving regulatory expectations

December 10, 2026

PC Academy: Waterborne Polymers and Film Formation

The trend towards waterborne polymers in the paint and coatings industry is clear; highlighting their environmentally friendly nature, regulatory considerations, growing market demand, and meeting sustainability goals.

View All Submit An Event

Products

Powder Coatings - Foundation for the Novice Formulator (ebook)

Powder Coatings - Foundation for the Novice Formulator (ebook)

See More Products
PCI news now promo ad

Related Articles

  • EPA Proposes Expansion of Reporting Requirements

    See More
  • Plaque sign on the outside of the United States Environmental Protection Agency

    EPA Proposes Changes to PFAS Reporting Requirements

    See More
  • Nanoscale Materials Grow With the Flow

    See More
×

Keep the info flowing with our eNewsletters!

Get the latest industry updates tailored your way.

JOIN TODAY!
  • RESOURCES
    • Advertise
    • Contact Us
    • Directories
    • Store
    • Manufacturing Division
  • JOIN TODAY
    • Create Account
    • eMagazine
    • Newsletters
    • Customer Service
    • Manage Preferences
  • SERVICES
    • Marketing Services
    • Reprints
    • Market Research
    • List Rental
    • Survey & Sample
  • STAY CONNECTED
    • LinkedIn
    • Facebook
    • Youtube
    • X (Twitter)
  • PRIVACY
    • PRIVACY POLICY
    • TERMS & CONDITIONS
    • DO NOT SELL MY PERSONAL INFORMATION
    • PRIVACY REQUEST
    • ACCESSIBILITY

Copyright ©2026. All Rights Reserved BNP Media, Inc. and BNP Media II, LLC.

Design, CMS, Hosting & Web Development :: ePublishing