Painting & Coating Industry (PCI) logo Powder coating summit logo
search
cart
facebook twitter linkedin youtube
  • Sign In
  • Join Today
  • Sign Out
  • My Account
Painting & Coating Industry (PCI) logo Powder coating summit logo
  • NEWS
    • Latest News
    • PCI News Now
    • Market Trends & Reports
    • Finishing News
    • Price Alerts
    • Global Top 10/ PCI 25
  • PRODUCTS
    • Product News
    • Featured Products
    • Must See Products and Services
  • MATERIALS
    • Additives
    • Resins/Polymers
    • Pigments
    • Equipment
    • Distributors
  • TECHNOLOGIES
    • Adhesives
    • Architectural Coatings
    • Finishing Articles
    • Finishing Technologies
    • Finishing Equipment
    • Industrial Coatings
    • Nanotechnology
    • Powder Coatings
    • Solventborne
    • Special Purpose Coatings
    • Sustainability
    • UV Coatings
    • Waterborne
  • EVENTS
    • Coatings Trends & Technologies Summit
    • Paint and Coatings Academy
    • Webinars
    • Calendar of Events
    • Lifetime Achievement Award
  • DIRECTORIES
    • Buyer's Guide
    • Equipment Directory
    • Materials Directory
  • RESOURCES
    • Columns
      • Did you know?
      • Distribution Dive
      • Formulating With Mike
      • Innovation Insights
      • Powder Coating Perspectives
      • TiO2 Insider
    • Blogs
      • Editor's Viewpoint
      • Industry Insights
    • Coatings Supplier Handbook
    • COAT-IT! Podcast
    • Videos
    • PCI Store
    • eBooks
    • Sponsor Insights
  • EMAGAZINE
    • eMagazine
    • Archive Issues
    • Editorial Advisory Board
    • CONTACT
    • Advertise
  • JOIN!
Industry News

Stanford Engineers Invent Transparent Coating That Cools Solar Cells to Boost Efficiency

September 27, 2015

PALO ALTO, CA - Every time you stroll outside you emit energy into the universe, as heat from the top of your head radiates into space as infrared light.

Now three Stanford engineers have developed a technology that improves on solar panel performance by exploiting this basic phenomenon. Their invention shunts away the heat generated by a solar cell under sunlight and cools it in a way that allows it to convert more photons into electricity.

The work by Shanhui Fan, a Professor of Electrical Engineering at Stanford, Research Associate Aaswath P. Raman and doctoral candidate Linxiao Zhu is described in the current issue of Proceedings of the National Academy of Sciences.

The group's discovery, tested on a Stanford rooftop, addresses a problem that has long bedeviled the solar industry: The hotter solar cells get, the less efficient they become at converting the photons in light into useful electricity.

The Stanford solution is based on a thin, patterned silica material laid on top of a traditional solar cell. The material is transparent to the visible sunlight that powers solar cells, but captures and emits thermal radiation, or heat, from infrared rays.

"Solar arrays must face the sun to function, even though that heat is detrimental to efficiency," Fan said. "Our thermal overlay allows sunlight to pass through, preserving or even enhancing sunlight absorption, but it also cools the cell by radiating the heat out and improving the cell efficiency."

A Cool Way to Improve Solar Efficiency

In 2014, the same trio of inventors developed an ultrathin material that radiated infrared heat directly back toward space without warming the atmosphere. They presented that work in Nature, describing it as "radiative cooling" because it shunted thermal energy directly into the deep, cold void of space.

In their new paper, the researchers applied that work to improve solar array performance when the sun is beating down.

The Stanford team tested their technology on a custom-made solar absorber – a device that mimics the properties of a solar cell without producing electricity – covered with a micron-scale pattern designed to maximize the capability to dump heat, in the form of infrared light, into space. Their experiments showed that the overlay allowed visible light to pass through to the solar cells, but that it also cooled the underlying absorber by as much as 23 °F.

For a typical crystalline silicon solar cell with an efficiency of 20 percent, 23 °F of cooling would improve absolute cell efficiency by over 1 percent, a figure that represents a significant gain in energy production.

The researchers said the new transparent thermal overlays work best in dry, clear environments, which are also preferred sites for large solar arrays. They believe they can scale things up so commercial and industrial applications are feasible, perhaps using nanoprint lithography, which is a common technique for producing nanometer-scale patterns.

"That's not necessarily the only way," said Raman, a co-first-author of the paper. "New techniques and machines for manufacturing these kinds of patterns will continue to advance. I'm optimistic."

Cooler Cars

Zhu said the technology has significant potential for any outdoor device or system that demands cooling but requires the preservation of the visible spectrum of sunlight for either practical or aesthetic reasons.

"Say you have a car that is bright red," Zhu said. "You really like that color, but you'd also like to take advantage of anything that could aid in cooling your vehicle during hot days. Thermal overlays can help with passive cooling, but it's a problem if they're not fully transparent."

That's because the perception of color requires objects to reflect visible light, so any overlay would need to be transparent, or else tuned such that it would absorb only light outside the visible spectrum.

"Our photonic crystal thermal overlay optimizes use of the thermal portions of the electromagnetic spectrum without affecting visible light," Zhu said, "so you can radiate heat efficiently without affecting color."

KEYWORDS: Research and Development Solar Coatings

Share This Story

Looking for a reprint of this article?
From high-res PDFs to custom plaques, order your copy today!

Recommended Content

JOIN TODAY
to unlock your recommendations.

Already have an account? Sign In

  • Double exposure of creative chemistry concept on laptop background, research and development concept

    Inside the AI Shift in Coatings

    Industry leaders share real-world examples of how AI is...
    Architectural Coatings
    By: PCI Editorial Staff
  • Global Top 10 and PCI Logo

    2026 Global Top 10: Top Paint and Coatings Companies

    See how the world’s largest paint and coatings companies...
    Global Top 10 and PCI 25
    By: Courtney Bassett
  • The 2026 PCI 25

    2026 PCI 25: Top Paint and Coatings Companies

    See how North America's largest paint and coatings...
    Global Top 10 and PCI 25
    By: Courtney Bassett
You must login or register in order to post a comment.

Report Abusive Comment

Manage My Account
  • Join Paint & Coatings Industry
  • Manage My Preferences
  • Customer Service

More Videos

Popular Stories

Mergers and aquisitions

BASF Ends Evonik Takeover Pursuit

Breaking News

H.B. Fuller to Close Seven Sites in Supply-Chain Overhaul

AkzoNobel Axalta

EU Clears $25B Akzo-Axalta Merger with One Big Condition

Events

December 2, 2026

Self-Activated Binder Technology: A New Path to Tin-Free Polyurethane Coatings

Through examples from protective and general industrial coating applications, attendees will learn how these innovative technologies can help maintain, and in some cases improve, coating performance while supporting safer, more sustainable formulations that align with evolving regulatory expectations

December 10, 2026

PC Academy: Waterborne Polymers and Film Formation

The trend towards waterborne polymers in the paint and coatings industry is clear; highlighting their environmentally friendly nature, regulatory considerations, growing market demand, and meeting sustainability goals.

View All Submit An Event

Products

Powder Coatings - Foundation for the Novice Formulator (ebook)

Powder Coatings - Foundation for the Novice Formulator (ebook)

See More Products
PCI news now promo ad

Related Articles

  • New Nanoparticles Make Solar Cells Cheaper to Manufacture

    See More
  • GettyImages-1266932482-1170.jpg

    New Coating Chemistries Boost Efficiency for Automakers

    See More
  • Jotun’s Hull Performance Solutions

    PETRONAS LNG Vessels to Cut Emissions and Boost Efficiency With Jotun Coatings

    See More

Events

View AllSubmit An Event
  • March 31, 2026

    Durability by Design: Waterborne Concrete Coatings that Protect, Beautify, and Extend Service Life

    On Demand Attend this webinar to understand how protecting concrete enables lifespan extension and reduction of the CO₂ emissions associated with premature repair or replacement.
View AllSubmit An Event
×

Keep the info flowing with our eNewsletters!

Get the latest industry updates tailored your way.

JOIN TODAY!
  • RESOURCES
    • Advertise
    • Contact Us
    • Directories
    • Store
    • Manufacturing Division
  • JOIN TODAY
    • Create Account
    • eMagazine
    • Newsletters
    • Customer Service
    • Manage Preferences
  • SERVICES
    • Marketing Services
    • Reprints
    • Market Research
    • List Rental
    • Survey & Sample
  • STAY CONNECTED
    • LinkedIn
    • Facebook
    • Youtube
    • X (Twitter)
  • PRIVACY
    • PRIVACY POLICY
    • TERMS & CONDITIONS
    • DO NOT SELL MY PERSONAL INFORMATION
    • PRIVACY REQUEST
    • ACCESSIBILITY

Copyright ©2026. All Rights Reserved BNP Media, Inc. and BNP Media II, LLC.

Design, CMS, Hosting & Web Development :: ePublishing