Painting & Coating Industry (PCI) logo Powder coating summit logo
search
cart
facebook twitter linkedin youtube
  • Sign In
  • Create Account
  • Sign Out
  • My Account
Painting & Coating Industry (PCI) logo Powder coating summit logo
  • NEWS
    • Latest News
    • Market Trends & Reports
    • Finishing News
    • Price Alerts
    • Subscribe to Newsletters
    • Global Top 10/ PCI 25
    • Weekly Featured Article
  • PRODUCTS
    • Product News
    • Featured Products
    • Must See Products and Services
  • MATERIALS
    • Additives
    • Resins/Polymers
    • Pigments
    • Equipment
    • Distributors
  • TECHNOLOGIES
    • Adhesives
    • Architectural Coatings
    • Finishing Articles
    • Finishing Technologies
    • Finishing Equipment
    • Industrial Coatings
    • Nanotechnology
    • Powder Coatings
    • Solventborne
    • Special Purpose Coatings
    • Sustainability
    • UV Coatings
    • Waterborne
  • RESOURCES
    • Columns
      • Did you know?
      • Distribution Dive
      • Formulating With Mike
      • Innovation Insights
      • Powder Coating Perspectives
      • TiO2 Insider
    • Blogs
      • Editor's Viewpoint
      • Industry Insights
    • Coatings Supplier Handbook
    • Podcasts and Videos
      • COAT-IT! Podcast
      • Videos/PCI TV
    • PCI Store
    • Classifieds
    • eBooks
    • Sponsor Insights
    • White Papers
    • COATLE Word Game
  • EVENTS
    • Coatings Trends & Technologies Summit
    • Paint and Coatings Academy
    • Webinars
    • Calendar of Events
    • Lifetime Achievement Award
  • DIRECTORIES
    • Buyer's Guide
    • Equipment Directory
    • Materials Directory
  • EMAGAZINE
    • Current Issue
    • eMagazine Archive
    • China Issue Archive
    • Editorial Advisory Board
  • CONTACT
    • Contact Us
    • Advertise
    • Subscribe to eMagazine
    • Subscribe to Newsletters
  • SIGN UP!
Company NewsEU Company News

Evonik Bundles Its Expertise in Crosslinking Technology

July 9, 2017

PARSIPPANY, NJ – Evonik Industries AG announced that it has combined its isophorone chemistry and epoxy curing agents business in the new Crosslinkers Business Line as of July 1, 2017. The newly formed business line, headed by Min Chong, will be part of the Resource Efficiency Segment.

With the acquisition of Air Products' epoxy curing agents business and Evonik's long-time experience in isophorone chemistry, Evonik has a very broad technology platform and expertise in crosslinker technology.

The new Crosslinkers Business Line offers a broad range of products and competencies for coatings and adhesives, civil engineering as well as for high-performance elastomers and composites.

Evonik is the pioneer in isophorone chemistry and covers the entire value chain: isophorone, diamine, as well as di-isocyanate and polyisocyanate. Additionally, the product portfolio contains a full toolbox of amine curing agents for ambient and heat-cure applications. The products are mainly used in industrial applications due to their mechanical strength, durability, chemical resistance and excellent adhesion properties.

“Combining both businesses into one new unit gives Evonik the chance to offer a variety of products for epoxy and polyurethane applications under one roof now, be it basic amines, isocyanate monomers, polyisocyanates or formulated epoxy hardeners,” said Claus Rettig, Chairman of the Board of Management, Evonik Resource Efficiency GmbH.

Production facilities in Europe, North America, and Asia ensure optimal proximity to markets and customers and open up attractive growth opportunities.

The Crosslinkers portfolio includes the following brands: Amicure®, Ancamide®, Ancamine®, Ancarez®, Ancatherm®, Anquamine®, Anquawhite®, Curezol®, Dicyanex®, Eplink™, Epodil®, Hybridur®, Imicure®, Nourybond®, Sunmide®, VESTAGON®, VESTAMIN®, VESTANAT® VESTASOL®.

For more information, visit www.evonik.com/crosslinkers.

KEYWORDS: crosslinkers curing agents for coatings

Share This Story

Looking for a reprint of this article?
From high-res PDFs to custom plaques, order your copy today!

Recommended Content

JOIN TODAY
to unlock your recommendations.

Already have an account? Sign In

  • Double exposure of creative chemistry concept on laptop background, research and development concept

    Inside the AI Shift in Coatings

    Industry leaders share real-world examples of how AI is...
    Paint and Coatings Additives
    By: PCI Editorial Staff
  • Global Top 10 and PCI Logo

    2026 Global Top 10: Top Paint and Coatings Companies

    See how the world’s largest paint and coatings companies...
    Global Top 10 and PCI 25
    By: Courtney Bassett
  • The 2026 PCI 25

    2026 PCI 25: Top Paint and Coatings Companies

    See how North America's largest paint and coatings...
    Global Top 10 and PCI 25
    By: Courtney Bassett
You must login or register in order to post a comment.

Report Abusive Comment

Manage My Account
  • eMagazine
  • Newsletters
  • Online Registration
  • Subscription Customer Service

More Videos

Sponsored Content

Sponsored Content is a special paid section where industry companies provide high quality, objective, non-commercial content around topics of interest to the PCI audience. All Sponsored Content is supplied by the advertising company and any opinions expressed in this article are those of the author and not necessarily reflect the views of PCI or its parent company, BNP Media. Interested in participating in our Sponsored Content section? Contact your local rep!

close
  • wooden kitchen set and shelving
    Sponsored bySirca North America

    Leveraging Coatings to Meet ESG Goals in Manufacturing

  • man woodworking in workshop
    Sponsored byGemini Industries, Inc.

    Waterborne Coatings Aren't the Future -- They're the New Performance Benchmark

Popular Stories

The 2026 PCI 25

2026 PCI 25: Top Paint and Coatings Companies

USA election voters in red and blue to represent democrats and republicans

The AkzoNobel-Axalta Vote is Over. What Will Regulators Ask Next?

Axalta Coating Systems Headquarters in Philadelphia, PA

Axalta Sets Two Records Ahead of Aug. 5 Merger Vote

The PCI 25 Annual Revenue Rankings

Events

September 15, 2026

Coatings Trends & Technologies Summit

The Coatings Trends & Technologies (CTT) Summit is an annual conference for both liquid and powder coatings formulators and manufacturers to discuss innovations in coatings technology. This event combines high-quality technical presentations, a resource-rich exhibit hall, and dedicated networking opportunities to connect scientific minds, foster innovation, and cultivate game-changing new ideas!

January 1, 2030

Webinar Sponsorship Information

For webinar sponsorship information, visit www.bnpevents.com/webinars or email webinars@bnpmedia.com.

View All Submit An Event

Products

Advanced Coating Materials

Advanced Coating Materials

See More Products
PCI Coat It! Podcast

Related Articles

  • AmCoat Lead Image.jpg

    Self-Crosslinking Polymer Technology for Longer-Lasting and Vibrant Colors

    See More
  • Henkel Adhesive Technologies Expands Expertise in Surface Treatment

    See More
  • Siltech Highlights Expertise in Reactive Silicones

    See More

Related Products

See More Products
  • laser tech.jpg

    Laser Technology: Applications in Adhesion and Related Areas

  • Cold Spray Technology

  • organic coatings.jpg

    Organic Coatings: Science and Technology, 4th Edition

See More Products

Events

View AllSubmit An Event
  • April 28, 2026

    Next Gen Dispersion Technology in Paint Production: Driving Higher Quality at Lower Costs

    On Demand Join this webinar to see how manufacturers reduce costs, energy use, raw materials, labor, and floor space while improving quality.
View AllSubmit An Event

Related Directories

  • Evonik Corp.

    The Coating Additives business line of Evonik offers a broad portfolio of products including specialty additives, matting agents, rheology modifiers, specialty fillers, co-binders and silicone resins. In addition to our traditional products, our multifunctional COATINO® service platform provides product recommendations, detailed technical information, and more at the quick click of a button.
  • Evonik Corp.

    The Coating Additives business line of Evonik offers a broad portfolio of high-performance specialty additives, silicas, co-binders, and silicone resins for the coatings and inks industries. In addition to our traditional product offerings, our COATINO® service platforms provide one-of-a-kind digital formulation support and interactive knowledge-sharing.
×

Keep the info flowing with our eNewsletters!

Get the latest industry updates tailored your way.

JOIN TODAY!
  • RESOURCES
    • Advertise
    • Contact Us
    • Directories
    • Store
    • Want More
    • Manufacturing Division
  • SIGN UP TODAY
    • Create Account
    • eMagazine
    • Newsletters
    • Customer Service
    • Manage Preferences
  • SERVICES
    • Marketing Services
    • Reprints
    • Market Research
    • List Rental
    • Survey & Sample
  • STAY CONNECTED
    • LinkedIn
    • Facebook
    • Youtube
    • X (Twitter)
  • PRIVACY
    • PRIVACY POLICY
    • TERMS & CONDITIONS
    • DO NOT SELL MY PERSONAL INFORMATION
    • PRIVACY REQUEST
    • ACCESSIBILITY

Copyright ©2026. All Rights Reserved BNP Media, Inc. and BNP Media II, LLC.

Design, CMS, Hosting & Web Development :: ePublishing