Painting & Coating Industry (PCI) logo Powder coating summit logo
search
cart
facebook twitter linkedin youtube
  • Sign In
  • Join Today
  • Sign Out
  • My Account
Painting & Coating Industry (PCI) logo Powder coating summit logo
  • NEWS
    • Latest News
    • PCI News Now
    • Market Trends & Reports
    • Finishing News
    • Price Alerts
    • Global Top 10/ PCI 25
  • PRODUCTS
    • Product News
    • Featured Products
    • Must See Products and Services
  • MATERIALS
    • Additives
    • Resins/Polymers
    • Pigments
    • Equipment
    • Distributors
  • TECHNOLOGIES
    • Adhesives
    • Architectural Coatings
    • Finishing Articles
    • Finishing Technologies
    • Finishing Equipment
    • Industrial Coatings
    • Nanotechnology
    • Powder Coatings
    • Solventborne
    • Special Purpose Coatings
    • Sustainability
    • UV Coatings
    • Waterborne
  • EVENTS
    • Coatings Trends & Technologies Summit
    • Paint and Coatings Academy
    • Webinars
    • Calendar of Events
    • Lifetime Achievement Award
  • DIRECTORIES
    • Buyer's Guide
    • Equipment Directory
    • Materials Directory
  • RESOURCES
    • Columns
      • Did you know?
      • Distribution Dive
      • Formulating With Mike
      • Innovation Insights
      • Powder Coating Perspectives
      • TiO2 Insider
    • Blogs
      • Editor's Viewpoint
      • Industry Insights
    • Coatings Supplier Handbook
    • COAT-IT! Podcast
    • Videos
    • PCI Store
    • eBooks
    • Sponsor Insights
  • EMAGAZINE
    • eMagazine
    • Archive Issues
    • Editorial Advisory Board
    • CONTACT
    • Advertise
  • JOIN!
Company News

AGM Advances Applications for Water-Based Anti-Corrosion Coatings

August 2, 2019

REDCAR, UK — Applied Graphene Materials (AGM), producer of specialty graphene materials, has achieved significant technological progress (patent pending) on the deployment of graphene into water-based coatings to enhance their barrier properties.

Water-based coating development remains a focus for industry formulators. This push is driven by the continuing tightening of regulations brought in to lessen the detrimental impact that solvent- based coatings have on both worker health and the environment. As the technology for water-based coatings continues to evolve, one of the key challenges that remains is to significantly improve their anti-corrosion performance. In doing so, this will fully extend their use away from decorative applications into broader industrial protective coatings.

Over recent years AGM has proven the outstanding barrier and anti-corrosion performance gains possible by incorporating graphene into solvent-based coating systems using its Genable® dispersion technology. This has been demonstrated with several commercial products reaching industrial end-user markets. However, effective incorporation of graphene into water-based systems has previously proven more problematic due to interrelated issues around materials compatibility and film formation.

This water-based breakthrough is again based on AGM's platform Genable technology, a range of master dispersions that are designed to facilitate the easy incorporation of graphene into coating formulations and existing processes. Genable dispersions are fully scalable industrial products and, based on initial findings, the addition levels required to significantly enhance anti-corrosion performance in water-based systems are low enough to ensure commercial viability, even in light industrial applications.

Adrian Potts, CEO of Applied Graphene Materials, said, “A key driver for coatings developers to upgrade their product formulations is increasing regulatory pressure to improve the environmental impact and safety of their products. This is why AGM is working to replicate the success we have already achieved with the incorporation of our Genable products into solvent-based products with its incorporation into water-based products. We are delighted to be able to present significant technological progress to our customers, reaffirming AGM as the leader in the development of cutting-edge graphene applications tailored to add significant value for paints and coatings manufacturers.”

While the findings being shared publicly are in a commercial acrylic DTM (direct-to-metal) coating, AGM believes that water-based Genable technology could, with considered formulating, be equally well adopted into epoxy chemistries and likewise into more complex formulated primer systems.

AGM remains the industry leader for graphene exploitation into the global paints and coatings industry, boasting a highly experienced formulations and applications team, supported by a well-equipped product development and characterization laboratory and production capability for consistent manufacturing.

KEYWORDS: graphene in coatings waterborne technology

Share This Story

Looking for a reprint of this article?
From high-res PDFs to custom plaques, order your copy today!

Recommended Content

JOIN TODAY
to unlock your recommendations.

Already have an account? Sign In

  • Double exposure of creative chemistry concept on laptop background, research and development concept

    Inside the AI Shift in Coatings

    Industry leaders share real-world examples of how AI is...
    Industrial Coatings
    By: PCI Editorial Staff
  • Global Top 10 and PCI Logo

    2026 Global Top 10: Top Paint and Coatings Companies

    See how the world’s largest paint and coatings companies...
    Global Top 10 and PCI 25
    By: Courtney Bassett
  • The 2026 PCI 25

    2026 PCI 25: Top Paint and Coatings Companies

    See how North America's largest paint and coatings...
    Global Top 10 and PCI 25
    By: Courtney Bassett
You must login or register in order to post a comment.

Report Abusive Comment

Manage My Account
  • Join Paint & Coatings Industry
  • Manage My Preferences
  • Customer Service

More Videos

Popular Stories

Mergers and aquisitions

BASF Ends Evonik Takeover Pursuit

Breaking News

H.B. Fuller to Close Seven Sites in Supply-Chain Overhaul

AkzoNobel Axalta

EU Clears $25B Akzo-Axalta Merger with One Big Condition

Events

December 2, 2026

Self-Activated Binder Technology: A New Path to Tin-Free Polyurethane Coatings

Through examples from protective and general industrial coating applications, attendees will learn how these innovative technologies can help maintain, and in some cases improve, coating performance while supporting safer, more sustainable formulations that align with evolving regulatory expectations

December 10, 2026

PC Academy: Waterborne Polymers and Film Formation

The trend towards waterborne polymers in the paint and coatings industry is clear; highlighting their environmentally friendly nature, regulatory considerations, growing market demand, and meeting sustainability goals.

View All Submit An Event

Products

Powder Coatings - Foundation for the Novice Formulator (ebook)

Powder Coatings - Foundation for the Novice Formulator (ebook)

See More Products
PCI news now promo ad

Related Articles

  • corrosion

    Water-Based Anti-Corrosion Coating

    See More
  • corrosion

    AGM Receives U.K. Patent for Water-Based Corrosion Innovation

    See More
  • pci0322-Target-F1-1170.jpg

    Global Market for Anti-Corrosion Coatings

    See More

Related Directories

  • Eagle Specialty Products

    Eagle is an ISO-certified manufacturer specializing in high-performance color pigment dispersions for water-based, solvent-based, 100%-solids, and universal solvent-and-water applications. We also offer opportunities for customization and toll manufacturing, as well as hazardous and non-hazardous warehousing services for chemical companies. In addition, we have a highly efficient drumming operation for solvent and water-based products.
  • Eagle Specialty Products

    Serving industrial paint and coatings manufacturers since 1959, we specialize in creating advanced color pigment dispersions for water, solvent-based, and 100%-solids applications. We also offer opportunities for customization. As an ISO 9001:2015-certified company, our research and development team is equipped to create custom colorants and even toll manufacture product. Whether it's Conventional, Low-VOC, or Solvent-Free formulation, we can outfit you with the perfect solution.
×

Keep the info flowing with our eNewsletters!

Get the latest industry updates tailored your way.

JOIN TODAY!
  • RESOURCES
    • Advertise
    • Contact Us
    • Directories
    • Store
    • Manufacturing Division
  • JOIN TODAY
    • Create Account
    • eMagazine
    • Newsletters
    • Customer Service
    • Manage Preferences
  • SERVICES
    • Marketing Services
    • Reprints
    • Market Research
    • List Rental
    • Survey & Sample
  • STAY CONNECTED
    • LinkedIn
    • Facebook
    • Youtube
    • X (Twitter)
  • PRIVACY
    • PRIVACY POLICY
    • TERMS & CONDITIONS
    • DO NOT SELL MY PERSONAL INFORMATION
    • PRIVACY REQUEST
    • ACCESSIBILITY

Copyright ©2026. All Rights Reserved BNP Media, Inc. and BNP Media II, LLC.

Design, CMS, Hosting & Web Development :: ePublishing