Painting & Coating Industry (PCI) logo Powder coating summit logo
search
cart
facebook twitter linkedin youtube
  • Sign In
  • Create Account
  • Sign Out
  • My Account
Painting & Coating Industry (PCI) logo Powder coating summit logo
  • NEWS
    • Latest News
    • Market Trends & Reports
    • Finishing News
    • Price Alerts
    • Subscribe to Newsletters
    • Global Top 10/ PCI 25
    • Weekly Featured Article
    • COATLE Word Game
  • PRODUCTS
    • Product News
    • Featured Products
    • Must See Products and Services
  • MATERIALS
    • Additives
    • Resins/Polymers
    • Pigments
    • Equipment
    • Distributors
  • TECHNOLOGIES
    • Adhesives
    • Architectural Coatings
    • Finishing Articles
    • Finishing Technologies
    • Finishing Equipment
    • Industrial Coatings
    • Nanotechnology
    • Powder Coatings
    • Solventborne
    • Special Purpose Coatings
    • Sustainability
    • UV Coatings
    • Waterborne
  • RESOURCES
    • Columns
      • Did you know?
      • Distribution Dive
      • Formulating With Mike
      • Innovation Insights
      • Powder Coating Perspectives
      • TiO2 Insider
    • Blogs
      • Editor's Viewpoint
      • Industry Insights
    • Coatings Supplier Handbook
    • Podcasts and Videos
      • COAT-IT! Podcast
      • Videos/PCI TV
    • PCI Store
    • Classifieds
    • eBooks
    • Sponsor Insights
    • White Papers
    • COATLE Word Game
  • EVENTS
    • Coatings Trends & Technologies Summit
    • Paint and Coatings Academy
    • Webinars
    • Calendar of Events
    • Lifetime Achievement Award
  • DIRECTORIES
    • Buyer's Guide
    • Equipment Directory
    • Materials Directory
  • EMAGAZINE
    • Current Issue
    • eMagazine Archive
    • China Issue Archive
    • Editorial Advisory Board
  • CONTACT
    • Contact Us
    • Advertise
    • Subscribe to eMagazine
    • Subscribe to Newsletters
  • SIGN UP!
Special Purpose Coatings

Polymeric Repair and Protection Systems Save Steel Fabricator Millions

By Belzona
Polymeric Repair and Protection Systems Save Steel Fabricator Millions
Steelworks in Scunthorpe, UK.
Polymeric Repair and Protection Systems Save Steel Fabricator Millions
Gas pipeline damaged by erosion and corrosion.
Polymeric Repair and Protection Systems Save Steel Fabricator Millions
Gas pipeline after grit-blasting.
Polymeric Repair and Protection Systems Save Steel Fabricator Millions
Pits filled with epoxy repair mortar, Belzona 4154 (bulkfill resin).
Polymeric Repair and Protection Systems Save Steel Fabricator Millions
Final coat of stainless steel protective coating, Belzona 5811 (immersion grade).
Polymeric Repair and Protection Systems Save Steel Fabricator Millions
Polymeric Repair and Protection Systems Save Steel Fabricator Millions
Polymeric Repair and Protection Systems Save Steel Fabricator Millions
Polymeric Repair and Protection Systems Save Steel Fabricator Millions
Polymeric Repair and Protection Systems Save Steel Fabricator Millions
September 23, 2021

Over the course of several years, a steel fabricator in Scunthorpe, UK, has saved millions of pounds by deploying a series of polymeric repair and protection systems, including epoxy repair mortars and stainless steel protective coatings, on their gas pipeline.

 

Severe Pitting and Corrosion Damage

In 2016, after 45 years of service, the gas main was exhibiting severe pitting and corrosion damage. This was taking place at the four o’clock and eight o’clock positions on the 2.7-m-diameter pipeline, where a waterline between liquid and gas forms.

Having previously opted to replace the steel pipes, the client was looking for an alternative solution to this, bypassing the costly fees that replacement can incur. For each meter of pipeline replaced, the client paid £8,000. This meant that to replace the 90-m section, the cost was £720,000.

 

Short Time-Frame Allocated for Pipe Repairs

Independent Consultant, David Keen, said, “The whole site is completely reliant on this pipeline. As such, the site allocate just 14 days for its annual outage. This short timescale seriously limits the amount of maintenance work that can be carried out.”

He continued, “In previous years, contractors were only able to replace small amounts of pipeline within this timescale. It was clear that this method of pipe maintenance had serious limitations, not to mention the significant amount of capital required to completely replace the damaged areas.”

 

Specification of Repair Mortars and Stainless Steel Protective Coatings

Following an inspection carried out by Belzona, international manufacturers of polymeric repair composites and industrial protective coatings, a series of systems were specified. These included: Belzona 1151 (Smoothing Metal), Belzona 4151 (Magma-Quartz Resin), Belzona 4154 (Bulkfill Resin) and Belzona 5811 (Immersion Grade).

Not only could these systems offer outstanding repair and protection, but the savings the client would make by avoiding the need to replace the assets were huge – approximately 16 million pounds.

In addition, as the polymeric systems can be applied without the use of hot work, this further ensures that downtime is kept to an absolute minimum. Thus allowing the steelworks to make further savings by investing in the composite repair materials and industrial coatings.

 

Simple Application Procedure

First, the area was cleared of residue, grit-blasted, and then 150 mm x 150 mm plates were bonded over any holed areas using Belzona 1151. Heavily pitted areas were filled with Belzona 4151 or Belzona 4154 combined with kiln-dried sand.

Next, in order to provide complete corrosion protection for the heavily pitted and holed areas, two coats of Belzona 5811 (Immersion Grade) were applied at double the thickness to the substrate, giving a total thickness of 1000μm.
 

Contractor Wins National Award with Polymer Technology

Giving an overview of the scale of the project, David Keen said, “By using the polymer systems, this enabled the client to protect much larger sections of the pipeline than was previously possible. Usually, this amounted to 350m each year.”

He added, “However, in 2018 they protected a phenomenal 750-m stretch of the pipeline in just nine days. In fact, this application won the Contractor a National Award for the speed in which the repair was carried out, as well as the huge savings it allowed the client to make.”
 

Over 2 km of Epoxy Protection By 2022

Starting in 2016 through to 2020, Belzona materials have been deployed across the pipeline to combat the widespread corrosion. This totals 1,300 m, with a further 730 m of repairs scheduled for 2021 and 2022.

This repeat business is testament to the polymeric systems’ excellent corrosion protection characteristics, along with quick and easy application method. The combination of which will save the client millions of pounds by the end of 2022.

KEYWORDS: Epoxy Resins Protective Coatings

Share This Story

Looking for a reprint of this article?
From high-res PDFs to custom plaques, order your copy today!

Recommended Content

JOIN TODAY
to unlock your recommendations.

Already have an account? Sign In

  • pci1022-Kinaltek-Lead-1170.jpg

    A Novel Pigment Production Technology

    Following an extensive R&D program that demonstrated...
    Paint and Coating Pigments
    By: Jawad Haidar and Nitin Soni
  • pci global top 10

    2025 Global Top 10: Top Paint and Coatings Companies

    The following is PCI’s annual ranking of the top 10...
    Global Top 10 and PCI 25
    By: Courtney Bassett
  • 2025 pci 25

    2025 PCI 25: Top Paint and Coatings Companies

    PCI's annual ranking of the top 25 North American paint...
    Global Top 10 and PCI 25
    By: Courtney Bassett

Post a comment to this article

Report Abusive Comment

Manage My Account
  • eMagazine
  • Newsletters
  • Online Registration
  • Subscription Customer Service

More Videos

Sponsored Content

Sponsored Content is a special paid section where industry companies provide high quality, objective, non-commercial content around topics of interest to the PCI audience. All Sponsored Content is supplied by the advertising company and any opinions expressed in this article are those of the author and not necessarily reflect the views of PCI or its parent company, BNP Media. Interested in participating in our Sponsored Content section? Contact your local rep!

close
  • wooden kitchen set and shelving
    Sponsored bySirca North America

    Leveraging Coatings to Meet ESG Goals in Manufacturing

  • man woodworking in workshop
    Sponsored byGemini Industries, Inc.

    Waterborne Coatings Aren't the Future -- They're the New Performance Benchmark

  • colorful building exterior
    Sponsored byDow

    Insights into Exterior Architectural Coating Degradation: Bridging Accelerated and Natural Weathering

Popular Stories

Supply chain question and cargo piles up and piling shipping containers question concept

Energy Disruptions Begin to Hit Coatings Supply Chain

basf

BASF Coatings Names Incoming CEO Ahead of Separation

PPG announced the installation of a state-of-the-art pilot finishing line that features IPG’s PhotoniCURE™ laser curing system at its powder manufacturing and technical facility in Strongsville, Ohio.

PPG Tests Laser Curing for Powder Coatings

POB-Point-and-Shoot

PCI Buyers Guide

Submit a Request for Proposal (RFP) to suppliers of your choice with details on what you need with a click of a button

Start your RFP

Browse our Buyers Guide for manufacturers and distributors of all types of coatings products and much more!

Find Suppliers

Events

September 4, 2025

N-Butylpyrrolidone (NBP) as a Green Solvent to Replace N-Methylpyrrolidone (NMP) in Industrial Coating Applications

ON DEMAND: EPA published a regulation proposal around N-methylpyrrolidone (NMP) in June 2024 to ban or limit NMP in many applications, such as paints and coatings and their removers. N-butylpyrrolidone (NBP) is a powerful and versatile solvent for a variety of industries looking for alternatives to substance of very high concern (SVHC)-listed solvents.

April 28, 2026

Next Gen Dispersion Technology in Paint Production: Driving Higher Quality at Lower Costs

Join this webinar to see how manufacturers reduce costs, energy use, raw materials, labor, and floor space while improving quality.

View All Submit An Event

Poll

Longest-running laboratory experiment

What is the longest-running laboratory experiment?
View Results Poll Archive

Products

Automotive Paints and Coatings, 2nd Edition

Now in its second edition and still the only book of its kind, this is an authoritative treatment of all stages of the coating process.

See More Products
Register for webinar: Next-Gen Dispersion Technology in Paint Production

Related Articles

  • Image 1.png

    Safeguarding Wind Turbine Blades with Polymeric Technology Supports a Net-Zero Future

    See More
  • pci1017-Clariant-157683862-900.jpg

    Fire Protection on Steel and Wood

    See More
  • Close up of a flame torch testing flame retardant material, demonstrating fire resistance and safety in industrial applications

    Understanding Fire Testing Practices for Cellulosic Passive Fire Protection Systems

    See More

Related Products

See More Products
  • corrosion of linings.jpg

    Corrosion of Linings & Coatings: Cathodic and Inhibitor Protection and Corrosion Monitoring

  • Principles and Applications of Emulsion Polymerization

  • pci march 2020

    PCI March 2020 Issue

See More Products
×

Keep the info flowing with our eNewsletters!

Get the latest industry updates tailored your way.

JOIN TODAY!
  • RESOURCES
    • Advertise
    • Contact Us
    • Directories
    • Store
    • Want More
    • Manufacturing Division
  • SIGN UP TODAY
    • Create Account
    • eMagazine
    • Newsletters
    • Customer Service
    • Manage Preferences
  • SERVICES
    • Marketing Services
    • Reprints
    • Market Research
    • List Rental
    • Survey & Sample
  • STAY CONNECTED
    • LinkedIn
    • Facebook
    • Youtube
    • X (Twitter)
  • PRIVACY
    • PRIVACY POLICY
    • TERMS & CONDITIONS
    • DO NOT SELL MY PERSONAL INFORMATION
    • PRIVACY REQUEST
    • ACCESSIBILITY

Copyright ©2026. All Rights Reserved BNP Media, Inc. and BNP Media II, LLC.

Design, CMS, Hosting & Web Development :: ePublishing