Painting & Coating Industry (PCI) logo Powder coating summit logo
search
cart
facebook twitter linkedin youtube
  • Sign In
  • Join Today
  • Sign Out
  • My Account
Painting & Coating Industry (PCI) logo Powder coating summit logo
  • NEWS
    • Latest News
    • PCI News Now
    • Market Trends & Reports
    • Finishing News
    • Price Alerts
    • Global Top 10/ PCI 25
  • PRODUCTS
    • Product News
    • Featured Products
    • Must See Products and Services
  • MATERIALS
    • Additives
    • Resins/Polymers
    • Pigments
    • Equipment
    • Distributors
  • TECHNOLOGIES
    • Adhesives
    • Architectural Coatings
    • Finishing Articles
    • Finishing Technologies
    • Finishing Equipment
    • Industrial Coatings
    • Nanotechnology
    • Powder Coatings
    • Solventborne
    • Special Purpose Coatings
    • Sustainability
    • UV Coatings
    • Waterborne
  • EVENTS
    • Coatings Trends & Technologies Summit
    • Paint and Coatings Academy
    • Webinars
    • Calendar of Events
    • Lifetime Achievement Award
  • DIRECTORIES
    • Buyer's Guide
    • Equipment Directory
    • Materials Directory
  • RESOURCES
    • Columns
      • Did you know?
      • Distribution Dive
      • Formulating With Mike
      • Innovation Insights
      • Powder Coating Perspectives
      • TiO2 Insider
    • Blogs
      • Editor's Viewpoint
      • Industry Insights
    • Coatings Supplier Handbook
    • COAT-IT! Podcast
    • Videos
    • PCI Store
    • eBooks
    • Sponsor Insights
  • EMAGAZINE
    • eMagazine
    • Archive Issues
    • Editorial Advisory Board
    • CONTACT
    • Advertise
  • JOIN!
Industrial Coatings

Enhancing Infrastructure Longevity with Damage-Tolerant Textured Epoxy Coatings

By Sherwin Williams
Sherwin Williams FT Lead Image.jpg

Image courtesy of Sherwin-Williams. 

May 21, 2024

Sherwin-Williams Protective & Marine launched Sher-Bar TEC, a transformative new coating technology for the concrete industry. Designed for an array of construction applications and environments, the textured epoxy coating (TEC) redefines standards for rebar coatings, offering increased bond strength, damage tolerance, and corrosion resistance for both horizontal and vertical concrete projects. These properties enable improved asset longevity and reduced environmental impacts associated with construction and maintenance.

“Sher-Bar TEC is a breakthrough in concrete and construction innovation,” says Jeffrey Rogozinski, Global Director of Functional Coatings for Sherwin-Williams Protective & Marine. “The textured epoxy coating has the potential to significantly extend the lifespan of critical infrastructure assets – offering a cost-effective solution that adds unprecedented value. With this novel TEC technology, Sherwin-Williams Protective & Marine is ushering in a new era of infrastructure protection and sustainability.”

As a secondary coating, the TEC provides added protection for the industry’s leading corrosion protection solution: epoxy-coated rebar (ECR), which is commonly referred to as “green bar.” With a smoother surface than uncoated rebar, ECR results in reduced bond strength with concrete, necessitating the use of more rebar in projects. This additional rebar adds costs and weight, as well as on-site rebar grid congestion when pouring concrete. These drawbacks have limited the use of ECR worldwide, leaving structures susceptible to corrosion and decay.

This TEC, with its textured elements, offers significant improvements over both ECR and uncoated rebar, known as “black bar.” Tests by independent labs and research universities have documented and demonstrated the coating’s superior performance in bond strength, durability, and corrosion resistance. The research led to the development of the new ASTM A1124/A1124M-23 Standard Specification for textured epoxy-coated steel reinforcing bars, underlining the importance of TEC in the construction industry.

SherwinWilliamsSher-Bar.jpg

According to a Wisconsin Department of Transportation study, this TEC can reduce rebar overlap by 10% to 60%, compared to black bar and ECR. This reduction helps to lower project weights, raw material costs and logistical expenses, while also potentially allowing for the use of higher grades of concrete.

Tests at the University of Illinois showed that cracks in concrete with the TEC-coated rebar were about half as wide as those with ECR bars, suggesting that less road salt and water will be able to infiltrate concrete and meet rebar where it could promote corrosion. Additional tests showed concrete with the TEC-coated rebar had lower levels of stress because the textured rebar was more engaged in the structure.

“Extensive testing has shown that Sher-Bar TEC is a unique and value-adding solution compared to existing rebar coatings and black bar,” says Anthony Del Percio, North American Sales Manager for Rebar, Valve and Traffic Markings for Sherwin-Williams Protective & Marine. “Its performance marks a significant leap forward in the realm of concrete reinforcement.” 

Application of the TEC is also practical and efficient in highly controlled shop conditions. After coating the rebar with powdered fusion-bonded epoxy to create ECR, the powdered TEC is immediately applied. The two layers cure simultaneously and form a seamless, monolithic coating that enhances barrier and durability properties to deliver superior corrosion resistance and damage tolerance. Additionally, the resulting texture restores the desired bonding interaction between the steel and concrete that is lost with smooth ECR surfaces.

A TEC also provides favorable sustainability impacts. Made with up to 30% upcycled materials redirected from landfills, Sher-Bar TEC supports environmentally friendly practices, and promotes the potential use of alternative cementitious technologies that could reduce the significant carbon emissions associated with concrete production.

For more information about Sher-Bar TEC from Sherwin-Williams Protective & Marine, visit here. 

*Images courtesy of Sherwin-Williams. 


 

KEYWORDS: epoxy coatings

Share This Story

Looking for a reprint of this article?
From high-res PDFs to custom plaques, order your copy today!

Recommended Content

JOIN TODAY
to unlock your recommendations.

Already have an account? Sign In

  • Double exposure of creative chemistry concept on laptop background, research and development concept

    Inside the AI Shift in Coatings

    Industry leaders share real-world examples of how AI is...
    Paint and Coating Equipment
    By: PCI Editorial Staff
  • Global Top 10 and PCI Logo

    2026 Global Top 10: Top Paint and Coatings Companies

    See how the world’s largest paint and coatings companies...
    Global Top 10 and PCI 25
    By: Courtney Bassett
  • The 2026 PCI 25

    2026 PCI 25: Top Paint and Coatings Companies

    See how North America's largest paint and coatings...
    Global Top 10 and PCI 25
    By: Courtney Bassett
You must login or register in order to post a comment.

Report Abusive Comment

Manage My Account
  • Join Paint & Coatings Industry
  • Manage My Preferences
  • Customer Service

More Videos

Popular Stories

industry news

Dozens Treated After Toledo Chemical Release

Mergers and aquisitions

Evonik Holds Off on BASF Takeover Talks

AkzoNobel Axalta

EU Clears $25B Akzo-Axalta Merger with One Big Condition

Events

November 11, 2026

ChinaCoat

CHINACOAT2026 returns to Guangzhou this year. Welcome to exhibit, visit and join the annual industry gathering!

November 12, 2026

Premium Leveling, Broad Compatibility: A Cost-Effective Flow and Leveling Additive

This new workhorse additive is recommended in all types of coatings. This highly compatible, 100% active siloxane product prevents defects and maintains good defoamer synergy.

View All Submit An Event

Products

Powder Coatings - Foundation for the Novice Formulator (ebook)

Powder Coatings - Foundation for the Novice Formulator (ebook)

See More Products
PCI news now promo ad

Related Articles

  • Lead Image.jpg

    The Hydropower Industry and Epoxy Coatings

    See More
  • Industry Study Predicts Growth in Epoxy Coatings Market

    See More
  • A Solid Epoxy Resin Emulsion for Acrylic-Epoxy Coatings

    See More

Related Products

See More Products
  • marketsandmarketslogo.jpg

    Protective Coatings Market by Resin Type...

See More Products

Related Directories

  • Westlake Epoxy

    Westlake Epoxy manufactures epoxy resins, modifiers, and curing agents for coatings, adhesives, and construction applications. Its portfolio includes EPON™ resins, EPI-REZ™ waterborne epoxy resins, HELOXY™ modifiers, and EPIKURE™ curing agents. These technologies help formulators meet performance requirements across a range of demanding environments and applications.
×

Keep the info flowing with our eNewsletters!

Get the latest industry updates tailored your way.

JOIN TODAY!
  • RESOURCES
    • Advertise
    • Contact Us
    • Directories
    • Store
    • Manufacturing Division
  • JOIN TODAY
    • Create Account
    • eMagazine
    • Newsletters
    • Customer Service
    • Manage Preferences
  • SERVICES
    • Marketing Services
    • Reprints
    • Market Research
    • List Rental
    • Survey & Sample
  • STAY CONNECTED
    • LinkedIn
    • Facebook
    • Youtube
    • X (Twitter)
  • PRIVACY
    • PRIVACY POLICY
    • TERMS & CONDITIONS
    • DO NOT SELL MY PERSONAL INFORMATION
    • PRIVACY REQUEST
    • ACCESSIBILITY

Copyright ©2026. All Rights Reserved BNP Media, Inc. and BNP Media II, LLC.

Design, CMS, Hosting & Web Development :: ePublishing