Painting & Coating Industry (PCI) logo Powder coating summit logo
search
cart
facebook twitter linkedin youtube
  • Sign In
  • Join Today
  • Sign Out
  • My Account
Painting & Coating Industry (PCI) logo Powder coating summit logo
  • NEWS
    • Latest News
    • PCI News Now
    • Market Trends & Reports
    • Finishing News
    • Price Alerts
    • Global Top 10/ PCI 25
  • PRODUCTS
    • Product News
    • Featured Products
    • Must See Products and Services
  • MATERIALS
    • Additives
    • Resins/Polymers
    • Pigments
    • Equipment
    • Distributors
  • TECHNOLOGIES
    • Adhesives
    • Architectural Coatings
    • Finishing Articles
    • Finishing Technologies
    • Finishing Equipment
    • Industrial Coatings
    • Nanotechnology
    • Powder Coatings
    • Solventborne
    • Special Purpose Coatings
    • Sustainability
    • UV Coatings
    • Waterborne
  • EVENTS
    • Coatings Trends & Technologies Summit
    • Paint and Coatings Academy
    • Webinars
    • Calendar of Events
    • Lifetime Achievement Award
  • DIRECTORIES
    • Buyer's Guide
    • Equipment Directory
    • Materials Directory
  • RESOURCES
    • Columns
      • Did you know?
      • Distribution Dive
      • Formulating With Mike
      • Innovation Insights
      • Powder Coating Perspectives
      • TiO2 Insider
    • Blogs
      • Editor's Viewpoint
      • Industry Insights
    • Coatings Supplier Handbook
    • COAT-IT! Podcast
    • Videos
    • PCI Store
    • eBooks
    • Sponsor Insights
  • EMAGAZINE
    • eMagazine
    • Archive Issues
    • Editorial Advisory Board
    • CONTACT
    • Advertise
  • JOIN!
New ProductsCompany News

PPG Launches Portfolio of Energy-Curable Coatings for Coiled Metal

PPG Launches Portfolio of Energy-Curable Coatings for Coiled Metal.jpg

Image courtesy of PPG via Business Wire. 

August 3, 2024

PPG announced the launch of the PPG DURANEXT™ portfolio of electron-beam- (EB) and ultraviolet- (UV) curable backers, primers, basecoats, and clearcoats that brings the energy efficiency and high speed of energy curing to metal coil coaters.

Unlike traditional coil coating systems that require very high temperatures to drive the curing process, PPG DuraNEXT coatings use an electron beam or ultra-violet energy to convert a liquid coating into a fully cured solid finish in seconds, without any significant loss of thickness or weight.

“As an early pioneer of energy-curable coatings for wood, PPG leveraged 30 years of expertise to develop these state-of-the-art technologies for interior and exterior metal building product applications,” said Irene Tasi, PPG Senior Vice President, Industrial Coatings. “Developing UV-and EB-curable coatings for pre-painted metal is a remarkable advancement in energy curing technologies and illustrates PPG’s commitment to innovation and more sustainable manufacturing across the industries that we serve.”

PPG DuraNEXT solutions are engineered for lasting durability and offer:

  • Reduced energy usage, water consumption and CO 2 emissions, compared to traditional thermal cure coatings.
  • Formulations made without solvents that release volatile organic compounds (VOCs).
  • Faster finishing with curing in less than one second without using heat.
  • Application with multiple methods, including roll-, curtain- and slot-die-coating
  • Solutions that can be customized to meet most requirements for weatherability, durability, chemical resistance and flexibility.

“There is no doubt that coil coaters will adopt these technologies with greater frequency due to their advantages, most notably significant energy savings and fast curing,” said Craig Smith, PPG Global Technical Platform Director, Coil Coatings, and one of the lead authors of the technical paper.

The PPG DuraNEXT portfolio includes:

  • Backers available in both UV and EB formulations to accommodate various application equipment setups. These can be applied over a primer or used as a direct-to-metal application.
  • Primers  available in UV-curable formulations. UV primer can be used under an EB topcoat or with a conventional thermal cure topcoat. These primers could also be used in conjunction with a wet-on-wet applied topcoat and cured with EB in a single pass.
  • Basecoats  available in a full range of glosses and colors for both interior and exterior applications and with options that include smooth, textured and wrinkled finishes. These can also be formulated as a one-coat direct-to-metal solution.
  • Clearcoats engineered to preserve digitally printed inks with a protective layer that adds weatherability and scratch- and abrasion-resistance for residential and commercial applications.

“Our portfolio of EB and UV coil coatings will grow as we continue to develop new energy curable solutions that meet the changing needs of our customers,” Smith said.

For more information on the full PPG DuraNEXT product portfolio, visit PPG DURANEXT TM | PPG Industrial Coatings.

KEYWORDS: Coil Coatings EB curing technology Metal Coatings UV UV & EB technology UV and EB curable coatings UV coatings UV Curable Coatings

Share This Story

Looking for a reprint of this article?
From high-res PDFs to custom plaques, order your copy today!

Recommended Content

JOIN TODAY
to unlock your recommendations.

Already have an account? Sign In

  • Double exposure of creative chemistry concept on laptop background, research and development concept

    Inside the AI Shift in Coatings

    Industry leaders share real-world examples of how AI is...
    Industrial Coatings
    By: PCI Editorial Staff
  • Global Top 10 and PCI Logo

    2026 Global Top 10: Top Paint and Coatings Companies

    See how the world’s largest paint and coatings companies...
    Global Top 10 and PCI 25
    By: Courtney Bassett
  • The 2026 PCI 25

    2026 PCI 25: Top Paint and Coatings Companies

    See how North America's largest paint and coatings...
    Global Top 10 and PCI 25
    By: Courtney Bassett
You must login or register in order to post a comment.

Report Abusive Comment

Manage My Account
  • Join Paint & Coatings Industry
  • Manage My Preferences
  • Customer Service

More Videos

Popular Stories

Breaking News

H.B. Fuller to Close Seven Sites in Supply-Chain Overhaul

AkzoNobel Axalta

EU Clears $25B Akzo-Axalta Merger with One Big Condition

A robotic hand points at a glowing compliance concept surrounded by various icons representing laws, regulations, governance, and standards in a digital workspace

Powder Coater’s $1.64M OSHA Case Follows Earlier Citations

Events

December 2, 2026

Self-Activated Binder Technology: A New Path to Tin-Free Polyurethane Coatings

Through examples from protective and general industrial coating applications, attendees will learn how these innovative technologies can help maintain, and in some cases improve, coating performance while supporting safer, more sustainable formulations that align with evolving regulatory expectations

December 10, 2026

PC Academy: Waterborne Polymers and Film Formation

The trend towards waterborne polymers in the paint and coatings industry is clear; highlighting their environmentally friendly nature, regulatory considerations, growing market demand, and meeting sustainability goals.

View All Submit An Event

Products

Powder Coatings - Foundation for the Novice Formulator (ebook)

Powder Coatings - Foundation for the Novice Formulator (ebook)

See More Products
PCI news now promo ad

Related Articles

  • PPG Launches New Website for Architectural Metal Coatings

    See More
  • Keyland Polymer Showcases its Portfolio of UV-Curable Solid Materials

    See More
  • PPG Launches CRRC, ENERGY STAR Color Registration Initiative

    See More

Related Products

See More Products
  • Kevin-Biller-PC-BOOK.jpg

    Powder Coatings - Foundation for the Novice Formulator (ebook)

See More Products

Related Directories

  • Schlenk Metallic Pigments

    SCHLENK supplies state-of-the-art metallic pigments, including solvent and waterborne aluminum and gold bronze pigments for all coatings and paint applications. In addition, we supply unique special effects like our Zenexo® ultra-thin colored aluminums that offer unmatched durable gold and orange effects. Our very broad Decomet® vacuum metallized pigment line allows formulators to achieve very smooth metal and chrome-like effects. SCHLENK products are available globally.
  • Epcon Industrial Systems LP

    Founded in 1977, Epcon has grown from a one-man operation to a global leader in developing and manufacturing innovative air pollution control technology and industrial heating equipment. Prime and Finish Coil Coating Ovens; Air Pollution Control for VOC / NOx Abatement; Heat Recovery Systems including Hot Water Heaters for Coil Coating lines
×

Keep the info flowing with our eNewsletters!

Get the latest industry updates tailored your way.

JOIN TODAY!
  • RESOURCES
    • Advertise
    • Contact Us
    • Directories
    • Store
    • Manufacturing Division
  • JOIN TODAY
    • Create Account
    • eMagazine
    • Newsletters
    • Customer Service
    • Manage Preferences
  • SERVICES
    • Marketing Services
    • Reprints
    • Market Research
    • List Rental
    • Survey & Sample
  • STAY CONNECTED
    • LinkedIn
    • Facebook
    • Youtube
    • X (Twitter)
  • PRIVACY
    • PRIVACY POLICY
    • TERMS & CONDITIONS
    • DO NOT SELL MY PERSONAL INFORMATION
    • PRIVACY REQUEST
    • ACCESSIBILITY

Copyright ©2026. All Rights Reserved BNP Media, Inc. and BNP Media II, LLC.

Design, CMS, Hosting & Web Development :: ePublishing