Painting & Coating Industry (PCI) logo Powder coating summit logo
search
cart
facebook twitter linkedin youtube
  • Sign In
  • Create Account
  • Sign Out
  • My Account
Painting & Coating Industry (PCI) logo Powder coating summit logo
  • NEWS
    • Latest News
    • Market Trends & Reports
    • Finishing News
    • Price Alerts
    • Global Top 10/ PCI 25
  • PRODUCTS
    • Product News
    • Featured Products
    • Must See Products and Services
  • MATERIALS
    • Additives
    • Resins/Polymers
    • Pigments
    • Equipment
    • Distributors
  • TECHNOLOGIES
    • Adhesives
    • Architectural Coatings
    • Finishing Articles
    • Finishing Technologies
    • Finishing Equipment
    • Industrial Coatings
    • Nanotechnology
    • Powder Coatings
    • Solventborne
    • Special Purpose Coatings
    • Sustainability
    • UV Coatings
    • Waterborne
  • EVENTS
    • Coatings Trends & Technologies Summit
    • Paint and Coatings Academy
    • Webinars
    • Calendar of Events
    • Lifetime Achievement Award
  • DIRECTORIES
    • Buyer's Guide
    • Equipment Directory
    • Materials Directory
  • RESOURCES
    • Columns
      • Did you know?
      • Distribution Dive
      • Formulating With Mike
      • Innovation Insights
      • Powder Coating Perspectives
      • TiO2 Insider
    • Blogs
      • Editor's Viewpoint
      • Industry Insights
    • Coatings Supplier Handbook
    • COAT-IT! Podcast
    • Videos
    • PCI Store
    • eBooks
    • Sponsor Insights
  • EMAGAZINE
    • eMagazine
    • Archive Issues
    • China Issue Archive
    • Editorial Advisory Board
    • CONTACT
    • Advertise
  • SIGN UP!
Company News

PPG Earns 2024 Altair Enlighten Award

PPG Earns 2024 Altair Enlighten Award.jpg

Image courtesy of PPG. 

August 19, 2024

PPG announced that it has received a 2024 Altair Enlighten Award from IT firm Altair Engineering, which honors sustainability and lightweighting advancements in the automotive industry. PPG and Toyota North America earned the runner-up award in the Sustainable Process category for the use of PPG ENVIRO-PRIME® EPIC 200X electrocoat at Toyota’s automotive manufacturing plant in Canada.

PPG Enviro-Prime EPIC 200X electrocoat was implemented at the Toyota Motor Manufacturing Canada North Plant in Cambridge, Ontario in 2023. The technology enhances corrosion protection for automotive bodies while significantly reducing environmental impact through lower material usage and energy requirements. At the Toyota facility, the product and application process enables a total reduction of 3,500 metric tons of CO2 emissions per year. The amount of applied product is reduced by 0.6 kg per vehicle, while the application process saves 5.6 million kWh of energy and 1.8 million gallons of water per year.

“PPG’s focus on sustainability helps automakers and Tier suppliers reduce their environmental impact in the midst of ever-increasing corporate targets and regulatory requirements,” said Andrew Carroll, PPG Vice President, Americas, Automotive OEM Coatings. “We collaborate closely with customers such as Toyota to ensure our products meet their performance expectations while delivering real-world sustainability and productivity advantages. We thank Altair for recognizing the environmental impact improvements delivered by PPG and Toyota.”

In May, PPG also earned an American Chemistry Council (ACC) 2024 Sustainability Leadership Award, which recognizes exemplary products, technologies and initiatives that help advance sustainability. PPG received the award in the Product Safety, Innovation and Transparency category for its PPG Enviro-Prime EPIC 300 electrocoat, which cures at lower temperatures than previous electrocoat technologies, helping reduce greenhouse gas emissions from coatings application in the automotive original equipment manufacturing process.

KEYWORDS: Automotive Coatings awards recognition

Share This Story

Looking for a reprint of this article?
From high-res PDFs to custom plaques, order your copy today!

Recommended Content

JOIN TODAY
to unlock your recommendations.

Already have an account? Sign In

  • Double exposure of creative chemistry concept on laptop background, research and development concept

    Inside the AI Shift in Coatings

    Industry leaders share real-world examples of how AI is...
    Sustainable
    By: PCI Editorial Staff
  • Global Top 10 and PCI Logo

    2026 Global Top 10: Top Paint and Coatings Companies

    See how the world’s largest paint and coatings companies...
    Global Top 10 and PCI 25
    By: Courtney Bassett
  • The 2026 PCI 25

    2026 PCI 25: Top Paint and Coatings Companies

    See how North America's largest paint and coatings...
    Global Top 10 and PCI 25
    By: Courtney Bassett
You must login or register in order to post a comment.

Report Abusive Comment

Manage My Account
  • eMagazine
  • Newsletters
  • Online Registration
  • Subscription Customer Service

More Videos

Sponsored Content

Sponsored Content is a special paid section where industry companies provide high quality, objective, non-commercial content around topics of interest to the PCI audience. All Sponsored Content is supplied by the advertising company and any opinions expressed in this article are those of the author and not necessarily reflect the views of PCI or its parent company, BNP Media. Interested in participating in our Sponsored Content section? Contact your local rep!

close
  • wooden kitchen set and shelving
    Sponsored bySirca North America

    Leveraging Coatings to Meet ESG Goals in Manufacturing

Popular Stories

Breaking News

Yenkin-Majestic Pleads Guilty in Fatal Resin Plant Explosion Case

Plaque sign on the outside of the United States Environmental Protection Agency

EPA Draft Finds Worker Risks From trans-1,2-Dichloroethylene

Solstice Logo

Solstice, Element Solutions Terminate $14.5B Deal

Webinar custom content box

Events

January 1, 2030

Webinar Sponsorship Information

For webinar sponsorship information, visit www.bnpevents.com/webinars or email webinars@bnpmedia.com.

View All Submit An Event

Products

Advanced Coating Materials

Advanced Coating Materials

See More Products
Webinar custom content box

Related Articles

  • Henkel Altair award

    Henkel Wins Altair Enlighten Award for Next-Generation Metal Pretreatment Process

    See More
  • PPG logo

    PPG Earns Equality 100 Award in 2023 Corporate Equality Index

    See More
  • PPG Earns 2016 John Deere Supplier of the Year Award

    See More

Related Products

See More Products
  • July 25, 2024

  • January 25, 2024

  • July 25, 2024

See More Products

Related Directories

  • WAB US Corp.

    WAB-GROUP® is a leading specialist in wet grinding technology, three-dimensional mixing technology and flow chemistry. The DYNO-MILL® wet milling and TURBULA® homogenous mixing brands support the paints and coatings industry globally with 70 years of experience. WAB is synonymous with highest efficiency, optimal performance, energy savings and lowest waste.
  • LANXESS Corp.

    LANXESS is a leading specialty chemicals company with sales of EUR 6.4 billion in 2024. The core business of LANXESS is the development, manufacturing and marketing of chemical intermediates, additives and consumer protection products. LANXESS holds leading positions in the Dow Jones Best-in-Class Index and the MSCI ESG and ISS ESG ratings, among others, for its commitment to sustainability.
×

Keep the info flowing with our eNewsletters!

Get the latest industry updates tailored your way.

JOIN TODAY!
  • RESOURCES
    • Advertise
    • Contact Us
    • Directories
    • Store
    • Want More
    • Manufacturing Division
  • SIGN UP TODAY
    • Create Account
    • eMagazine
    • Newsletters
    • Customer Service
    • Manage Preferences
  • SERVICES
    • Marketing Services
    • Reprints
    • Market Research
    • List Rental
    • Survey & Sample
  • STAY CONNECTED
    • LinkedIn
    • Facebook
    • Youtube
    • X (Twitter)
  • PRIVACY
    • PRIVACY POLICY
    • TERMS & CONDITIONS
    • DO NOT SELL MY PERSONAL INFORMATION
    • PRIVACY REQUEST
    • ACCESSIBILITY

Copyright ©2026. All Rights Reserved BNP Media, Inc. and BNP Media II, LLC.

Design, CMS, Hosting & Web Development :: ePublishing