Painting & Coating Industry (PCI) logo Powder coating summit logo
search
cart
facebook twitter linkedin youtube
  • Sign In
  • Join Today
  • Sign Out
  • My Account
Painting & Coating Industry (PCI) logo Powder coating summit logo
  • NEWS
    • Latest News
    • PCI News Now
    • Market Trends & Reports
    • Finishing News
    • Price Alerts
    • Global Top 10/ PCI 25
  • PRODUCTS
    • Product News
    • Featured Products
    • Must See Products and Services
  • MATERIALS
    • Additives
    • Resins/Polymers
    • Pigments
    • Equipment
    • Distributors
  • TECHNOLOGIES
    • Adhesives
    • Architectural Coatings
    • Finishing Articles
    • Finishing Technologies
    • Finishing Equipment
    • Industrial Coatings
    • Nanotechnology
    • Powder Coatings
    • Solventborne
    • Special Purpose Coatings
    • Sustainability
    • UV Coatings
    • Waterborne
  • EVENTS
    • Coatings Trends & Technologies Summit
    • Paint and Coatings Academy
    • Webinars
    • Calendar of Events
    • Lifetime Achievement Award
  • DIRECTORIES
    • Buyer's Guide
    • Equipment Directory
    • Materials Directory
  • RESOURCES
    • Columns
      • Did you know?
      • Distribution Dive
      • Formulating With Mike
      • Innovation Insights
      • Powder Coating Perspectives
      • TiO2 Insider
    • Blogs
      • Editor's Viewpoint
      • Industry Insights
    • Coatings Supplier Handbook
    • COAT-IT! Podcast
    • Videos
    • PCI Store
    • eBooks
    • Sponsor Insights
  • EMAGAZINE
    • eMagazine
    • Archive Issues
    • Editorial Advisory Board
    • CONTACT
    • Advertise
  • JOIN!
New Products

Bung Entering Mixers

Bung Entering Mixers.jpg

Image courtesy of INDCO. 

August 24, 2024

INDCO offers bung entering mixers with efficient and hassle-free options for light and medium viscosity materials in 55-gallon drums. CB-series mixers are direct driven and designed for low- to medium-viscosity materials and suspending settled solids. They are available with ¾ - 4 HP air motors that operate from 300-3000 rpm, ½- 1 HP TEFC electric motors at 1750 rpm, or ½ - 1 HP variable speed electric motors that operate from 35 – 1750 RPM.  Gear-driven CBG-series models bring more power to tougher jobs, featuring a heavy-duty 5:1 ratio helical gearbox for ample torque. They’re ideal for mixing medium-viscosity materials such as paints, resins, and polymers. CBG models are available with ¾ - 1 ½ HP air motors which operate from 60-600 RPM, or ½- 1/3 HP electric motors at 350 RPM, or variable speed electric motors from 1/3 – ½ HP that operate from 0-350 RPM. All mixers feature a clamp that adjusts to the rim of steel drums with a hand knob and sits at an angle, allowing entry through a drum lid bung. The unique folding propellers collapse to fit easily through 2” NPT openings, then expand to 4” or 7” inches depending on the model, working well with closed or open drums. All wetted parts are made of stainless steel for chemical resistance and long-lasting performance.

CB- and CBG-series mixers come in multiple motor types and options to ensure compatibility with power and safety requirements. Totally Enclosed, Fan-Cooled (TEFC), and air motors are available as standard. TEFC models come with a cord, switch, and three-prong plug, while electric variable-speed models feature a speed controller mounted directly on and prewired to the motor. Air motors deliver variable speed for maximum flexibility or multiple applications, are lighter in weight than electric models, and reduce the possibility of explosion in a combustible environment. EP explosion proof electric units have motor leads only, ensuring safe operation in hazardous environments. CB- and CBG-series mixers are manufactured in INDCO’s New Albany, IN factory and typically ship within 2 business days. Contact factory for details. 

Located in New Albany, Indiana, INDCO is a leading manufacturer of industrial mixers. Since 1975 they have designed and manufactured a completed lineup of mixers for batch sizes up to 50,000 gallons. They use premium brand components in their robust designs to deliver high quality mixers that earn their customer’s trust. In addition to premier equipment, INDCO prides itself on providing fast, friendly customer service and immediate technical support. Full information is available on their comprehensive website, www.INDCO.com, by calling (800) 851-1049, or via email at info@INDCO.com. 

KEYWORDS: Mixers

Share This Story

Looking for a reprint of this article?
From high-res PDFs to custom plaques, order your copy today!

Recommended Content

JOIN TODAY
to unlock your recommendations.

Already have an account? Sign In

  • Double exposure of creative chemistry concept on laptop background, research and development concept

    Inside the AI Shift in Coatings

    Industry leaders share real-world examples of how AI is...
    Paint and Coating Pigments
    By: PCI Editorial Staff
  • Global Top 10 and PCI Logo

    2026 Global Top 10: Top Paint and Coatings Companies

    See how the world’s largest paint and coatings companies...
    Global Top 10 and PCI 25
    By: Courtney Bassett
  • The 2026 PCI 25

    2026 PCI 25: Top Paint and Coatings Companies

    See how North America's largest paint and coatings...
    Global Top 10 and PCI 25
    By: Courtney Bassett
You must login or register in order to post a comment.

Report Abusive Comment

Manage My Account
  • Join Paint & Coatings Industry
  • Manage My Preferences
  • Customer Service

More Videos

Popular Stories

Mergers and aquisitions

BASF Ends Evonik Takeover Pursuit

industry news

Dozens Treated After Toledo Chemical Release

Breaking News

H.B. Fuller to Close Seven Sites in Supply-Chain Overhaul

Events

December 2, 2026

Self-Activated Binder Technology: A New Path to Tin-Free Polyurethane Coatings

Through examples from protective and general industrial coating applications, attendees will learn how these innovative technologies can help maintain, and in some cases improve, coating performance while supporting safer, more sustainable formulations that align with evolving regulatory expectations

December 10, 2026

PC Academy: Waterborne Polymers and Film Formation

The trend towards waterborne polymers in the paint and coatings industry is clear; highlighting their environmentally friendly nature, regulatory considerations, growing market demand, and meeting sustainability goals.

View All Submit An Event

Products

Powder Coatings - Foundation for the Novice Formulator (ebook)

Powder Coatings - Foundation for the Novice Formulator (ebook)

See More Products
PCI news now promo ad

Related Articles

  • Top-Entering Mixers

    See More
  • Top-Entering, Portable Mixers

    See More
  • Gear-Drive Drum Mixers

    Bung-Mount Mixer Supports High-Viscosity Blending in Drum Applications

    See More

Events

View AllSubmit An Event
  • March 31, 2026

    Durability by Design: Waterborne Concrete Coatings that Protect, Beautify, and Extend Service Life

    On Demand Attend this webinar to understand how protecting concrete enables lifespan extension and reduction of the CO₂ emissions associated with premature repair or replacement.
View AllSubmit An Event

Related Directories

  • Myers Mixers

    Myers Mixers offers solutions for fluid and semi-solid mixing, dispersing, and homogenizing. From dispersing to complex compounding, Myers specializes in off-the-shelf and custom-designed equipment to make any mixing and dispersing process as efficient as possible. Equipment offered includes multi-shaft mixing and dispersing equipment, hydraulic ram presses, mixer controls and data-logging.
  • ROSS Mixers

    Founded in 1842, Charles Ross & Son Company is a leading manufacturer of mixing, blending, and dispersion equipment. With over 180 years of innovation and experience, ROSS serves customers across the paint, ink, coating, adhesive, and advanced materials industries worldwide. The ROSS Test & Development Center in Hauppauge, New York, provides application testing and process development support and is an invaluable resource for customers looking to improve their mixing processes.
  • Myers Mixers LLC

    Myers Mixers offers solutions for fluid and semi-solid mixing, dispersing and homogenizing. From dispersing to complex compounding, Myers specializes in off-the-shelf and custom-designed equipment to make any mixing and dispersing process as efficient as possible. Equipment offered includes multi-shaft mixing and dispersing equipment, hydraulic ram presses, mixer controls and data-logging.
×

Keep the info flowing with our eNewsletters!

Get the latest industry updates tailored your way.

JOIN TODAY!
  • RESOURCES
    • Advertise
    • Contact Us
    • Directories
    • Store
    • Manufacturing Division
  • JOIN TODAY
    • Create Account
    • eMagazine
    • Newsletters
    • Customer Service
    • Manage Preferences
  • SERVICES
    • Marketing Services
    • Reprints
    • Market Research
    • List Rental
    • Survey & Sample
  • STAY CONNECTED
    • LinkedIn
    • Facebook
    • Youtube
    • X (Twitter)
  • PRIVACY
    • PRIVACY POLICY
    • TERMS & CONDITIONS
    • DO NOT SELL MY PERSONAL INFORMATION
    • PRIVACY REQUEST
    • ACCESSIBILITY

Copyright ©2026. All Rights Reserved BNP Media, Inc. and BNP Media II, LLC.

Design, CMS, Hosting & Web Development :: ePublishing