Painting & Coating Industry (PCI) logo Powder coating summit logo
search
cart
facebook twitter linkedin youtube
  • Sign In
  • Create Account
  • Sign Out
  • My Account
Painting & Coating Industry (PCI) logo Powder coating summit logo
  • NEWS
    • Latest News
    • Market Trends & Reports
    • Finishing News
    • Price Alerts
    • Subscribe to Newsletters
    • Global Top 10/ PCI 25
    • Weekly Featured Article
    • COATLE Word Game
  • PRODUCTS
    • Product News
    • Featured Products
    • Must See Products and Services
  • MATERIALS
    • Additives
    • Resins/Polymers
    • Pigments
    • Equipment
    • Distributors
  • TECHNOLOGIES
    • Adhesives
    • Architectural Coatings
    • Finishing Articles
    • Finishing Technologies
    • Finishing Equipment
    • Industrial Coatings
    • Nanotechnology
    • Powder Coatings
    • Solventborne
    • Special Purpose Coatings
    • Sustainability
    • UV Coatings
    • Waterborne
  • RESOURCES
    • Columns
      • Did you know?
      • Distribution Dive
      • Formulating With Mike
      • Innovation Insights
      • Powder Coating Perspectives
      • TiO2 Insider
    • Blogs
      • Editor's Viewpoint
      • Industry Insights
    • Coatings Supplier Handbook
    • Podcasts and Videos
      • COAT-IT! Podcast
      • Videos/PCI TV
    • PCI Store
    • Classifieds
    • eBooks
    • Sponsor Insights
    • White Papers
    • COATLE Word Game
  • EVENTS
    • Coatings Trends & Technologies Summit
    • Paint and Coatings Academy
    • Webinars
    • Calendar of Events
    • Lifetime Achievement Award
  • DIRECTORIES
    • Buyer's Guide
    • Equipment Directory
    • Materials Directory
  • EMAGAZINE
    • Current Issue
    • eMagazine Archive
    • China Issue Archive
    • Editorial Advisory Board
  • CONTACT
    • Contact Us
    • Advertise
    • Subscribe to eMagazine
    • Subscribe to Newsletters
  • SIGN UP!
Industrial CoatingsSustainableFinishing Articles

How High Can You Go with Bio-Based Rust Prevention?

By Cortec Corporation
Cortec lead image.jpg
August 26, 2024

Cortec Image 1.jpgToday’s emphasis on sustainability and the circular economy may leave some manufacturers wondering: "Can I really get the results I need while increasing my use of bio-based content?” Cortec® shares two viable rust preventatives that allow users to go as high as 72% or 99% bio-based content for metals protection in humid environments.

Canola Oil-Based Rust Preventatives

EcoLine® 3690 and EcoLine® 3220 are two wet-film rust preventatives from Cortec. Each includes a special package of corrosion inhibitors in a canola oil base for protection in high-humidity conditions. EcoLine 3690 contains 72% USDA-certified bio-based content. EcoLine 3220 goes even higher; it contains 99% USDA-certified bio-based content. Both can be applied by spray, brush, or dip like traditional wet-film rust preventatives, leaving behind a tenacious oily film that clings to metal surfaces and provides excellent contact corrosion protection.

Where to Use the Preventatives

These two temporary bio-based coatings can be used in a variety of applications. Among the most common is rust prevention in various stages of the manufacturing process or during storage and shipment. The coatings protect both ferrous and yellow metals, and can be applied to wire, sheet metals, pipes, flanges, gears, and equipment. Furthermore, a low pour point of -0 °F (-18 °C) makes the 3220 product good for application in cold conditions where other rust preventatives might freeze.

Bio-Based Rust Prevention in Action

With almost three-quarters of its content coming from a renewable cooking oil, 3690 has been used to replace products that were less friendly to workers and the environment. In one case, a tube manufacturer investigated the use of the coating as a rust preventative for the ends of pipes bundled and stored for 9-12 months outdoors. They were impressed with the results on the test bundle after eight months and expressed satisfaction with its level of worker safety as they decided to use it going forward.

In another case, the coating was adopted for protection of automotive all-time-buys that needed be stored for up to 10 years after tooling retirement. The previous rust preventative had been used for decades but was hard to remove and raised worker and environmental concerns. Cortec’s coating underwent necessary testing and met the automaker’s requirements for rust prevention, so it was written into the automaker’s specifications for aftermarket engineering processes. The third-party packager started using it in 2019 for crankshafts, camshafts, and cylinder heads going into long-term storage.

Cortec Image 2.jpgA protected camshaft four days in salt spray conditions.

Time to Up Your Bio-Based Content?

Being able to reduce the amount of petroleum-based solvents in a product and replace them with gentler bio-based material such as canola oil is a great option whenever an effective, affordable product results. To learn more visit and contact Cortec here. 

 *Images courtesy of Cortec. 

KEYWORDS: bio-based bio-based coatings rust and corrosion inhibitors rust preventative

Share This Story

Looking for a reprint of this article?
From high-res PDFs to custom plaques, order your copy today!

By Cortec® Corporation, St. Paul, Minnesota

Recommended Content

JOIN TODAY
to unlock your recommendations.

Already have an account? Sign In

  • pci1022-Kinaltek-Lead-1170.jpg

    A Novel Pigment Production Technology

    Following an extensive R&D program that demonstrated...
    Paint and Coating Pigments
    By: Jawad Haidar and Nitin Soni
  • pci global top 10

    2025 Global Top 10: Top Paint and Coatings Companies

    The following is PCI’s annual ranking of the top 10...
    Paint and Coating Market Reports
    By: Courtney Bassett
  • 2025 pci 25

    2025 PCI 25: Top Paint and Coatings Companies

    PCI's annual ranking of the top 25 North American paint...
    Paint and Coating Market Reports
    By: Courtney Bassett
You must login or register in order to post a comment.

Report Abusive Comment

Manage My Account
  • eMagazine
  • Newsletters
  • Online Registration
  • Subscription Customer Service

More Videos

Sponsored Content

Sponsored Content is a special paid section where industry companies provide high quality, objective, non-commercial content around topics of interest to the PCI audience. All Sponsored Content is supplied by the advertising company and any opinions expressed in this article are those of the author and not necessarily reflect the views of PCI or its parent company, BNP Media. Interested in participating in our Sponsored Content section? Contact your local rep!

close
  • wooden kitchen set and shelving
    Sponsored bySirca North America

    Leveraging Coatings to Meet ESG Goals in Manufacturing

  • man woodworking in workshop
    Sponsored byGemini Industries, Inc.

    Waterborne Coatings Aren't the Future -- They're the New Performance Benchmark

Popular Stories

Akzo, SW, Nippon Logos

AkzoNobel Rejects Cash Offer From Nippon Paint, Sherwin-Williams

BASF SE Logo

BASF Announces Strategic Business Sale

AkzoSWNipponEndTalks

Nippon Paint, Sherwin-Williams End AkzoNobel Pursuit

POB-Point-and-Shoot

PCI Buyers Guide

Submit a Request for Proposal (RFP) to suppliers of your choice with details on what you need with a click of a button

Start your RFP

Browse our Buyers Guide for manufacturers and distributors of all types of coatings products and much more!

Find Suppliers

Events

September 4, 2025

N-Butylpyrrolidone (NBP) as a Green Solvent to Replace N-Methylpyrrolidone (NMP) in Industrial Coating Applications

ON DEMAND: EPA published a regulation proposal around N-methylpyrrolidone (NMP) in June 2024 to ban or limit NMP in many applications, such as paints and coatings and their removers. N-butylpyrrolidone (NBP) is a powerful and versatile solvent for a variety of industries looking for alternatives to substance of very high concern (SVHC)-listed solvents.

September 15, 2026

Coatings Trends & Technologies Summit

The Coatings Trends & Technologies (CTT) Summit is an annual conference for both liquid and powder coatings formulators and manufacturers to discuss innovations in coatings technology. This event combines high-quality technical presentations, a resource-rich exhibit hall, and dedicated networking opportunities to connect scientific minds, foster innovation, and cultivate game-changing new ideas!

View All Submit An Event

Poll

Longest-running laboratory experiment

What is the longest-running laboratory experiment?
View Results Poll Archive

Products

Automotive Paints and Coatings, 2nd Edition

Now in its second edition and still the only book of its kind, this is an authoritative treatment of all stages of the coating process.

See More Products
Inside the AI Shift in Coatings - See the article now

Related Articles

  • Electrocoat Finishes: How Low Can You Go?

    See More
  • Discovering Long-Term Rust Prevention for Automotive and Heavy Equipment Parts

    Discovering Long-Term Rust Prevention for Automotive and Heavy Equipment Parts

    See More
  • Student Wins Hanna Award for Rust-Prevention Analysis

    See More

Related Products

See More Products
  • biopolymer.jpg

    Biopolymer-Based Films and Coatings Trends and Challenges

  • pci august 2019

    PCI August 2019 Issue

See More Products

Related Directories

  • Vertec BioSolvents Inc.

    Sustainable, safe, bio-based performance solvents and blends from renewable resources to replace petroleum-based solvents for formulating, blending and cleaning.
×

Keep the info flowing with our eNewsletters!

Get the latest industry updates tailored your way.

JOIN TODAY!
  • RESOURCES
    • Advertise
    • Contact Us
    • Directories
    • Store
    • Want More
    • Manufacturing Division
  • SIGN UP TODAY
    • Create Account
    • eMagazine
    • Newsletters
    • Customer Service
    • Manage Preferences
  • SERVICES
    • Marketing Services
    • Reprints
    • Market Research
    • List Rental
    • Survey & Sample
  • STAY CONNECTED
    • LinkedIn
    • Facebook
    • Youtube
    • X (Twitter)
  • PRIVACY
    • PRIVACY POLICY
    • TERMS & CONDITIONS
    • DO NOT SELL MY PERSONAL INFORMATION
    • PRIVACY REQUEST
    • ACCESSIBILITY

Copyright ©2026. All Rights Reserved BNP Media, Inc. and BNP Media II, LLC.

Design, CMS, Hosting & Web Development :: ePublishing