Painting & Coating Industry (PCI) logo Powder coating summit logo
search
cart
facebook twitter linkedin youtube
  • Sign In
  • Join Today
  • Sign Out
  • My Account
Painting & Coating Industry (PCI) logo Powder coating summit logo
  • NEWS
    • Latest News
    • PCI News Now
    • Market Trends & Reports
    • Finishing News
    • Price Alerts
    • Global Top 10/ PCI 25
  • PRODUCTS
    • Product News
    • Featured Products
    • Must See Products and Services
  • MATERIALS
    • Additives
    • Resins/Polymers
    • Pigments
    • Equipment
    • Distributors
  • TECHNOLOGIES
    • Adhesives
    • Architectural Coatings
    • Finishing Articles
    • Finishing Technologies
    • Finishing Equipment
    • Industrial Coatings
    • Nanotechnology
    • Powder Coatings
    • Solventborne
    • Special Purpose Coatings
    • Sustainability
    • UV Coatings
    • Waterborne
  • EVENTS
    • Coatings Trends & Technologies Summit
    • Paint and Coatings Academy
    • Webinars
    • Calendar of Events
    • Lifetime Achievement Award
  • DIRECTORIES
    • Buyer's Guide
    • Equipment Directory
    • Materials Directory
  • RESOURCES
    • Columns
      • Did you know?
      • Distribution Dive
      • Formulating With Mike
      • Innovation Insights
      • Powder Coating Perspectives
      • TiO2 Insider
    • Blogs
      • Editor's Viewpoint
      • Industry Insights
    • Coatings Supplier Handbook
    • COAT-IT! Podcast
    • Videos
    • PCI Store
    • eBooks
    • Sponsor Insights
  • EMAGAZINE
    • eMagazine
    • Archive Issues
    • Editorial Advisory Board
    • CONTACT
    • Advertise
  • JOIN!
Industrial CoatingsSpecial Purpose Coatings

Advanced Fluoropolymer Coatings Ensure Durability and Color Match

By Linetec
The National Aquarium Linetec Coatings.jpg

Image courtesy of Linetec. 

August 30, 2024

The National Aquarium in Baltimore renovated its iconic pyramid-shaped skylight that caps its “Upland Tropical Rain Forest” immersive exhibit on Pier 3 of the Inner Harbor. The project was completed in partnership with architectural firm Design Collective, general contractor Plano-Coudon and Super Sky Products Enterprises. According to the Aquarium, this critical improvement ensures the future of the glass pyramid for the next half-century.

To refresh its appearance and update its performance, Super Sky teamed with Skylight Partners of America to repair and replace the existing skylight. Where necessary, Super Sky manufactured and installed new aluminum framing systems. Along with bird-friendly glass, the updated skylight features aluminum framing finished by Linetec to meet coastal conditions and to preserve the existing exterior and interior color palette.

Super Sky’s renovation manager, Todd Wilde, enthusiastically shared his compliments saying, “This very high-profile, monumental project turned out looking great and was a very successful project. There is great satisfaction in seeing your repair concept come to fruition, get completed without too many issues, look like a brand-new product once completed and know that you helped the owner improve the aesthetics and performance of the buildings – all while minimizing the impact to the occupants.”

The national aquarium linetec coatings 4The national aquarium linetec coatings 2The national aquarium linetec coatings 1The national aquarium linetec coatings 3
×

Finding an Ideal (Color) Match

For many years and many high-profile projects, Super Sky has relied on Linetec as its single solution for architectural finishing. To help ensure color consistency with the critical appearance, Linetec paint technicians examine a finished part from the existing building to create the closest match possible. Even if the precise details from the original finish are known, adjustments can be made so the newly finished material aligns with the correct vintage of color currently on the building.

“For existing buildings in need of color matching, our unparalleled expertise ensures near-perfect results,” said Tammy Schroeder, director of marketing for Linetec. “We use the latest technologies to analyze and formulate thousands of color variations, ensuring creation of the exact color specified. With our in-house experts and computerized blending capabilities, we’ve applied more than 65,000 unique colors.”

For Super Sky’s aluminum-framed skylight system on the National Aquarium, the design team specified Quaker Bronze as the color. Different paint coating manufacturers each have their own special shades of Quaker Bronze. To ensure the correct match, the design team references the unique Linetec color code, which is LT602. This is one of 20 standard in-house colors offered by Linetec. Standard colors generally provide the most economical choice for architectural coatings, while still delivering the highest performance painted finish.

Ensuring Durable Finishes for Coastal Environments

In addition to matching the aesthetic requirements for finishing Super Sky’s aluminum-framed skylight system on the National Aquarium, Linetec also meets the high-performance requirements for the project. The design team specified a 70% fluoropolymer resin-based coating that meets AAMA 2605. Published by the Fenestration and Glazing Industry Alliance (FGIA), this is the most stringent industry standard for painted coatings available for aluminum-framed skylights and other architectural aluminum building products.

For the National Aquarium, Linetec applied a PPG Duranar® two-coat architectural liquid paint to Super Sky’s extruded aluminum framing members under factory quality-controlled conditions. Standard color two-coat systems consist of a primer and color coat. The Duranar coating’s fluoropolymer formulation includes 70% polyvinylidene fluoride (PVDF) resin.

Considering Baltimore’s hot summers, cold winters and proximity to the coast, fluoropolymer coatings with 70% PVDF resin offer the ultimate protection in building performance. In compliance with AAMA 2605, these finishes exhibit outstanding resistance to humidity, color change, chalking, gloss loss, chemicals and salt spray. Linetec ensures a long-lasting, durable finish, typically supported with a 10-year warranty. No other coating system can withstand the rigors of nature and time like those based on 70% PVDF resin coatings.

Respecting the Environment – Inside and Out

As an environmentally responsible finisher, Linetec safely captures and destroys volatile organic compounds (VOCs) associated with liquid coatings during its paint application process and repurposes the heat produced from their reclamation. This means that when the finished products from Linetec are installed on a building project, such as the National Aquarium, there are no adverse effects from “off gassing” on the building’s indoor air quality or on its human and animal occupants.

The renovated skylight also helps protect the birds outside the National Aquarium. The glass panes had not been replaced since the National Aquarium opened 41 years ago and were due for an upgrade. Design Collective selected an opaque glass with an acid-etched pattern that deters bird collisions.

The new glass and the skylight’s surrounding LEDs minimize light pollution, creating an ambient nighttime glow from the outside. On the inside, the glass provides a diffused light and its low-e coating helps maintain the required climate, offering a comfortable experience for both animals and guests. Visitors can see a variety of colorful tropical birds, two-toed sloths, blue poison dart frogs, yellow-footed tortoises and golden lion tamarins, along with 160 species of continuously growing plants from South America that feed and shelter the animals.

Overcoming Challenges for a Successful Completion

Replacement and installation on the Aquarium skylight’s 679 glazing units began in March 2022 and progressed as planned through completion in September. To replace the pyramid’s glazing, the team needed to work at 96-foot heights on a sloped surface.

“There are not many subcontractors in the country qualified to do this kind of work,” said Plano-Coudon’s vice president, Cliff Milstead, LEED AP. “They did a really great job figuring out some challenging logistics.”

At the November 2022 reopening celebration event, National Aquarium’s president and CEO John Racanelli said, “Though many of the changes… may not be noticeable to the eye, they have greatly improved the environment for the animals and plants, as well as made it safer for our staff.”

Recognizing the thoughtful and successful renovation, the National Aquarium and its project team have received several accolades. At the Associated Builders and Contractors of Greater Baltimore’s 2023 Excellence in Construction Awards, the project was recognized as a Gold Winner. The Metropolitan Baltimore’s Building Congress & Exchange also honored the project with multiple 2023 Craftsmanship Awards including for the skylight renovation and for the overall building.

*Images courtesy of Linetec. 

KEYWORDS: color matching fluoropolymer coatings Protective Coatings

Share This Story

Looking for a reprint of this article?
From high-res PDFs to custom plaques, order your copy today!

By Linetec, Wausau, Wisconsin

Recommended Content

JOIN TODAY
to unlock your recommendations.

Already have an account? Sign In

  • Double exposure of creative chemistry concept on laptop background, research and development concept

    Inside the AI Shift in Coatings

    Industry leaders share real-world examples of how AI is...
    Architectural Coatings
    By: PCI Editorial Staff
  • Global Top 10 and PCI Logo

    2026 Global Top 10: Top Paint and Coatings Companies

    See how the world’s largest paint and coatings companies...
    Global Top 10 and PCI 25
    By: Courtney Bassett
  • The 2026 PCI 25

    2026 PCI 25: Top Paint and Coatings Companies

    See how North America's largest paint and coatings...
    Global Top 10 and PCI 25
    By: Courtney Bassett
You must login or register in order to post a comment.

Report Abusive Comment

Manage My Account
  • Join Paint & Coatings Industry
  • Manage My Preferences
  • Customer Service

More Videos

Popular Stories

Mergers and aquisitions

Evonik Holds Off on BASF Takeover Talks

industry news

Dozens Treated After Toledo Chemical Release

Breaking News

H.B. Fuller to Close Seven Sites in Supply-Chain Overhaul

Events

November 19, 2026

Reformulating Paints with AI: Turn Change into a Competitive Advantage

Join industry leaders and experts for real case studies showing how AI helps R&D teams use existing paint formulation and test data to evaluate alternatives, predict trade-offs, and prioritize experiments.

December 10, 2026

PC Academy: Waterborne Polymers and Film Formation

The trend towards waterborne polymers in the paint and coatings industry is clear; highlighting their environmentally friendly nature, regulatory considerations, growing market demand, and meeting sustainability goals.

View All Submit An Event

Products

Powder Coatings - Foundation for the Novice Formulator (ebook)

Powder Coatings - Foundation for the Novice Formulator (ebook)

See More Products
PCI news now promo ad

Related Articles

  • Axalta Coating Systems Introduces ReplaShade Custom Powder Color Match Program

    See More
  • Webinar Addresses Life Cycle Cost Considerations in Selecting Fluoropolymer Coatings

    See More
  • Performance of Durable Fluoropolymer Coatings

    See More

Related Directories

  • X-Rite Pantone

    X-Rite delivers advanced color measurement and management solutions for the paints and coatings industry. Its instruments and software support precise color formulation, quality control, and consistency across production. X-Rite empowers manufacturers to achieve accurate, repeatable color, reduce waste, and enhance product appeal in decorative, industrial, and automotive coatings.
×

Keep the info flowing with our eNewsletters!

Get the latest industry updates tailored your way.

JOIN TODAY!
  • RESOURCES
    • Advertise
    • Contact Us
    • Directories
    • Store
    • Manufacturing Division
  • JOIN TODAY
    • Create Account
    • eMagazine
    • Newsletters
    • Customer Service
    • Manage Preferences
  • SERVICES
    • Marketing Services
    • Reprints
    • Market Research
    • List Rental
    • Survey & Sample
  • STAY CONNECTED
    • LinkedIn
    • Facebook
    • Youtube
    • X (Twitter)
  • PRIVACY
    • PRIVACY POLICY
    • TERMS & CONDITIONS
    • DO NOT SELL MY PERSONAL INFORMATION
    • PRIVACY REQUEST
    • ACCESSIBILITY

Copyright ©2026. All Rights Reserved BNP Media, Inc. and BNP Media II, LLC.

Design, CMS, Hosting & Web Development :: ePublishing