Painting & Coating Industry (PCI) logo Powder coating summit logo
search
cart
facebook twitter linkedin youtube
  • Sign In
  • Create Account
  • Sign Out
  • My Account
Painting & Coating Industry (PCI) logo Powder coating summit logo
  • NEWS
    • Latest News
    • Market Trends & Reports
    • Finishing News
    • Price Alerts
    • Global Top 10/ PCI 25
  • PRODUCTS
    • Product News
    • Featured Products
    • Must See Products and Services
  • MATERIALS
    • Additives
    • Resins/Polymers
    • Pigments
    • Equipment
    • Distributors
  • TECHNOLOGIES
    • Adhesives
    • Architectural Coatings
    • Finishing Articles
    • Finishing Technologies
    • Finishing Equipment
    • Industrial Coatings
    • Nanotechnology
    • Powder Coatings
    • Solventborne
    • Special Purpose Coatings
    • Sustainability
    • UV Coatings
    • Waterborne
  • EVENTS
    • Coatings Trends & Technologies Summit
    • Paint and Coatings Academy
    • Webinars
    • Calendar of Events
    • Lifetime Achievement Award
  • DIRECTORIES
    • Buyer's Guide
    • Equipment Directory
    • Materials Directory
  • RESOURCES
    • Columns
      • Did you know?
      • Distribution Dive
      • Formulating With Mike
      • Innovation Insights
      • Powder Coating Perspectives
      • TiO2 Insider
    • Blogs
      • Editor's Viewpoint
      • Industry Insights
    • Coatings Supplier Handbook
    • COAT-IT! Podcast
    • Videos
    • PCI Store
    • eBooks
    • Sponsor Insights
  • EMAGAZINE
    • eMagazine
    • Archive Issues
    • China Issue Archive
    • Editorial Advisory Board
    • CONTACT
    • Advertise
  • SIGN UP!
Paint and Coating EquipmentManufacturing Equipment

Choosing the Right Lab Mixer for Your Coating

By Del Williams, Technical Writer, Torrance, California
Kett mixer
June 9, 2025

For coatings manufacturers, laboratory mixing is an exact science. A wide variety of coatings rely on precise mixing where specific formulations, molecular structures or product characteristics are critical. Many coatings require precise formulations for optimal performance. The chemical formulation of paints and coatings also requires careful blending of pigments, binders, solvents and additives.

“The products developed in labs touch nearly every part of our lives. So, when mixing coatings, the results must be accurate, reliable and perhaps most importantly, repeatable. Consequently, utilizing the proper instruments is essential,” says John Bogart, managing director of Kett US, a manufacturer of a full range of laboratory mixing as well as moisture and organic composition measurement equipment.

The challenge is that any mixer that isn’t well suited to a lab’s requirements can be very disruptive. For example, the mixer may lack sufficient speed, leading to incomplete mixing or poor homogeneity. A mixer may also insufficiently combine materials with multiple viscosities, resulting in “ring layers” where the various viscosities settle at different depths in a poorly mixed product. These kinds of issues are problematic when mixtures or products are in laboratory development and accuracy is critical for the results to be reproducible on a larger scale.

According to Bogart, the key for coatings manufacturers is not only finding lab mixers that can perform as desired but also selecting those that can reliably do so while withstanding the toughest viscosities over time. As an industry expert, Bogart shares what coatings manufacturers need to know about selecting the most effective lab mixers for their specific applications.

Choosing the Best Mixer for Your Lab

For coatings manufacturers, the most important step to take in choosing the right mixer is determining the performance specifications that need to be met. For most labs, the prime factors to consider are speed, related torque, safety, viscosity and versatility, according to Bogart.

Kett-ZMixer.jpg

Mixing Speed and Related Torque

The optimal mixing speed depends on the chemical properties, desired reaction outcome and the specific equipment used. Mixing speeds that are too high or too low can both negatively impact the quality, safety and efficiency of the mixing process. Therefore, choosing a mixer capable of reliably providing the right mixing speed is essential for achieving uniformity, controlling reactions and ensuring the desired product characteristics.

In fluid mixing, torque plays a key role in how effectively a mixture is blended. When mixing, torque is the force that the motor applies to turn blades or impellers, which create the necessary shear and turbulence to mix the components. Adequate torque ensures that the entire fluid or material is mixed uniformly. Without enough torque, areas of the mixture may remain unmixed or may not achieve the desired properties.

Consequently, coatings manufacturers should select a mixer that satisfies their performance requirements in terms of mixing speed and related torque. To meet this need, Kett, for example, manufactures three categories of mixers that fulfill the performance specifications of coatings manufacturers.

An entry-level model with an rpm rate between 0 and 300 rotations per minute provides a related torque of 9.0 kgf·cm and is capable of withstanding high viscosities. A mid-level model can reach up to 600 rpm with related torque of 10.0 kgf·cm, which is ideal for medium-to-high viscosities. A high-performance model can reach up to 1,000 rpm with related torque of 3.0 kgf·cm, covering a low to medium viscosity range.

A basic model will typically provide forward/reverse rotation for efficient mixing. A mid-tier model will have a higher-powered motor in the range of 70 W with automatic forward/reverse rotation for improved mixing performance. A higher-end model will provide a more robust motor, such as 120 W, for high-viscosity liquids and enhanced torque, expanding its application range, according to Bogart.

Safety

Some lab mixers have inherent defects that can present problems when mixing coatings. For example, lesser mixers can have motor issues that spark during operation. Since coatings are often comprised of volatile substances, this can lead to a fire.

Brushless motors can help to eliminate the fire risk. “Brushless motors have been specially engineered to prevent sparking, nearly eliminating the risk of fire, and are entirely encased to prevent particles from creeping in and damaging the inner workings of the motor,” says Bogart.

He adds that dual safety systems, with thermal motor protection and a current limiter, can also help to protect the mixer from overheating.

Maintaining Mixing Speed

Laboratory and factory mixing can be challenging, particularly when coatings manufacture involves materials with varying viscosities. Multiple viscosities can lead to “ring layers” in a mixture, where the varying viscosities settle at different heights within the mixture, resulting in poorly mixed, inadequate materials or products.

To resolve this issue, Kett developed its Z+ model of mixers, which provide high torque regardless of the thickness or viscosity of the mixture.

“Even as mixtures change in viscosity as they are combined and materials react with one another, the speed remains constant,” says Bogart.

To expedite the mixing process and eliminate unmixed “ring regions” toward the top or bottom of a blend with varying viscosities, the OEM offers models that raise and lower when mixing. This reciprocating motion ensures that the entire batch of each coating material is entirely and evenly mixed.

Mixing Versatility

In the course of development over time, coatings manufacturers will often need to mix a wide range of formulations and sample sizes in special conditions. Consequently, it can be advantageous to have a host of options and tools available that can increase the safety, flexibility, efficiency and accuracy of mixer use.

In this vein, keyless chucks can help to streamline the change of mixing shafts with safe, secure attachment to the mixer without a key. Free-Joint™ swivel mounts enable changing shafts and adjusting the mixing height without moving the motor, according to Bogart.

Programmable settings, digital controls, LED digital displays, 0.5-second sampling frequencies and change of rotational direction with the touch of a button can improve mixer accuracy and efficiency as well, he suggests.

To further enhance safety, utilizing a remote control mixer model equipped for fume hood use, with external output for rotation speed and torque control can be helpful. A model with a remote-controlled agitator can be ideal for demanding agitation tasks and external control capabilities. Using a model that provides analog voltage outputs for rotation speed and torque, allowing viscosity monitoring with a recording meter during agitation can help to improve quality control, adds Bogart.

With all the options available, working with an expert OEM that provides a comprehensive range of mixers and accessories along with engineering assistance and technical expertise can help coatings manufacturers select the equipment most suitable for their lab. Utilizing the most accurate, reliable, repeatable and versatile equipment, in turn, will not only streamline product development but also promote quality and successful production scale-up down the line.

For more info, contact Kett: call 800-438-5388; email support@kett.com; or visit www.kett.com.

*Images courtesy of Kett. 

KEYWORDS: formulating tips innovations in coatings laboratories laboratory instruments Labs manufacturing Mixers mixing equipment Quality Control Viscosity Control viscosity measurement

Share This Story

Looking for a reprint of this article?
From high-res PDFs to custom plaques, order your copy today!

Del Williams is a technical writer based in Torrance, California. He writes about health, business, technology and educational issues.

Recommended Content

JOIN TODAY
to unlock your recommendations.

Already have an account? Sign In

  • Double exposure of creative chemistry concept on laptop background, research and development concept

    Inside the AI Shift in Coatings

    Industry leaders share real-world examples of how AI is...
    Paint and Coating Pigments
    By: PCI Editorial Staff
  • Global Top 10 and PCI Logo

    2026 Global Top 10: Top Paint and Coatings Companies

    See how the world’s largest paint and coatings companies...
    Global Top 10 and PCI 25
    By: Courtney Bassett
  • The 2026 PCI 25

    2026 PCI 25: Top Paint and Coatings Companies

    See how North America's largest paint and coatings...
    Global Top 10 and PCI 25
    By: Courtney Bassett
You must login or register in order to post a comment.

Report Abusive Comment

Manage My Account
  • eMagazine
  • Newsletters
  • Online Registration
  • Subscription Customer Service

More Videos

Sponsored Content

Sponsored Content is a special paid section where industry companies provide high quality, objective, non-commercial content around topics of interest to the PCI audience. All Sponsored Content is supplied by the advertising company and any opinions expressed in this article are those of the author and not necessarily reflect the views of PCI or its parent company, BNP Media. Interested in participating in our Sponsored Content section? Contact your local rep!

close
  • wooden kitchen set and shelving
    Sponsored bySirca North America

    Leveraging Coatings to Meet ESG Goals in Manufacturing

Popular Stories

Breaking News

16 Taken to Hospitals After Incident at Massachusetts Coating Facility

Breaking News

Yenkin-Majestic Pleads Guilty in Fatal Resin Plant Explosion Case

Solstice Logo

Solstice, Element Solutions Terminate $14.5B Deal

Webinar custom content box

Events

September 15, 2026

Coatings Trends & Technologies Summit

The Coatings Trends & Technologies (CTT) Summit is an annual conference for both liquid and powder coatings formulators and manufacturers to discuss innovations in coatings technology. This event combines high-quality technical presentations, a resource-rich exhibit hall, and dedicated networking opportunities to connect scientific minds, foster innovation, and cultivate game-changing new ideas!

January 1, 2030

Webinar Sponsorship Information

For webinar sponsorship information, visit www.bnpevents.com/webinars or email webinars@bnpmedia.com.

View All Submit An Event

Products

Advanced Coating Materials

Advanced Coating Materials

See More Products
Webinar custom content box

Related Articles

  • pci0219-PCK-838578926-900.jpg

    Choosing the Right Pasta for Your Powder Coating Dish

    See More
  • pci0123-Formulating-874157664-1170.jpg

    Selecting the Right Resin for Your Coating

    See More
  • Industry Insights Sheboygan Resins

    Choosing the Right Resin for Industrial Coatings

    See More

Related Products

See More Products
  • Hansen Solubility Parameters – A Scientific Approach for Coating Formulators (Virtual Course - 11/19/26)

  • Kevin-Biller-PC-BOOK.jpg

    Powder Coatings - Foundation for the Novice Formulator (ebook)

  • pci may 2020

    PCI May 2020 Issue

See More Products

Related Directories

  • ROSS Mixers

    Ross is a leading manufacturer of mixing, blending, drying, emulsification, homogenization, dispersion and control equipment for the paint, coatings, ink and chemical industries.
  • Myers Mixers

    Myers Mixers offers solutions for fluid and semi-solid mixing, dispersing, and homogenizing. From dispersing to complex compounding, Myers specializes in off-the-shelf and custom-designed equipment to make any mixing and dispersing process as efficient as possible. Equipment offered includes multi-shaft mixing and dispersing equipment, hydraulic ram presses, mixer controls and data-logging.
×

Keep the info flowing with our eNewsletters!

Get the latest industry updates tailored your way.

JOIN TODAY!
  • RESOURCES
    • Advertise
    • Contact Us
    • Directories
    • Store
    • Want More
    • Manufacturing Division
  • SIGN UP TODAY
    • Create Account
    • eMagazine
    • Newsletters
    • Customer Service
    • Manage Preferences
  • SERVICES
    • Marketing Services
    • Reprints
    • Market Research
    • List Rental
    • Survey & Sample
  • STAY CONNECTED
    • LinkedIn
    • Facebook
    • Youtube
    • X (Twitter)
  • PRIVACY
    • PRIVACY POLICY
    • TERMS & CONDITIONS
    • DO NOT SELL MY PERSONAL INFORMATION
    • PRIVACY REQUEST
    • ACCESSIBILITY

Copyright ©2026. All Rights Reserved BNP Media, Inc. and BNP Media II, LLC.

Design, CMS, Hosting & Web Development :: ePublishing