Nottingham Lab Automates Sample Preparation for Heat-Resistant Coatings Research

University of Nottingham researchers demonstrated a robotic workflow that prepares materials and processes them at high temperatures, an approach they are exploring for thermal barrier coatings research.
The team linked liquid dispensing, robotic sample handling and furnace processing. In a demonstration, the system prepared a precursor solution, transferred it to a furnace, managed cooling and retrieved the sample.
In related research, a Nottingham team used active learning to guide the search for low-thermal-conductivity ceramic candidates for thermal barrier coatings. The robotic workflow was described in a ChemRxiv preprint. The active-learning study appeared in Engineering Applications of Artificial Intelligence.
The demonstration points to how coating equipment for R&D can connect sample preparation with high-temperature processing.