Painting & Coating Industry (PCI) logo Powder coating summit logo
search
cart
facebook twitter linkedin youtube
  • Sign In
  • Join Today
  • Sign Out
  • My Account
Painting & Coating Industry (PCI) logo Powder coating summit logo
  • NEWS
    • Latest News
    • PCI News Now
    • Market Trends & Reports
    • Finishing News
    • Price Alerts
    • Global Top 10/ PCI 25
  • PRODUCTS
    • Product News
    • Featured Products
    • Must See Products and Services
  • MATERIALS
    • Additives
    • Resins/Polymers
    • Pigments
    • Equipment
    • Distributors
  • TECHNOLOGIES
    • Adhesives
    • Architectural Coatings
    • Finishing Articles
    • Finishing Technologies
    • Finishing Equipment
    • Industrial Coatings
    • Nanotechnology
    • Powder Coatings
    • Solventborne
    • Special Purpose Coatings
    • Sustainability
    • UV Coatings
    • Waterborne
  • EVENTS
    • Coatings Trends & Technologies Summit
    • Paint and Coatings Academy
    • Webinars
    • Calendar of Events
    • Lifetime Achievement Award
  • DIRECTORIES
    • Buyer's Guide
    • Equipment Directory
    • Materials Directory
  • RESOURCES
    • Columns
      • Did you know?
      • Distribution Dive
      • Formulating With Mike
      • Innovation Insights
      • Powder Coating Perspectives
      • TiO2 Insider
    • Blogs
      • Editor's Viewpoint
      • Industry Insights
    • Coatings Supplier Handbook
    • COAT-IT! Podcast
    • Videos
    • PCI Store
    • eBooks
    • Sponsor Insights
  • EMAGAZINE
    • eMagazine
    • Archive Issues
    • Editorial Advisory Board
    • CONTACT
    • Advertise
  • JOIN!
Company NewsFinishing News

Boreal Bioproducts and Emulco Partner on Bio-Based Barrier Coatings

GettyImages-1170x878-1392287714.jpg
Getty Images/iStockphoto
Sakorn Sukkasemsakorn, iStock / Getty Images Plus, via Getty Images. 
November 26, 2026

Finnish biorefinery startup Boreal Bioproducts and Belgian emulsion technology specialist Emulco have signed a joint development agreement to develop and commercialize fully bio-based barrier coatings for paper and fiber-based food packaging.

The companies aim to combine Boreal's SpruceSugar material with Emulco's AquaVeg coating technology to provide grease, oxygen, water and water-vapor resistance without relying on conventional plastic- or PFAS-based barrier systems.

The agreement follows two years of collaboration during which the companies evaluated the complementary properties of their materials and identified potential formulation approaches.

Combining Complementary Barrier Technologies

SpruceSugar is a galactoglucomannan, the principal hemicellulose found in spruce wood, recovered from forestry side streams. Within the proposed coating system, the material is intended to act as a binder while providing grease and oxygen barrier properties.

Boreal currently produces SpruceSugar at pilot scale at its Turku, Finland, facility, supplying material to industrial customers for application trials and laboratory-scale product validation.

Emulco's AquaVeg technology is based on vegetable-wax emulsions designed to provide resistance to water and water vapor.

The company has manufactured wax emulsions since 1996 and has produced water-based bio-emulsions and coatings at its Ghent, Belgium, facility since 2014.

By combining these materials, the partners aim to develop a coating architecture in which individual bio-based components perform different barrier functions. The formulation strategy is intended to achieve the required properties without relying on extensive chemical modification of the starting materials.

The companies are also incorporating recyclability and compatibility with industrial coating and converting processes into the development program.

Development and Scale-Up Plans

The first development phase, now underway, focuses on laboratory formulation, performance testing and optimization.

If successful, selected formulations will advance to pilot-scale and roll-to-roll coating trials. In these processes, coating formulations are applied continuously to a moving paper web, allowing the companies to evaluate performance under conditions more representative of industrial packaging production.

Further trials with packaging manufacturers would evaluate the materials in actual packaging applications.

The companies have not announced commercial production dates or final performance specifications for the combined coating system.

Marja Jaurakkajärvi, chief commercial officer of Boreal Bioproducts, said replacing plastics requires combining materials with complementary properties rather than relying on a single universal substitute.

"Our strength at Boreal Bioproducts is transforming underutilised forestry side streams into functional raw materials. Emulco brings emulsion technology and industrial scale-up," Jaurakkajärvi said.

Jean Vanhoebost, managing director of Emulco, said the companies' earlier collaboration demonstrated how SpruceSugar and AquaVeg address different barrier requirements.

He said the new agreement provides a framework for continuing development of coatings designed around the specific performance needs of individual packaging applications.

Regulatory Pressure on Packaging Materials

The development comes as European packaging rules place additional requirements on material selection, recyclability and substances used in food-contact applications.

The European Union's Packaging and Packaging Waste Regulation (EU) 2025/40 began applying August 12, 2026. Among its provisions are restrictions on PFAS concentrations in food-contact packaging.

Additional harmonized design-for-recycling requirements are scheduled to apply beginning January 1, 2030, or later depending on the implementation timetable established in the regulation.

These requirements are increasing interest in barrier systems that can provide the moisture, oxygen and grease resistance required for fiber packaging while supporting recyclability and reducing reliance on fossil-based materials.

Boreal Bioproducts, founded in 2018, develops bio-based ingredients from forestry side streams for industrial applications, including coatings, adhesives and packaging. Emulco develops and produces emulsions for food-contact packaging and other industrial applications, including polymer-based systems.

The development program represents an early-stage approach to replacing conventional barrier technologies, with commercial feasibility dependent on the results of laboratory, pilot-scale and packaging-converter trials.


For coatings formulators, the collaboration highlights an approach to developing multifunctional barrier systems through combinations of renewable binders and water-based emulsion technologies.

KEYWORDS: barriers bio-based bio-based coatings

Share This Story

Looking for a reprint of this article?
From high-res PDFs to custom plaques, order your copy today!

Recommended Content

JOIN TODAY
to unlock your recommendations.

Already have an account? Sign In

  • Double exposure of creative chemistry concept on laptop background, research and development concept

    Inside the AI Shift in Coatings

    Industry leaders share real-world examples of how AI is...
    Architectural Coatings
    By: PCI Editorial Staff
  • Global Top 10 and PCI Logo

    2026 Global Top 10: Top Paint and Coatings Companies

    See how the world’s largest paint and coatings companies...
    Global Top 10 and PCI 25
    By: Courtney Bassett
  • The 2026 PCI 25

    2026 PCI 25: Top Paint and Coatings Companies

    See how North America's largest paint and coatings...
    Global Top 10 and PCI 25
    By: Courtney Bassett
You must login or register in order to post a comment.

Report Abusive Comment

Manage My Account
  • Join Paint & Coatings Industry
  • Manage My Preferences
  • Customer Service

More Videos

Popular Stories

Mergers and aquisitions

BASF Ends Evonik Takeover Pursuit

Breaking News

H.B. Fuller to Close Seven Sites in Supply-Chain Overhaul

AkzoNobel Axalta

EU Clears $25B Akzo-Axalta Merger with One Big Condition

Events

December 2, 2026

Self-Activated Binder Technology: A New Path to Tin-Free Polyurethane Coatings

Through examples from protective and general industrial coating applications, attendees will learn how these innovative technologies can help maintain, and in some cases improve, coating performance while supporting safer, more sustainable formulations that align with evolving regulatory expectations

December 10, 2026

PC Academy: Waterborne Polymers and Film Formation

The trend towards waterborne polymers in the paint and coatings industry is clear; highlighting their environmentally friendly nature, regulatory considerations, growing market demand, and meeting sustainability goals.

View All Submit An Event

Products

Powder Coatings - Foundation for the Novice Formulator (ebook)

Powder Coatings - Foundation for the Novice Formulator (ebook)

See More Products
PCI news now promo ad

Related Articles

  • Market Reports.jpg

    Water-Based Barrier Coatings Market Headed for $1.85B

    See More
  • Repura Stahl Coating

    Barrier Coatings Support Paper-Based Packaging

    See More
  • Mono_PE_pet_food_bag.jpg

    Inline Printable Barrier Coatings that Enable Mono-Material Pet Food Packaging

    See More

Related Products

See More Products
  • pci march 2020

    PCI March 2020 Issue

See More Products

Related Directories

  • Integrity Bio-Chemicals

    Integrity BioChem delivers innovative, patented bio-based surfactants and dispersants designed to enhance performance in paints and coatings applications. Proudly manufactured in the USA, with additional global manufacturing capabilities in Europe and Australia, our sustainable solutions combine advanced chemistry, renewable raw materials, and reliable supply to support the evolving needs of the coatings industry..
×

Keep the info flowing with our eNewsletters!

Get the latest industry updates tailored your way.

JOIN TODAY!
  • RESOURCES
    • Advertise
    • Contact Us
    • Directories
    • Store
    • Manufacturing Division
  • JOIN TODAY
    • Create Account
    • eMagazine
    • Newsletters
    • Customer Service
    • Manage Preferences
  • SERVICES
    • Marketing Services
    • Reprints
    • Market Research
    • List Rental
    • Survey & Sample
  • STAY CONNECTED
    • LinkedIn
    • Facebook
    • Youtube
    • X (Twitter)
  • PRIVACY
    • PRIVACY POLICY
    • TERMS & CONDITIONS
    • DO NOT SELL MY PERSONAL INFORMATION
    • PRIVACY REQUEST
    • ACCESSIBILITY

Copyright ©2026. All Rights Reserved BNP Media, Inc. and BNP Media II, LLC.

Design, CMS, Hosting & Web Development :: ePublishing