    • Weekly Featured Article
    • COATLE Word Game
  • PRODUCTS
    • Product News
    • Featured Products
    • Must See Products and Services
  • MATERIALS
    • Additives
    • Resins/Polymers
    • Pigments
    • Equipment
    • Distributors
  • TECHNOLOGIES
    • Adhesives
    • Architectural Coatings
    • Finishing Articles
    • Finishing Technologies
    • Finishing Equipment
    • Industrial Coatings
    • Nanotechnology
    • Powder Coatings
    • Solventborne
    • Special Purpose Coatings
    • Sustainability
    • UV Coatings
    • Waterborne
  • RESOURCES
    • Columns
      • Did you know?
      • Distribution Dive
      • Formulating With Mike
      • Innovation Insights
      • Powder Coating Perspectives
      • TiO2 Insider
    • Blogs
      • Editor's Viewpoint
      • Industry Insights
    • Coatings Supplier Handbook
    • Podcasts and Videos
      • COAT-IT! Podcast
      • Videos/PCI TV
    • PCI Store
    • Classifieds
    • eBooks
    • Sponsor Insights
    • White Papers
    • COATLE Word Game
  • EVENTS
    • Coatings Trends & Technologies Summit
    • Paint and Coatings Academy
    • Webinars
    • Calendar of Events
    • Lifetime Achievement Award
  • DIRECTORIES
    • Buyer's Guide
    • Equipment Directory
    • Materials Directory
  • EMAGAZINE
    • Current Issue
    • eMagazine Archive
    • China Issue Archive
    • Editorial Advisory Board
  • CONTACT
    • Contact Us
    • Advertise
    • Subscribe to eMagazine
    • Subscribe to Newsletters
  • SIGN UP!

Launch of New Technology for Safer Solvents

September 1, 2009
The launch of a new facility will revolutionize the industrial processes of electropolishing, metal oxide processing and electroplating.

The launch of a new facility that will revolutionize the industrial processes of electropolishing, metal oxide processing and electroplating took place on June 3, when a pioneering Ionics Liquid Demonstrator was formally launched at the University of Leicester in the United Kingdom by the Vice Chancellor Professor Robert Burgess.

The development of this multi-application pilot plant facility has been carried out by Professor Andy Abbott, Head of the University’s Department of Chemistry and Director of the University spin-out company, Scionix, in collaboration with the Leicester Shire Economic Partnership (LSEP).

The Ionic Liquids Demonstrator (ILD) project builds on the historic and ongoing research and development activities in the Green Chemistry group at the University of Leicester to transfer its ionic liquids applications know-how to Leicestershire business.

Ionic liquids are fluid at ambient temperatures. They have several advantages over conventional molecular solvents, making them a viable environmentally compatible alternative to traditional solvents. Ionic liquids have physical properties that make them very interesting as potential solvents for synthesis.

The University of Leicester has established a multi-application pilot plant facility at the university offering a range of small-scale process demonstrations in the practical application of ionic liquids to metal-related industrial processes.

The Leicester ionic liquid applications have real potential to bring new value-added gains to existing businesses within the sub-region.

As an environmentally friendly, non-toxic substitute for current processes, their use would create both health, and safety and environmental benefits, in addition to competitive product advantage achieved through better tailoring of product characteristics (hardness, fineness, adherence, etc.).

By removing harsh acid-based processes, ionic liquid applications improve energy efficiency and decrease the emission of chemicals to the environment.

The project will work with local businesses to encourage end users to explore and evaluate, in a tangible way, the benefits of industrial processes based on ionic liquids.

Most of the solvents Scionix has developed are based on vitamin B4 (choline chloride), which is safe and easy to manufacture in large quantities.  Its use does not have to be registered. By combining the basic liquid with other molecules or salts a range of processes can be tailored to individual companies’ use.

Professor Andy Abbott commented, “This is a fantastic opportunity for us to collaborate with local industry and hopefully bring new technology to expand their product ranges. Our local partnerships have so far been very successful and we would like to extend them using this unit.”

Nick Carter, chairman of Prospect Leicestershire, said, “Our universities are a tremendous resource for the local economy. This initiative by the University of Leicester has the potential to help local businesses with cutting edge technology – as well as enhancing the reputation of the university nationally and internationally.”

Scionix was launched in 1999 and is a partnership between the University of Leicester Department of Chemistry and the London-based company Whyte Chemicials. Prospect Leicestershire is the new economic development company for Leicester and Leicestershire. Its responsibilities include continuing the regeneration of the city and delivering inward investment, business innovation and support and facilitating economic growth.

LSEP was a not-for-profit company established by the East Midlands Development Agency to promote economic development in Leicester and Leicestershire.

For more information on this please contact Professor Andy Abbott, Head of the Department of Chemistry and Director of Scionix, tel +44 (0) 116 252 2087, e-mail apa1@le.ac.uk.

Share This Story

Looking for a reprint of this article?
From high-res PDFs to custom plaques, order your copy today!

Recommended Content

JOIN TODAY
to unlock your recommendations.

Already have an account? Sign In

  • pci1022-Kinaltek-Lead-1170.jpg

    A Novel Pigment Production Technology

    Following an extensive R&D program that demonstrated...
    Paint and Coating Pigments
    By: Jawad Haidar and Nitin Soni
  • pci global top 10

    2025 Global Top 10: Top Paint and Coatings Companies

    The following is PCI’s annual ranking of the top 10...
    Paint and Coating Market Reports
    By: Courtney Bassett
  • 2025 pci 25

    2025 PCI 25: Top Paint and Coatings Companies

    PCI's annual ranking of the top 25 North American paint...
    Global Top 10 and PCI 25
    By: Courtney Bassett
You must login or register in order to post a comment.

Report Abusive Comment

Manage My Account
  • eMagazine
  • Newsletters
  • Online Registration
  • Subscription Customer Service

More Videos

Sponsored Content

Sponsored Content is a special paid section where industry companies provide high quality, objective, non-commercial content around topics of interest to the PCI audience. All Sponsored Content is supplied by the advertising company and any opinions expressed in this article are those of the author and not necessarily reflect the views of PCI or its parent company, BNP Media. Interested in participating in our Sponsored Content section? Contact your local rep!

close
  • man woodworking in workshop
    Sponsored byGemini Industries, Inc.

    Waterborne Coatings Aren't the Future -- They're the New Performance Benchmark

  • colorful building exterior
    Sponsored byDow

    Insights into Exterior Architectural Coating Degradation: Bridging Accelerated and Natural Weathering

Popular Stories

AkzoNobel Annual Report

AkzoNobel Reports Margin Gains and Portfolio Shifts

PPG announced the installation of a state-of-the-art pilot finishing line that features IPG’s PhotoniCURE™ laser curing system at its powder manufacturing and technical facility in Strongsville, Ohio.

PPG Tests New Laser-Based Approach to Powder Coating Curing

Business network concept. Human Resources. Group of businesspeople. Management strategy

Sun Chemical Plans $10M Quinacridone Investment

pci academy

PCI Buyers Guide

Submit a Request for Proposal (RFP) to suppliers of your choice with details on what you need with a click of a button

Start your RFP

Browse our Buyers Guide for manufacturers and distributors of all types of coatings products and much more!

Find Suppliers

Events

September 4, 2025

N-Butylpyrrolidone (NBP) as a Green Solvent to Replace N-Methylpyrrolidone (NMP) in Industrial Coating Applications

ON DEMAND: EPA published a regulation proposal around N-methylpyrrolidone (NMP) in June 2024 to ban or limit NMP in many applications, such as paints and coatings and their removers. N-butylpyrrolidone (NBP) is a powerful and versatile solvent for a variety of industries looking for alternatives to substance of very high concern (SVHC)-listed solvents.

March 24, 2026

The Manufacturing & Automation eXchange (MAX)

MAX presents a rare opportunity to observe the full scope of manufacturing in one environment. From systems integration and materials handling to automation, quality, safety, and packaging, each discipline is represented through live, operational displays. By experiencing these technologies side by side, as they are on actual production floors, attendees gain a grounded understanding of how manufacturing functions align, overlap, and evolve in practice.

View All Submit An Event

Poll

Longest-running laboratory experiment

What is the longest-running laboratory experiment?
View Results Poll Archive

Products

Automotive Paints and Coatings, 2nd Edition

Now in its second edition and still the only book of its kind, this is an authoritative treatment of all stages of the coating process.

See More Products
Register for PCI Academy course: Surfactants and Rheology

PCI webinar arkema

Related Articles

  • pci0819-Circa-913786496-900.jpg

    New Bio-Based Solvent Supports Quest for Safer and More Sustainable Coatings

    See More
  • Sansin Introduces Color System for its Interior Enviro Stain; Safer, Far Less Toxic Alternative to Traditional Dyes

    See More
  • SCAQMD Asked to Reconsider New Rules on Use of Cleanup Solvents

    See More

Related Products

See More Products
  • Handbook of Adhesives and Surface Preparation

  • organic coatings.jpg

    Organic Coatings: Science and Technology, 4th Edition

  • 9780323355957.jpg

    Adhesives Technology Handbook, 3rd Edition

See More Products

Related Directories

  • Vertec BioSolvents Inc.

    Sustainable, safe, bio-based performance solvents and blends from renewable resources to replace petroleum-based solvents for formulating, blending and cleaning.
×

Keep the info flowing with our eNewsletters!

Get the latest industry updates tailored your way.

JOIN TODAY!
  • RESOURCES
    • Advertise
    • Contact Us
    • Directories
    • Store
    • Want More
    • Manufacturing Division
  • SIGN UP TODAY
    • Create Account
    • eMagazine
    • Newsletters
    • Customer Service
    • Manage Preferences
  • SERVICES
    • Marketing Services
    • Reprints
    • Market Research
    • List Rental
    • Survey & Sample
  • STAY CONNECTED
    • LinkedIn
    • Facebook
    • Youtube
    • X (Twitter)
  • PRIVACY
    • PRIVACY POLICY
    • TERMS & CONDITIONS
    • DO NOT SELL MY PERSONAL INFORMATION
    • PRIVACY REQUEST
    • ACCESSIBILITY

Copyright ©2026. All Rights Reserved BNP Media, Inc. and BNP Media II, LLC.

Design, CMS, Hosting & Web Development :: ePublishing