Painting & Coating Industry (PCI) logo Powder coating summit logo
search
cart
facebook twitter linkedin youtube
  • Sign In
  • Join Today
  • Sign Out
  • My Account
Painting & Coating Industry (PCI) logo Powder coating summit logo
  • NEWS
    • Latest News
    • PCI News Now
    • Market Trends & Reports
    • Finishing News
    • Price Alerts
    • Global Top 10/ PCI 25
  • PRODUCTS
    • Product News
    • Featured Products
    • Must See Products and Services
  • MATERIALS
    • Additives
    • Resins/Polymers
    • Pigments
    • Equipment
    • Distributors
  • TECHNOLOGIES
    • Adhesives
    • Architectural Coatings
    • Finishing Articles
    • Finishing Technologies
    • Finishing Equipment
    • Industrial Coatings
    • Nanotechnology
    • Powder Coatings
    • Solventborne
    • Special Purpose Coatings
    • Sustainability
    • UV Coatings
    • Waterborne
  • EVENTS
    • Coatings Trends & Technologies Summit
    • Paint and Coatings Academy
    • Webinars
    • Calendar of Events
    • Lifetime Achievement Award
  • DIRECTORIES
    • Buyer's Guide
    • Equipment Directory
    • Materials Directory
  • RESOURCES
    • Columns
      • Did you know?
      • Distribution Dive
      • Formulating With Mike
      • Innovation Insights
      • Powder Coating Perspectives
      • TiO2 Insider
    • Blogs
      • Editor's Viewpoint
      • Industry Insights
    • Coatings Supplier Handbook
    • COAT-IT! Podcast
    • Videos
    • PCI Store
    • eBooks
    • Sponsor Insights
  • EMAGAZINE
    • eMagazine
    • Archive Issues
    • Editorial Advisory Board
    • CONTACT
    • Advertise
  • JOIN!
Breaking News

Study Suggests 'Self-Cleaning' Pollution-Control Technology Could Do More Harm Than Good

July 22, 2013

BLOOMINGTON, IN - Research by Indiana University environmental scientists shows that air-pollution-removal technology used in "self-cleaning" paints and building surfaces may actually cause more problems than they solve.

The study finds that titanium dioxide coatings, seen as promising for their role in breaking down airborne pollutants on contact, are likely in real-world conditions to convert abundant ammonia to nitrogen oxide, the key precursor of harmful ozone pollution.

"As air quality standards become more stringent, people are going to be thinking about other technologies that can reduce pollution," said Jonathan D. Raff, Assistant Professor in the School of Public and Environmental Affairs at IU Bloomington and an author of the study. "Our research suggests that this may not be one of them."

"Photooxidation of Ammonia on TiO2 as a Source of NO and NO2 under Atmospheric Conditions" is being published by the Journal of the American Chemical Society and is available online. Other authors include SPEA doctoral students Mulu Kebede and Nicole Scharko, Mychel Varner of the University of California-Irvine and R. Benny Gerber of UC-Irvine and the Hebrew University in Jerusalem.

The researchers calculate that, in areas where the titanium dioxide technology is used, ammonia degradation could account for up to 13 percent of the nitrogen oxides in the immediate vicinity. This suggests that widespread use of the technology could contribute significantly to ozone formation.

The findings are timely because the Environmental Protection Agency is developing stricter regulations for ground-level ozone, a primary component in photochemical smog. The pollution is linked to serious health problems, including breathing difficulties and heart and lung disease.

Ozone is produced by reactions involving nitrogen oxides (NOx), which come primarily from motor vehicle emissions, and VOCs resulting from industrial processes. Equipping cars with catalytic converters has been effective at reducing ozone in urban areas, but different technologies may be needed to meet tighter air-quality standards of the future.

The need has sparked interest in titanium dioxide. The compound acts as a photocatalyst, breaking down nitrogen oxides, ammonia and other pollutants in the presence of sunlight. "Self-cleaning" surfaces coated with titanium dioxide can break down chemical grime that will otherwise adhere to urban buildings. News stories have celebrated "smog-eating" tiles and concrete surfaces coated with the compound.

But Raff and his colleagues show that, in normal environmental conditions, titanium dioxide also catalyzes the incomplete breakdown of ammonia into nitrogen oxides. Ammonia is an abundant constituent in motor vehicle emissions, and its conversion to nitrogen oxides could result in increases in harmful ozone concentrations.

"We show that uptake of atmospheric NH3 (ammonia) onto surfaces containing TiO2 is not a permanent removal process, as previously thought, but rather a photochemical route for generating reactive oxides of nitrogen that play a role in air pollution and are associated with significant health effects," the authors write.

Raff, who is also an Adjunct Professor of Chemistry in the IU College of Arts and Sciences, said other studies missed the effect on ammonia because they investigated reactions that occur with high levels of emissions under industrial conditions, not the low levels and actual humidity levels typically present in urban environments.

The findings also call into question other suggestions for using titanium dioxide for environmental remediation -- for example, to remove odor-causing organic compounds from emissions produced by confined livestock feeding operations. Titanium dioxide has also been suggested as a geo-engineering substance that could be injected into the upper atmosphere to reflect sunlight away from the Earth and combat global warming.

Further studies in Raff's lab are aimed at producing better understanding of the molecular processes involved when titanium dioxide catalyzes the breakdown of ammonia. The results could suggest approaches for developing more effective pollution-control equipment as well as improvements in industrial processes involving ammonia.

KEYWORDS: Self-Cleaning Coating

Share This Story

Looking for a reprint of this article?
From high-res PDFs to custom plaques, order your copy today!

Recommended Content

JOIN TODAY
to unlock your recommendations.

Already have an account? Sign In

  • Double exposure of creative chemistry concept on laptop background, research and development concept

    Inside the AI Shift in Coatings

    Industry leaders share real-world examples of how AI is...
    Paint and Coating Pigments
    By: PCI Editorial Staff
  • Global Top 10 and PCI Logo

    2026 Global Top 10: Top Paint and Coatings Companies

    See how the world’s largest paint and coatings companies...
    Global Top 10 and PCI 25
    By: Courtney Bassett
  • The 2026 PCI 25

    2026 PCI 25: Top Paint and Coatings Companies

    See how North America's largest paint and coatings...
    Global Top 10 and PCI 25
    By: Courtney Bassett
You must login or register in order to post a comment.

Report Abusive Comment

Manage My Account
  • Join Paint & Coatings Industry
  • Manage My Preferences
  • Customer Service

More Videos

Popular Stories

Mergers and aquisitions

BASF Ends Evonik Takeover Pursuit

industry news

Dozens Treated After Toledo Chemical Release

Breaking News

H.B. Fuller to Close Seven Sites in Supply-Chain Overhaul

Events

December 2, 2026

Self-Activated Binder Technology: A New Path to Tin-Free Polyurethane Coatings

Through examples from protective and general industrial coating applications, attendees will learn how these innovative technologies can help maintain, and in some cases improve, coating performance while supporting safer, more sustainable formulations that align with evolving regulatory expectations

December 10, 2026

PC Academy: Waterborne Polymers and Film Formation

The trend towards waterborne polymers in the paint and coatings industry is clear; highlighting their environmentally friendly nature, regulatory considerations, growing market demand, and meeting sustainability goals.

View All Submit An Event

Products

Powder Coatings - Foundation for the Novice Formulator (ebook)

Powder Coatings - Foundation for the Novice Formulator (ebook)

See More Products
PCI news now promo ad

Related Articles

  • Chemical companies

    Lubrizol’s Science Lends Support During COVID-19, Company Pledges $2 Million to Do Even More

    See More
  • UQ's Dr Asep Nugraha is developing a self-healing rust-proof coating that could protect steel structures for hundreds of years.

    Self-Repairing Waterborne Coating Slows Corrosion More Than 600-Fold

    See More
  • Air Control Offers More Than Just Safety

    See More

Events

View AllSubmit An Event
  • December 2, 2026

    Self-Activated Binder Technology: A New Path to Tin-Free Polyurethane Coatings

    Through examples from protective and general industrial coating applications, attendees will learn how these innovative technologies can help maintain, and in some cases improve, coating performance while supporting safer, more sustainable formulations that align with evolving regulatory expectations
View AllSubmit An Event

Related Directories

  • Epcon Industrial Systems LP

    Founded in 1977, Epcon has grown from a one-man operation to a global leader in developing and manufacturing innovative air pollution control technology and industrial heating equipment. Prime and Finish Coil Coating Ovens; Air Pollution Control for VOC / NOx Abatement; Heat Recovery Systems including Hot Water Heaters for Coil Coating lines
×

Keep the info flowing with our eNewsletters!

Get the latest industry updates tailored your way.

JOIN TODAY!
  • RESOURCES
    • Advertise
    • Contact Us
    • Directories
    • Store
    • Manufacturing Division
  • JOIN TODAY
    • Create Account
    • eMagazine
    • Newsletters
    • Customer Service
    • Manage Preferences
  • SERVICES
    • Marketing Services
    • Reprints
    • Market Research
    • List Rental
    • Survey & Sample
  • STAY CONNECTED
    • LinkedIn
    • Facebook
    • Youtube
    • X (Twitter)
  • PRIVACY
    • PRIVACY POLICY
    • TERMS & CONDITIONS
    • DO NOT SELL MY PERSONAL INFORMATION
    • PRIVACY REQUEST
    • ACCESSIBILITY

Copyright ©2026. All Rights Reserved BNP Media, Inc. and BNP Media II, LLC.

Design, CMS, Hosting & Web Development :: ePublishing