Painting & Coating Industry (PCI) logo Powder coating summit logo
search
cart
facebook twitter linkedin youtube
  • Sign In
  • Create Account
  • Sign Out
  • My Account
Painting & Coating Industry (PCI) logo Powder coating summit logo
  • NEWS
    • Latest News
    • Market Trends & Reports
    • Finishing News
    • Price Alerts
    • Global Top 10/ PCI 25
  • PRODUCTS
    • Product News
    • Featured Products
    • Must See Products and Services
  • MATERIALS
    • Additives
    • Resins/Polymers
    • Pigments
    • Equipment
    • Distributors
  • TECHNOLOGIES
    • Adhesives
    • Architectural Coatings
    • Finishing Articles
    • Finishing Technologies
    • Finishing Equipment
    • Industrial Coatings
    • Nanotechnology
    • Powder Coatings
    • Solventborne
    • Special Purpose Coatings
    • Sustainability
    • UV Coatings
    • Waterborne
  • EVENTS
    • Coatings Trends & Technologies Summit
    • Paint and Coatings Academy
    • Webinars
    • Calendar of Events
    • Lifetime Achievement Award
  • DIRECTORIES
    • Buyer's Guide
    • Equipment Directory
    • Materials Directory
  • RESOURCES
    • Columns
      • Did you know?
      • Distribution Dive
      • Formulating With Mike
      • Innovation Insights
      • Powder Coating Perspectives
      • TiO2 Insider
    • Blogs
      • Editor's Viewpoint
      • Industry Insights
    • Coatings Supplier Handbook
    • COAT-IT! Podcast
    • Videos
    • PCI Store
    • eBooks
    • Sponsor Insights
  • EMAGAZINE
    • eMagazine
    • Archive Issues
    • Editorial Advisory Board
    • CONTACT
    • Advertise
  • SIGN UP!
Home » Surfactants

Articles Tagged with ''Surfactants''

Distributors.jpg

Brenntag Expands Distribution Agreement with Kao Chemicals

May 12, 2023
No Comments

Brenntag and Kao have a long-standing successful partnership in Sweden and Norway, and will now serve customers in the entire Nordic region with a portfolio of surfactant solutions.


Read More
abstract design for European Coatings Show

Laser-Focused on Sustainability

Kristin Johansson
May 7, 2023
2 Comments

Sustainability dominated every conversation at the 2023 European Coatings Show. Learn about some of the innovative technologies that were introduced to help the industry formulate, manufacture, and apply the coatings of tomorrow.


Read More
pci0323-BASF-167762605-1170.jpg

Alternatives to Fluorosurfactants for Water-Based Floor-Care Coatings

Tony Moy
March 2, 2023
No Comments

Increased regulatory pressure around the use of fluorosurfactants has led to a search for alternative surfactants that still provide good wetting and leveling attributes.


Read More
pci0323-Formulating-F2-1170.jpg

Study of Surfactant Tail Variations, Part 2

Mike Praw
March 1, 2023
No Comments

Learn how the amount of actual dispersant added on pigment solids will have an effect on tinting power, stability, compatibility of formulations, and other properties.


Read More
pci0123-Formulating-874157664-1170.jpg

Study of Surfactant Tail Variations, Part One

Mike Praw
February 7, 2023
No Comments

This month's Formulating with Mike column discusses the development of surfactant molecules for use as a carbon black pigment dispersant. 


Read More
pci1122-DidYouKnowq-F1-1170.jpg

How are Surfactants Distributed within Latex?

Emulsion Polymers Consulting and Education (EPCEd)
November 4, 2022
No Comments

The surfactants we add to synthetic latexes have allowed us to create wonderful nanoparticles and at the same time provide colloidal stability to the dispersions. But they also can cause foaming problems when mixing and transporting the latexes, and remain in the final products, causing potential water absorption problems in films and coatings. 


Read More
Photo of the groundbreaking ceremony for Colonial Chemical M.E. Arabia

Colonial Chemical Breaks Ground on New Plant in Saudi Arabia

June 2, 2022
No Comments

Colonial Chemical Inc. held a groundbreaking earlier this year for a new specialty chemicals manufacturing plant in Dammam, Saudi Arabia. 


Read More

Indorama Ventures Acquires Oxiteno

April 12, 2022
No Comments

Chemical company Indorama Ventures Public Co. Ltd. (IVL) recently completed its acquisition of Brazil-based Oxiteno S.A. Indústria e Comércio.


Read More
Image of chart explaining Clariant's Vita range

Clariant Launches 100% Bio-Based Surfactants Range

February 8, 2022
One Comment

Clariant has unveiled its new Vita 100% bio-based surfactants and polyethylene glycols (PEGs) to help directly address climate change by helping remove fossil carbon from the value chain. 


Read More
pilot chemical
advertisement

Anionic Surfactants for All Your EP Applications

February 7, 2022
No Comments
Pilot Chemical is the world’s largest manufacturer of disulfonates and owns the most state-of-the-art continuous-sulfonation process in North America.
Read More
Previous 1 2 3 4 5 6 7 8 9 10 Next
Manage My Account
  • eMagazine
  • Newsletters
  • Online Registration
  • Subscription Customer Service

More Videos

Popular Stories

Evonik Logo

Evonik to Close Two German Sites

Mergers-and-Company-Strategies.jpg

BASF Confirms Exploratory Talks on Potential Evonik Takeover

Breaking News

Evonik Rejected €10.3 Billion BASF Offer, Reuters Reports

Webinar custom content box

Events

October 8, 2026

AI-Powered Reformulation: Finding PFAS-Free, Lower-VOC Formulations Faster

In this webinar, we will use case studies from industry to illustrate how AI can be used to identify PFAS-free formulations and select surfactant blends for water-based products.

January 1, 2030

Webinar Sponsorship Information

For webinar sponsorship information, visit www.bnpevents.com/webinars or email webinars@bnpmedia.com.

View All Submit An Event

Products

Advanced Coating Materials

Advanced Coating Materials

See More Products
Webinar custom content box

Keep the info flowing with our eNewsletters!

Get the latest industry updates tailored your way.

JOIN TODAY!
  • RESOURCES
    • Advertise
    • Contact Us
    • Directories
    • Store
    • Want More
    • Manufacturing Division
  • SIGN UP TODAY
    • Create Account
    • eMagazine
    • Newsletters
    • Customer Service
    • Manage Preferences
  • SERVICES
    • Marketing Services
    • Reprints
    • Market Research
    • List Rental
    • Survey & Sample
  • STAY CONNECTED
    • LinkedIn
    • Facebook
    • Youtube
    • X (Twitter)
  • PRIVACY
    • PRIVACY POLICY
    • TERMS & CONDITIONS
    • DO NOT SELL MY PERSONAL INFORMATION
    • PRIVACY REQUEST
    • ACCESSIBILITY

Copyright ©2026. All Rights Reserved BNP Media, Inc. and BNP Media II, LLC.

Design, CMS, Hosting & Web Development :: ePublishing