Painting & Coating Industry (PCI) logo Powder coating summit logo
search
cart
facebook twitter linkedin youtube
  • Sign In
  • Join Today
  • Sign Out
  • My Account
Painting & Coating Industry (PCI) logo Powder coating summit logo
  • NEWS
    • Latest News
    • PCI News Now
    • Market Trends & Reports
    • Finishing News
    • Price Alerts
    • Global Top 10/ PCI 25
  • PRODUCTS
    • Product News
    • Featured Products
    • Must See Products and Services
  • MATERIALS
    • Additives
    • Resins/Polymers
    • Pigments
    • Equipment
    • Distributors
  • TECHNOLOGIES
    • Adhesives
    • Architectural Coatings
    • Finishing Articles
    • Finishing Technologies
    • Finishing Equipment
    • Industrial Coatings
    • Nanotechnology
    • Powder Coatings
    • Solventborne
    • Special Purpose Coatings
    • Sustainability
    • UV Coatings
    • Waterborne
  • EVENTS
    • Coatings Trends & Technologies Summit
    • Paint and Coatings Academy
    • Webinars
    • Calendar of Events
    • Lifetime Achievement Award
  • DIRECTORIES
    • Buyer's Guide
    • Equipment Directory
    • Materials Directory
  • RESOURCES
    • Columns
      • Did you know?
      • Distribution Dive
      • Formulating With Mike
      • Innovation Insights
      • Powder Coating Perspectives
      • TiO2 Insider
    • Blogs
      • Editor's Viewpoint
      • Industry Insights
    • Coatings Supplier Handbook
    • COAT-IT! Podcast
    • Videos
    • PCI Store
    • eBooks
    • Sponsor Insights
  • EMAGAZINE
    • eMagazine
    • Archive Issues
    • Editorial Advisory Board
    • CONTACT
    • Advertise
  • JOIN!
Home » polyurethane coatings

Articles Tagged with ''polyurethane coatings''

Empty underground parking in modern building with new floor

Water-Based Polyester Polyol Dispersion for VOC-Compliant, Ambient-Cure Polyurethane Floor Coatings

Dr. Ashish Zore C. Dylan Thomas Dr. Nitin Sharma Max Calenberg Taylor Scicchitano
February 5, 2025
No Comments

A DIY garage floor coating system uses a waterborne resin to achieve low VOCs, lasting durability, and high performance for industrial and consumer applications.


Read More
Web-GettyImages-873600660-1170x658.jpg

Anti-Fatberg Invention Could Help Unclog City Sewers

Will Wright
January 13, 2025
No Comments

Engineers from RMIT University have invented a protective coating for concrete pipes that could help drastically reduce the formation of fatbergs in sewers.


Read More
Italian-Made Wood Finish Coatings Now Available in North America.jpg

Italian-Made Wood Finishing Coatings Now Available in North America

September 15, 2024
No Comments

“We are excited to bring these high-quality waterborne and polyurethane coatings to wood finishers in our region," says Cate Donovan, VP of Sales for ML Campbell.


Read More
High-Solids Polyurethane Dispersion for Low-VOC Wood Floor Coatings.jpg

High-Solids Polyurethane Dispersion for Low-VOC Wood Floor Coatings

August 10, 2024
No Comments

Designed for protection in clear wood finishes, the new product is  a TEA-free, low-VOC, 50% solids, self-crosslinking waterborne polyurethane dispersion that delivers high abrasion, chemical, and black heel mark resistance. 


Read More
AkzoNobel Launches New 2K High-Performance Polyurethane and Acrylic Wood Coatings System.jpg

New 2K High-Performance Polyurethane and Acrylic Wood Coatings Systems

July 17, 2024
No Comments

The new range provides a complete spectrum of sheens, from high gloss to dead flat, and draws inspiration from the rich heritage and craftsmanship of trusted, Italian-inspired formulations. 



Read More
GettyImages-1165170451-1170.jpg

Aliphatic Polyurea Coating Systems

Their Network Formation and Influencing Factors
Rolf Klucker Adrien Topalian
July 9, 2024
No Comments

Two-component aliphatic polyurea coating systems offer fast return to service and high film builds, and their use is on the rise. This article studies the network structure of these coatings to improve their properties.



Read More
2024 Polyurethane Innovation Award Submissions Now Open.jpg

2024 Polyurethane Innovation Award Submissions Now Open

March 27, 2024
No Comments

Innovators can compete for this award honoring new products or technologies brought to market. The award is presented by the American Chemistry Council’s (ACC) Center for the Polyurethanes Industry (CPI).


Read More
Market-Reports.jpg

New Global Polyurethane Coatings Market Report Projects Robust Growth

January 25, 2024
No Comments

In a report released by ResearchandMarkets, the PU coatings market was valued at $18.26 billion in 2022 and is anticipated to grow with a CAGR of 5.21% through 2028.


Read More
GettyImages-1478160399-1170.jpg

Polyurethane and Polyurea Coatings

A Primer on the Nomenclature, Technology, Properties, and In-Market Use
Steven Reinstadtler
January 10, 2024
8 Comments

This article examines the physical properties of polyurethanes and polyureas, their differences, and a technology review with benefits and drawbacks of sub-coating classes.



Read More
GettyImages-937689336-1170x878.jpg

Evaluation of PDO-Based Polyols in Cast Elastomer Protective Liners

Sean Gahan Ibrahim Sendijarevic Dr. Aisa Sendijarevic
October 2, 2023
No Comments

Cast elastomers based on PDO-sebacate polyol exhibit an excellent combination of tensile properties, abrasion resistance, thermal, hydrolytic, and solvent resistance, as well as adhesion to metal substrates. These are desirable properties for cast elastomers intended for applications as protective coatings for pipes, and coatings for sieves typically used in drilling and mining applications. 


Read More
Previous 1 2 3 Next
Manage My Account
  • Join Paint & Coatings Industry
  • Manage My Preferences
  • Customer Service

More Videos

Popular Stories

Mergers and aquisitions

Evonik Holds Off on BASF Takeover Talks

industry news

Dozens Treated After Toledo Chemical Release

Breaking News

H.B. Fuller to Close Seven Sites in Supply-Chain Overhaul

Events

November 19, 2026

Reformulating Paints with AI: Turn Change into a Competitive Advantage

Join industry leaders and experts for real case studies showing how AI helps R&D teams use existing paint formulation and test data to evaluate alternatives, predict trade-offs, and prioritize experiments.

December 10, 2026

PC Academy: Waterborne Polymers and Film Formation

The trend towards waterborne polymers in the paint and coatings industry is clear; highlighting their environmentally friendly nature, regulatory considerations, growing market demand, and meeting sustainability goals.

View All Submit An Event

Products

Powder Coatings - Foundation for the Novice Formulator (ebook)

Powder Coatings - Foundation for the Novice Formulator (ebook)

See More Products
PCI news now promo ad

Keep the info flowing with our eNewsletters!

Get the latest industry updates tailored your way.

JOIN TODAY!
  • RESOURCES
    • Advertise
    • Contact Us
    • Directories
    • Store
    • Manufacturing Division
  • JOIN TODAY
    • Create Account
    • eMagazine
    • Newsletters
    • Customer Service
    • Manage Preferences
  • SERVICES
    • Marketing Services
    • Reprints
    • Market Research
    • List Rental
    • Survey & Sample
  • STAY CONNECTED
    • LinkedIn
    • Facebook
    • Youtube
    • X (Twitter)
  • PRIVACY
    • PRIVACY POLICY
    • TERMS & CONDITIONS
    • DO NOT SELL MY PERSONAL INFORMATION
    • PRIVACY REQUEST
    • ACCESSIBILITY

Copyright ©2026. All Rights Reserved BNP Media, Inc. and BNP Media II, LLC.

Design, CMS, Hosting & Web Development :: ePublishing