Painting & Coating Industry (PCI) logo Powder coating summit logo
search
cart
facebook twitter linkedin youtube
  • Sign In
  • Create Account
  • Sign Out
  • My Account
Painting & Coating Industry (PCI) logo Powder coating summit logo
  • NEWS
    • Latest News
    • PCI News Now
    • Market Trends & Reports
    • Finishing News
    • Price Alerts
    • Global Top 10/ PCI 25
  • PRODUCTS
    • Product News
    • Featured Products
    • Must See Products and Services
  • MATERIALS
    • Additives
    • Resins/Polymers
    • Pigments
    • Equipment
    • Distributors
  • TECHNOLOGIES
    • Adhesives
    • Architectural Coatings
    • Finishing Articles
    • Finishing Technologies
    • Finishing Equipment
    • Industrial Coatings
    • Nanotechnology
    • Powder Coatings
    • Solventborne
    • Special Purpose Coatings
    • Sustainability
    • UV Coatings
    • Waterborne
  • EVENTS
    • Coatings Trends & Technologies Summit
    • Paint and Coatings Academy
    • Webinars
    • Calendar of Events
    • Lifetime Achievement Award
  • DIRECTORIES
    • Buyer's Guide
    • Equipment Directory
    • Materials Directory
  • RESOURCES
    • Columns
      • Did you know?
      • Distribution Dive
      • Formulating With Mike
      • Innovation Insights
      • Powder Coating Perspectives
      • TiO2 Insider
    • Blogs
      • Editor's Viewpoint
      • Industry Insights
    • Coatings Supplier Handbook
    • COAT-IT! Podcast
    • Videos
    • PCI Store
    • eBooks
    • Sponsor Insights
  • EMAGAZINE
    • eMagazine
    • Archive Issues
    • Editorial Advisory Board
    • CONTACT
    • Advertise
  • SIGN UP!
Home » Topics » Weekly Web Articles

Weekly Web Articles
Weekly Web Articles RSS Feed RSS

First-Ever Anti-Mosquito Paint Approved By the EPA

First-Ever Anti-Mosquito Paint Approved By the EPA

August 1, 2018
No Comments
This anti-mosquito paint is the only anti-mosquito paint that is approved by the EPA. It is currently approved in Uganda and Zambia and is expected to be available in the U.S. by summer of 2018.
Read More
Pink Stain Damage on Vinyl Surfaces

Pink Stain Damage on Vinyl Surfaces

Hugh Barrett
July 1, 2018
No Comments
Pink stain is a common problem on marine fabrics such as seating cushions, upholstery flooring and other vinyl surfaces. Once the stain happens, it cannot be cleaned. However, there are ways to prevent pink stain in the first place, through either preventing the growth of the bacteria that causes it or by sealing the substrate with a coating.
Read More
durr

Paint Shop for Electric Vehicles in China

July 1, 2018
No Comments

Dürr is currently building a fully automatic paint shop for a local OEM in Hefei in the Anhui Province of China. The plant is designed to handle 100,000 units per year, and will commence operation in June 2018. The integration of numerous digital@DÜRR solutions turns the paint shop into a Smart Factory with extensive use of data.


Read More
ocsial

Graphene Nanotubes Are on Duty Protecting Storage Tanks

July 1, 2018
No Comments
Manufacturers of storage tanks and antistatic lining coatings can gain a competitive edge by switching to graphene nanotube-based concentrates for their products. Uniform, permanent and stable resistivity ensures enhanced safety at their clients’ highly hazardous plants and reduces the cost of lining coatings.
Read More
sherwin williams

Transportation Center Presents Paragon of Sustainability

July 1, 2018
No Comments
Well known for its high-performance qualities and durability, including superior resistance to ultraviolet rays and exceptional dirt and stain resistance, Sherwin-Williams Coil Coating's Fluropon offers many valuable features.
Read More
pci0518-SinClair-671415012-900.jpg

Dissecting Orange Peel – A Process-Oriented Approach, Part II

Michael Bonner
June 1, 2018
No Comments

In this two-part series, we explore how this carefully crafted design of experiments (DOE) isolated and contrasted the impact and interaction of three key process variables: film build; atomization, and coating viscosity (as determined by temperature).


Read More
Science and Tech Solutions Meet the Flooring Crisis

Science and Tech Solutions Meet the Flooring Crisis

Vik Vithlani
June 1, 2018
No Comments

Environmental issues and shortages in supply chain raw materials are stretching the flooring industry worldwide. Here, Vik Vithlani, of Sherwin-Williams Protective & Marine Coatings EMEAI, examines how science and technology are finding the solutions.


Read More
New Application Success for Silicone-Epoxy Coatings Containing Bio-Repellent Ingredient

New Application Success for Silicone-Epoxy Coatings Containing Bio-Repellent Ingredient

Dan Isaksson Catherine Austin Oliver Weigenand John Smith
June 1, 2018
No Comments

The development of two-part epoxy resin coatings that harness antifouling properties is gaining importance as biofouling challenges increase across the global maritime fleet.


Read More
Largest Microwave-Powered and UV LED Wide-Format Curing Line Launches for R&D Testing Scaled to Production

Largest Microwave-Powered and UV LED Wide-Format Curing Line Launches for R&D Testing Scaled to Production

June 1, 2018
No Comments

ChemQuest Technology Institute (CQTI), in partnership with Heraeus Noblelight America, has begun scheduling trials on its newly installed, state-of-the-art, microwave-powered and UV LED wide-format curing systems


Read More
Metal Coatings Add Curve and Character to Fire Station

Metal Coatings Add Curve and Character to Fire Station

May 2, 2018
No Comments

Sherwin-Williams Coil Coatings and McElroy Metal team up to add curve and character to the Tyler Fire Station #5 in east Texas.


Read More
Previous 1 2 … 36 37 38 39 40 41 42 43 44 … 108 109 Next
Manage My Account
  • eMagazine
  • Newsletters
  • Online Registration
  • Subscription Customer Service

More Videos

Popular Stories

Sherwin-Williams

Sherwin-Williams Opens Largest North American Plant

AkzoNobel, Nippon

AkzoNobel to Sell Southeast Asia Decorative Paints Business to Nippon Paint for $1.35 Billion

Breaking News

Evonik Rejected €10.3 Billion BASF Offer, Reuters Reports

Events

November 5, 2026

Advancing Polyester Powder Coatings: Breakthroughs in Flexibility and Low-Cure Performance

Join us to learn how to improve coating durability while keeping your manufacturing process efficient. Explore the latest advancements in polyester powder coating technology.

November 12, 2026

Premium Leveling, Broad Compatibility: A Cost-Effective Flow and Leveling Additive

This new workhorse additive is recommended in all types of coatings. This highly compatible, 100% active siloxane product prevents defects and maintains good defoamer synergy.

View All Submit An Event
PCI news now promo ad

Keep the info flowing with our eNewsletters!

Get the latest industry updates tailored your way.

JOIN TODAY!
  • RESOURCES
    • Advertise
    • Contact Us
    • Directories
    • Store
    • Want More
    • Manufacturing Division
  • SIGN UP TODAY
    • Create Account
    • eMagazine
    • Newsletters
    • Customer Service
    • Manage Preferences
  • SERVICES
    • Marketing Services
    • Reprints
    • Market Research
    • List Rental
    • Survey & Sample
  • STAY CONNECTED
    • LinkedIn
    • Facebook
    • Youtube
    • X (Twitter)
  • PRIVACY
    • PRIVACY POLICY
    • TERMS & CONDITIONS
    • DO NOT SELL MY PERSONAL INFORMATION
    • PRIVACY REQUEST
    • ACCESSIBILITY

Copyright ©2026. All Rights Reserved BNP Media, Inc. and BNP Media II, LLC.

Design, CMS, Hosting & Web Development :: ePublishing