Painting & Coating Industry (PCI) logo Powder coating summit logo
search
cart
facebook twitter linkedin youtube
  • Sign In
  • Create Account
  • Sign Out
  • My Account
Painting & Coating Industry (PCI) logo Powder coating summit logo
  • NEWS
    • Latest News
    • Market Trends & Reports
    • Finishing News
    • Price Alerts
    • Global Top 10/ PCI 25
  • PRODUCTS
    • Product News
    • Featured Products
    • Must See Products and Services
  • MATERIALS
    • Additives
    • Resins/Polymers
    • Pigments
    • Equipment
    • Distributors
  • TECHNOLOGIES
    • Adhesives
    • Architectural Coatings
    • Finishing Articles
    • Finishing Technologies
    • Finishing Equipment
    • Industrial Coatings
    • Nanotechnology
    • Powder Coatings
    • Solventborne
    • Special Purpose Coatings
    • Sustainability
    • UV Coatings
    • Waterborne
  • EVENTS
    • Coatings Trends & Technologies Summit
    • Paint and Coatings Academy
    • Webinars
    • Calendar of Events
    • Lifetime Achievement Award
  • DIRECTORIES
    • Buyer's Guide
    • Equipment Directory
    • Materials Directory
  • RESOURCES
    • Columns
      • Did you know?
      • Distribution Dive
      • Formulating With Mike
      • Innovation Insights
      • Powder Coating Perspectives
      • TiO2 Insider
    • Blogs
      • Editor's Viewpoint
      • Industry Insights
    • Coatings Supplier Handbook
    • COAT-IT! Podcast
    • Videos
    • PCI Store
    • eBooks
    • Sponsor Insights
  • EMAGAZINE
    • eMagazine
    • Archive Issues
    • China Issue Archive
    • Editorial Advisory Board
    • CONTACT
    • Advertise
  • SIGN UP!
Home » Topics » Paint and Coatings Additives

Paint and Coatings Additives
Paint and Coatings Additives RSS Feed RSS

New Aspects in the Sustainability of Nanoparticle-Modified Coatings

Robert H. McMullin
June 1, 2011
No Comments
Predispersed nanoparticles can be very beneficial to the life cycle of coatings.
Read More

Application of Hollow Microspheres in Coatings

Sagar Gade
May 1, 2011
No Comments
Hollow micro spheres (especially glass microspheres) offer improved scrub and burnish properties, gloss, stain resistance, viscosity control, thermal insulation and sound-dampening characteristics.
Read More

A New Substrate Wetting Additive for Low-VOC Aqueous Adhesive Products

Peter Sheridan
April 1, 2011
No Comments
Troy Corp.’s multifunctional Troysol™ LAC provides excellent wetting of low-energy and contaminated surfaces, resulting in strong adhesive bonding.
Read More

A New Environmentally Friendly Wetting Agent for Architectural Coatings

Paul C. Marcella Jeanine M. Snyder
April 1, 2011
No Comments
The choice of wetting agents used in architectural coatings can have a significant impact when formulating low- to zero-VOC paints.
Read More

Ultrafine Nepheline Syenite as a Durable and Transparent Additive to Accelerate

Scott P. Van Remortel Robert E. Ratcliff
March 1, 2011
No Comments
Newer ultrafine nepheline syenite sizes have refractive index and physical properties that are particularly well suited for use as a performance additive in radiation-curable coatings, inks and adhesives.
Read More

Novel Acrylic Polymer Adhesion Technology for Coating Weathered TPO Roofing Membranes

Joe Rokowski
March 1, 2011
One Comment
RHOPLEX EC-3100 is an all-acrylic polymer designed primarily for use in pigmented elastomeric basecoats to provide adhesion to weathered TPO roofing membranes.
Read More

Cobalt-Free Catalyst Gives New Life to the Alkyd Coatings Market

Shelley Parkerson
March 1, 2011
No Comments
This article highlights a new cobalt-free catalyst that helps to achieve the necessary cure time as well as improve properties associated with water-based, high solids alkyds and alkyd-modified resins.
Read More

Novel Matting Agent for Low-Gloss UV Coatings

Maria Nargiello Andreas Feller Hans-Dieter Christian Reinhard Behl
March 1, 2011
No Comments
This article focuses on matting agents based on SiO2 from precipitated and gel processes, which are marketed specifically for the UV coatings segment.
Read More

Recent Advances in Photocuring and Stabilization of Waterborne Coatings

I.M. Spinu K.O. Sass E.V. Sitzmann K.P. Milks
February 1, 2011
No Comments
This article explores the use of NEAT additives for a UV-curable waterborne resin, which yields a photostable coating. 
Read More

Designing, Formulating and Measuring Coatings for Optimum Rheology

Dr. Daniel Saucy Vinnie Hebert
February 1, 2011
No Comments
The rheology of the coating plays a critical role in the actual process of applying the coating to the substrate. 
Read More
Previous 1 2 … 45 46 47 48 49 50 51 52 53 Next
Manage My Account
  • eMagazine
  • Newsletters
  • Online Registration
  • Subscription Customer Service

More Videos

Sponsored Content

Sponsored Content is a special paid section where industry companies provide high quality, objective, non-commercial content around topics of interest to the PCI audience. All Sponsored Content is supplied by the advertising company and any opinions expressed in this article are those of the author and not necessarily reflect the views of PCI or its parent company, BNP Media. Interested in participating in our Sponsored Content section? Contact your local rep!

close
  • wooden kitchen set and shelving
    Sponsored bySirca North America

    Leveraging Coatings to Meet ESG Goals in Manufacturing

Popular Stories

Breaking News

Yenkin-Majestic Pleads Guilty in Fatal Resin Plant Explosion Case

Plaque sign on the outside of the United States Environmental Protection Agency

EPA Draft Finds Worker Risks From trans-1,2-Dichloroethylene

Solstice Logo

Solstice, Element Solutions Terminate $14.5B Deal

Webinar custom content box

Events

January 1, 2030

Webinar Sponsorship Information

For webinar sponsorship information, visit www.bnpevents.com/webinars or email webinars@bnpmedia.com.

View All Submit An Event

Products

Advanced Coating Materials

Advanced Coating Materials

See More Products
Webinar custom content box

Keep the info flowing with our eNewsletters!

Get the latest industry updates tailored your way.

JOIN TODAY!
  • RESOURCES
    • Advertise
    • Contact Us
    • Directories
    • Store
    • Want More
    • Manufacturing Division
  • SIGN UP TODAY
    • Create Account
    • eMagazine
    • Newsletters
    • Customer Service
    • Manage Preferences
  • SERVICES
    • Marketing Services
    • Reprints
    • Market Research
    • List Rental
    • Survey & Sample
  • STAY CONNECTED
    • LinkedIn
    • Facebook
    • Youtube
    • X (Twitter)
  • PRIVACY
    • PRIVACY POLICY
    • TERMS & CONDITIONS
    • DO NOT SELL MY PERSONAL INFORMATION
    • PRIVACY REQUEST
    • ACCESSIBILITY

Copyright ©2026. All Rights Reserved BNP Media, Inc. and BNP Media II, LLC.

Design, CMS, Hosting & Web Development :: ePublishing