Painting & Coating Industry (PCI) logo Powder coating summit logo
search
cart
facebook twitter linkedin youtube
  • Sign In
  • Create Account
  • Sign Out
  • My Account
Painting & Coating Industry (PCI) logo Powder coating summit logo
  • NEWS
    • Latest News
    • PCI News Now
    • Market Trends & Reports
    • Finishing News
    • Price Alerts
    • Global Top 10/ PCI 25
  • PRODUCTS
    • Product News
    • Featured Products
    • Must See Products and Services
  • MATERIALS
    • Additives
    • Resins/Polymers
    • Pigments
    • Equipment
    • Distributors
  • TECHNOLOGIES
    • Adhesives
    • Architectural Coatings
    • Finishing Articles
    • Finishing Technologies
    • Finishing Equipment
    • Industrial Coatings
    • Nanotechnology
    • Powder Coatings
    • Solventborne
    • Special Purpose Coatings
    • Sustainability
    • UV Coatings
    • Waterborne
  • EVENTS
    • Coatings Trends & Technologies Summit
    • Paint and Coatings Academy
    • Webinars
    • Calendar of Events
    • Lifetime Achievement Award
  • DIRECTORIES
    • Buyer's Guide
    • Equipment Directory
    • Materials Directory
  • RESOURCES
    • Columns
      • Did you know?
      • Distribution Dive
      • Formulating With Mike
      • Innovation Insights
      • Powder Coating Perspectives
      • TiO2 Insider
    • Blogs
      • Editor's Viewpoint
      • Industry Insights
    • Coatings Supplier Handbook
    • COAT-IT! Podcast
    • Videos
    • PCI Store
    • eBooks
    • Sponsor Insights
  • EMAGAZINE
    • eMagazine
    • Archive Issues
    • Editorial Advisory Board
    • CONTACT
    • Advertise
  • SIGN UP!
Home » Topics » FT Archives

FT Archives
FT Archives RSS Feed RSS

A "Killer" Paint

Anne Trafton
March 1, 2007
No Comments
Researchers at the Massachusetts Institute of Technology (MIT) have developed an “antimicrobial paint” that can kill influenza viruses that land on surfaces coated with it, potentially offering a new weapon in the battle against a disease that kills nearly 40,000 Americans per year.
Read More

Safe and Effective Powder Stripping

Todd Cottrell
March 1, 2007
One Comment
Four basic stripping methods are typically used to remove cured powder coatings: mechanical, thermal, thermomechanical and chemical. Each method has advantages and disadvantages that must be considered in making a selection. Recently, a new chemical process has been developed that offers quick coating removal at ambient temperatures and is safe for workers and the environment.
Read More

Harnessing the Cleaning Power of Dry Ice

BNP Media Staff
March 1, 2007
No Comments
Dry ice blasting can safely remove coatings and contaminants from surfaces without the secondary waste treatment and disposal often required with pretreatment chemicals and other cleaning methods. As a result, it offers benefits such as cost reductions, extension of equipment's useful life, minimized substrate damage and improved environmental safety compared to other cleaning methods.
Read More

A Brilliant Finish

Inès A. Melamies
March 1, 2007
No Comments
A new atmospheric plasma technology has been developed to eliminate common problems and improve the quality of the finish, thereby driving down the number of rejects. The technology can produce ultrafine cleaning and high activation on a wide range of surfaces, including plastics, metal and glass; these benefits, in turn, can promote the optimum adhesion of paints and coatings.
Read More

FINISHING DEFENSE - MIL-DTL-53039 or MIL-DTL-64159: Which Topcoat is Right for You?

Jon Pollina
March 1, 2007
No Comments
In life and in business, it’s always nice to know that you have options. As a chemical agent resistant coating (CARC) applicator, you should already know that two exterior topcoats are available, both of which are fully supported by the Army: MIL-DTL-53039 and MIL-DTL-64159.
Read More

Faster E-Coating with Advanced Ultrafiltration

Mark Rizzone
March 1, 2007
No Comments
Ames True Temper needed to increase its ultrafiltration capacity significantly, but additional floor space was not available. Complicating matters was the need for all new UF equipment to quickly accommodate changes in paint color. The company asked three membrane companies to submit proposals for systems and provide price quotations.
Read More

OUTSIDE THE BOX - Pushing the Boundaries

Paul Fisher
March 1, 2007
No Comments
I recently had the pleasure of meeting some of the staff from Finishing Today at the predominantly plating-oriented National Association for Surface Finishing (NASF) Southeast Regional conference in Orlando. This magazine, which has a rich history rooted in the painting side of the metal finishing industry, was stretching its boundaries - an exercise we all could benefit from.
Read More

A Lean, Mean Powder Coating Machine

Ken Kreeger
March 1, 2007
No Comments
While inventories continue to shrink and lean operations rapidly replace yesterday’s traditional production methods, choosing powder coating can be a giant step toward greater efficiency, productivity and cost effectiveness in your operations. Yet to maximize your capital equipment investment, you should first wisely invest both time and thought into your current - and future - requirements before making the move.
Read More

FINISHING VIEWPOINT - Bad Trees and Coating Defects

Kevin Biller
March 1, 2007
No Comments
"Can a bad tree bear good fruit?" This concept has surfaced repeatedly throughout my career in the coatings field. A finisher facing trouble with corrosion resistance, blistering, peeling, impact resistance or color often would consider the coating as a probable cause of the defect. My mind would always take a couple steps back, recalling the words from my youth.
Read More

Ask Joe Powder

March 1, 2007
No Comments
Dear Joe,
We recently installed a powder line for automotive parts. Now we would like to install an in-line stripping process for our racks. Can you help us?
Read More
Previous 1 2 … 107 108 109 110 111 112 113 114 115 … 231 232 Next
Manage My Account
  • eMagazine
  • Newsletters
  • Online Registration
  • Subscription Customer Service

More Videos

Popular Stories

Sherwin-Williams

Sherwin-Williams Opens Largest North American Plant

AkzoNobel, Nippon

AkzoNobel to Sell Southeast Asia Decorative Paints Business to Nippon Paint for $1.35 Billion

Mergers-and-Company-Strategies.jpg

BASF Confirms Exploratory Talks on Potential Evonik Takeover

Events

November 5, 2026

Advancing Polyester Powder Coatings: Breakthroughs in Flexibility and Low-Cure Performance

Join us to learn how to improve coating durability while keeping your manufacturing process efficient. Explore the latest advancements in polyester powder coating technology.

November 12, 2026

Premium Leveling, Broad Compatibility: A Cost-Effective Flow and Leveling Additive

This new workhorse additive is recommended in all types of coatings. This highly compatible, 100% active siloxane product prevents defects and maintains good defoamer synergy.

View All Submit An Event
PCI news now promo ad

Keep the info flowing with our eNewsletters!

Get the latest industry updates tailored your way.

JOIN TODAY!
  • RESOURCES
    • Advertise
    • Contact Us
    • Directories
    • Store
    • Want More
    • Manufacturing Division
  • SIGN UP TODAY
    • Create Account
    • eMagazine
    • Newsletters
    • Customer Service
    • Manage Preferences
  • SERVICES
    • Marketing Services
    • Reprints
    • Market Research
    • List Rental
    • Survey & Sample
  • STAY CONNECTED
    • LinkedIn
    • Facebook
    • Youtube
    • X (Twitter)
  • PRIVACY
    • PRIVACY POLICY
    • TERMS & CONDITIONS
    • DO NOT SELL MY PERSONAL INFORMATION
    • PRIVACY REQUEST
    • ACCESSIBILITY

Copyright ©2026. All Rights Reserved BNP Media, Inc. and BNP Media II, LLC.

Design, CMS, Hosting & Web Development :: ePublishing