The Canadian Paint and Coatings Association (CPCA) held its 105th Annual Conference and Annual General Meeting (AGM) in Toronto on May 23-24, where eight new members were elected to the CPCA Board of Directors.
NACE International has formed the NACE Corrosion Consortia, a new service facilitating corrosion-mitigation research for companies, government bodies, research organizations, universities and other associations seeking to solve corrosion issues.
Materials scientists at Southwest Research Institute (SwRI) have developed a superhydrophobic coating and a process for applying it to the internal surfaces of long tubular structures.
The entry submission process is now open for the annual Sherwin-Williams Impact Award, which recognizes excellence on North American water and wastewater projects.
AkzoNobel has secured a two-year deal to continue supplying its Intersleek 1100SR foul-release coating to Qatari shipping and maritime giant Nakilat (Qatar Gas Transport Co. Ltd).