Painting & Coating Industry (PCI) logo Powder coating summit logo
search
cart
facebook twitter linkedin youtube
  • Sign In
  • Create Account
  • Sign Out
  • My Account
Painting & Coating Industry (PCI) logo Powder coating summit logo
  • NEWS
    • Latest News
    • Market Trends & Reports
    • Finishing News
    • Price Alerts
    • Global Top 10/ PCI 25
  • PRODUCTS
    • Product News
    • Featured Products
    • Must See Products and Services
  • MATERIALS
    • Additives
    • Resins/Polymers
    • Pigments
    • Equipment
    • Distributors
  • TECHNOLOGIES
    • Adhesives
    • Architectural Coatings
    • Finishing Articles
    • Finishing Technologies
    • Finishing Equipment
    • Industrial Coatings
    • Nanotechnology
    • Powder Coatings
    • Solventborne
    • Special Purpose Coatings
    • Sustainability
    • UV Coatings
    • Waterborne
  • EVENTS
    • Coatings Trends & Technologies Summit
    • Paint and Coatings Academy
    • Webinars
    • Calendar of Events
    • Lifetime Achievement Award
  • DIRECTORIES
    • Buyer's Guide
    • Equipment Directory
    • Materials Directory
  • RESOURCES
    • Columns
      • Did you know?
      • Distribution Dive
      • Formulating With Mike
      • Innovation Insights
      • Powder Coating Perspectives
      • TiO2 Insider
    • Blogs
      • Editor's Viewpoint
      • Industry Insights
    • Coatings Supplier Handbook
    • COAT-IT! Podcast
    • Videos
    • PCI Store
    • eBooks
    • Sponsor Insights
  • EMAGAZINE
    • eMagazine
    • Archive Issues
    • China Issue Archive
    • Editorial Advisory Board
    • CONTACT
    • Advertise
  • SIGN UP!
Company News

BASF Partners with Color Compass Corp. to Sponsor ARA Pedal

Graphic about the Pedal Car Challenge
March 21, 2022

SOUTHFIELD, MI — Students across British Columbia, Canada, who are interested in the automotive industry will have a unique opportunity to design and manufacture their own toy pedal cars, thanks to the Automotive Retailers Association (ARA) hosting the event sponsored by BASF and Color Compass Corp.

Over the next three months, the ARA’s Pedal Car Challenge will provide a pedal car kit to participating schools. Students will be able to apply their unique creative abilities while building and/or modifying the car using provided specifications. The project will also help students understand the teamwork, discipline and dedication needed to be successful in the automotive field.

“Working in the automotive industry is fun and rewarding, and this project gives students a great example of what to look forward to in their careers,” said Mark Huisman, Business Manager for BASF Refinish Canada. “This is an industry where the sky really is the limit. We are committed to demonstrating how artistic and technical abilities come together to create beautiful, innovative solutions for the future of automotive. It all starts with involving them with fun projects like the ARA Pedal Car Challenge.”

Each completed car will be auctioned off to raise funds for the Automotive Retailers Foundation, a program that provides scholarships to students pursuing a career in the automotive industry.

“We appreciate BASF’s forward thinking in supporting students and Industry. It is only with business partners like BASF that we are able to make this idea a reality,” said Adrian Scovell, President and CEO of ARA.

For more information about the project, visit https://www.events.ara.bc.ca/event/pedal-4-glory-school-challenge-toy-car-event-2022/.  

KEYWORDS: Automotive Coatings

Share This Story

Looking for a reprint of this article?
From high-res PDFs to custom plaques, order your copy today!

Recommended Content

JOIN TODAY
to unlock your recommendations.

Already have an account? Sign In

  • Double exposure of creative chemistry concept on laptop background, research and development concept

    Inside the AI Shift in Coatings

    Industry leaders share real-world examples of how AI is...
    Paint and Coating Resins & Polymers
    By: PCI Editorial Staff
  • Global Top 10 and PCI Logo

    2026 Global Top 10: Top Paint and Coatings Companies

    See how the world’s largest paint and coatings companies...
    Global Top 10 and PCI 25
    By: Courtney Bassett
  • The 2026 PCI 25

    2026 PCI 25: Top Paint and Coatings Companies

    See how North America's largest paint and coatings...
    Global Top 10 and PCI 25
    By: Courtney Bassett
You must login or register in order to post a comment.

Report Abusive Comment

Manage My Account
  • eMagazine
  • Newsletters
  • Online Registration
  • Subscription Customer Service

More Videos

Sponsored Content

Sponsored Content is a special paid section where industry companies provide high quality, objective, non-commercial content around topics of interest to the PCI audience. All Sponsored Content is supplied by the advertising company and any opinions expressed in this article are those of the author and not necessarily reflect the views of PCI or its parent company, BNP Media. Interested in participating in our Sponsored Content section? Contact your local rep!

close
  • wooden kitchen set and shelving
    Sponsored bySirca North America

    Leveraging Coatings to Meet ESG Goals in Manufacturing

Popular Stories

Breaking News

Yenkin-Majestic Pleads Guilty in Fatal Resin Plant Explosion Case

Plaque sign on the outside of the United States Environmental Protection Agency

EPA Draft Finds Worker Risks From trans-1,2-Dichloroethylene

Solstice Logo

Solstice, Element Solutions Terminate $14.5B Deal

Webinar custom content box

Events

January 1, 2030

Webinar Sponsorship Information

For webinar sponsorship information, visit www.bnpevents.com/webinars or email webinars@bnpmedia.com.

View All Submit An Event

Products

Advanced Coating Materials

Advanced Coating Materials

See More Products
Webinar custom content box

Related Articles

  • BASF Partners With Kia Motors

    See More
  • BASF Partners With Collision Hub on Waterborne Panel Broadcast

    See More
  • OEMs Join SME to Sponsor Conference

    See More

Related Directories

  • BASF Corp., Dispersions & Resins

    BASF offers the widest portfolio of raw materials for the coatings industry, including resins, latex, specialty additives, dispersants and stabilizers.
  • BASF Corp., Dispersions, Resins & Additives

    BASF offers a strong portfolio of industry-leading additives for the Coatings Industry to deliver eco-efficient solutions that meet performance requirements. The BASF Performance and Formulation additives portfolio encompasses a technology base of dispersing agents, wetting agents and surface modifiers, defoamers, rheology modifiers, film forming agents, antioxidants, light stabilizers and UV absorbers.
×

Keep the info flowing with our eNewsletters!

Get the latest industry updates tailored your way.

JOIN TODAY!
  • RESOURCES
    • Advertise
    • Contact Us
    • Directories
    • Store
    • Want More
    • Manufacturing Division
  • SIGN UP TODAY
    • Create Account
    • eMagazine
    • Newsletters
    • Customer Service
    • Manage Preferences
  • SERVICES
    • Marketing Services
    • Reprints
    • Market Research
    • List Rental
    • Survey & Sample
  • STAY CONNECTED
    • LinkedIn
    • Facebook
    • Youtube
    • X (Twitter)
  • PRIVACY
    • PRIVACY POLICY
    • TERMS & CONDITIONS
    • DO NOT SELL MY PERSONAL INFORMATION
    • PRIVACY REQUEST
    • ACCESSIBILITY

Copyright ©2026. All Rights Reserved BNP Media, Inc. and BNP Media II, LLC.

Design, CMS, Hosting & Web Development :: ePublishing