Avecia offers Solsperse® 38500, a new polymeric hyperdispersant that offers multicompatibility for solvent-based industrial tinters. It comes as a ready-to-use, 40% active material in a solution of methoxyl propyl acetate. The material is compatible with a range of resins, including nitrocellulose, alkyd, polyurethane and acrylic.