Painting & Coating Industry (PCI) logo Powder coating summit logo
search
cart
facebook twitter linkedin youtube
  • Sign In
  • Create Account
  • Sign Out
  • My Account
Painting & Coating Industry (PCI) logo Powder coating summit logo
  • NEWS
    • Latest News
    • PCI News Now
    • Market Trends & Reports
    • Finishing News
    • Price Alerts
    • Global Top 10/ PCI 25
  • PRODUCTS
    • Product News
    • Featured Products
    • Must See Products and Services
  • MATERIALS
    • Additives
    • Resins/Polymers
    • Pigments
    • Equipment
    • Distributors
  • TECHNOLOGIES
    • Adhesives
    • Architectural Coatings
    • Finishing Articles
    • Finishing Technologies
    • Finishing Equipment
    • Industrial Coatings
    • Nanotechnology
    • Powder Coatings
    • Solventborne
    • Special Purpose Coatings
    • Sustainability
    • UV Coatings
    • Waterborne
  • EVENTS
    • Coatings Trends & Technologies Summit
    • Paint and Coatings Academy
    • Webinars
    • Calendar of Events
    • Lifetime Achievement Award
  • DIRECTORIES
    • Buyer's Guide
    • Equipment Directory
    • Materials Directory
  • RESOURCES
    • Columns
      • Did you know?
      • Distribution Dive
      • Formulating With Mike
      • Innovation Insights
      • Powder Coating Perspectives
      • TiO2 Insider
    • Blogs
      • Editor's Viewpoint
      • Industry Insights
    • Coatings Supplier Handbook
    • COAT-IT! Podcast
    • Videos
    • PCI Store
    • eBooks
    • Sponsor Insights
  • EMAGAZINE
    • eMagazine
    • Archive Issues
    • Editorial Advisory Board
    • CONTACT
    • Advertise
  • SIGN UP!
Home » Topics » Paint and Coating Pigments

Paint and Coating Pigments
Paint and Coating Pigments RSS Feed RSS

Achieving the Full Potential of Low- and Zero-VOC Paints

Romesh Kumar Ph.D. Robert Rudzinski
March 1, 2013
No Comments
Combining improved dispensing systems and low-VOC-optimized colorant formulations can help meet stringent environmental regulations.
Read More

Potential for a New Generation of Solar-Reflective Coatings

New Coating Pigment Gives High Infrared Reflectance
Dr. Robert Portsmouth
March 1, 2013
No Comments
The ALTIRIS pigment has been engineered to reflect infrared radiation from the sun, yielding high solar reflectance in a range of colors.
Read More

CABOT CORP.

CABOT CORP.
January 4, 2013
No Comments
CABOT CORP. launched EMPEROR® 1600 and EMPEROR® 1200 premium carbon black pigments for coatings applications where exceptional color and superior processability are primary objectives.
Read More

LANXESS IPG

January 4, 2013
No Comments
LANXESS IPG introduced Bayferrox® 912LOM, a tailor-made, unique yellow iron oxide pigment.
Read More

Influence of Nanoclay on Elastic and Adhesion Properties in Polyurethane Coatings

G.Ramachandra Reddy C. Sugumar S. Venkatanaidu
January 4, 2013
No Comments
Current automotive coatings systems consist of several layers, such as an adhesion-promoting layer, primer, basecoat and clearcoat.
Read More

New Functionalized Particles

Solutions for Enhanced Performance, Efficiency and Sustainability
Milan W. Krumble
January 4, 2013
No Comments
Today’s coatings market expects more from its white pigments than brightness and opacity. White pigments, such as titanium dioxide (TiO2), barium sulfate (BaSO4) and zinc sulphide, are just examples of many ingredients possible in a complex coatings formulation.


Read More

Pushing the Edge of the Durable Color Envelope

New High-Performance Pigments for Lead Chromate Replacement in the Yellow and Orange Color Space
Mark M. Ryan Jr.
January 4, 2013
No Comments
The trade-off in the yellow and orange color space between the weatherability, heat stability and opacity of inorganic pigments versus the chromaticity, brightness and tint strength of organic colorants, in light of the decrease in use of pigments based on deprecated metals, has opened an opportunity for new colored pigment chemistries.


Read More

Performance Expectations for UV-Durable Coil Coatings

Scott Moffatt
December 3, 2012
No Comments
Although silicone-modified polyester (SMP) and super-polyester coatings are well-suited for specific applications, they cannot provide the same proven long-term performance as 70% polyvinylidene (PVDF) coatings due to the latter’s superior chemistry.


Read More

Sulphate pigments

December 3, 2012
No Comments
New functionalized pigments from the Sachtoperse family of barium sulphate pigments are optimally tailored to their respective binder and designed to provide secure bonding between pigment and resin.


Read More

Calcium Carbonate

December 3, 2012
No Comments
ImExtend™ 14CCL is a new ultrafine calcium carbonate developed for household-appliance powder coatings.


Read More
Previous 1 2 … 18 19 20 21 22 23 24 25 26 27 Next
Manage My Account
  • eMagazine
  • Newsletters
  • Online Registration
  • Subscription Customer Service

More Videos

Popular Stories

Sherwin-Williams

Sherwin-Williams Opens Largest North American Plant

Mergers-and-Company-Strategies.jpg

BASF Confirms Exploratory Talks on Potential Evonik Takeover

AkzoNobel, Nippon

AkzoNobel to Sell Southeast Asia Decorative Paints Business to Nippon Paint for $1.35 Billion

Events

November 5, 2026

Advancing Polyester Powder Coatings: Breakthroughs in Flexibility and Low-Cure Performance

Join us to learn how to improve coating durability while keeping your manufacturing process efficient. Explore the latest advancements in polyester powder coating technology.

January 1, 2030

Webinar Sponsorship Information

For webinar sponsorship information, visit www.bnpevents.com/webinars or email webinars@bnpmedia.com.

View All Submit An Event
PCI news now promo ad

Keep the info flowing with our eNewsletters!

Get the latest industry updates tailored your way.

JOIN TODAY!
  • RESOURCES
    • Advertise
    • Contact Us
    • Directories
    • Store
    • Want More
    • Manufacturing Division
  • SIGN UP TODAY
    • Create Account
    • eMagazine
    • Newsletters
    • Customer Service
    • Manage Preferences
  • SERVICES
    • Marketing Services
    • Reprints
    • Market Research
    • List Rental
    • Survey & Sample
  • STAY CONNECTED
    • LinkedIn
    • Facebook
    • Youtube
    • X (Twitter)
  • PRIVACY
    • PRIVACY POLICY
    • TERMS & CONDITIONS
    • DO NOT SELL MY PERSONAL INFORMATION
    • PRIVACY REQUEST
    • ACCESSIBILITY

Copyright ©2026. All Rights Reserved BNP Media, Inc. and BNP Media II, LLC.

Design, CMS, Hosting & Web Development :: ePublishing