Painting & Coating Industry (PCI) logo Powder coating summit logo
search
cart
facebook twitter linkedin youtube
  • Sign In
  • Create Account
  • Sign Out
  • My Account
Painting & Coating Industry (PCI) logo Powder coating summit logo
  • NEWS
    • Latest News
    • Market Trends & Reports
    • Finishing News
    • Price Alerts
    • Global Top 10/ PCI 25
  • PRODUCTS
    • Product News
    • Featured Products
    • Must See Products and Services
  • MATERIALS
    • Additives
    • Resins/Polymers
    • Pigments
    • Equipment
    • Distributors
  • TECHNOLOGIES
    • Adhesives
    • Architectural Coatings
    • Finishing Articles
    • Finishing Technologies
    • Finishing Equipment
    • Industrial Coatings
    • Nanotechnology
    • Powder Coatings
    • Solventborne
    • Special Purpose Coatings
    • Sustainability
    • UV Coatings
    • Waterborne
  • EVENTS
    • Coatings Trends & Technologies Summit
    • Paint and Coatings Academy
    • Webinars
    • Calendar of Events
    • Lifetime Achievement Award
  • DIRECTORIES
    • Buyer's Guide
    • Equipment Directory
    • Materials Directory
  • RESOURCES
    • Columns
      • Did you know?
      • Distribution Dive
      • Formulating With Mike
      • Innovation Insights
      • Powder Coating Perspectives
      • TiO2 Insider
    • Blogs
      • Editor's Viewpoint
      • Industry Insights
    • Coatings Supplier Handbook
    • COAT-IT! Podcast
    • Videos
    • PCI Store
    • eBooks
    • Sponsor Insights
  • EMAGAZINE
    • eMagazine
    • Archive Issues
    • China Issue Archive
    • Editorial Advisory Board
    • CONTACT
    • Advertise
  • SIGN UP!
Home » Topics » Special Purpose Coatings

Special Purpose Coatings
Special Purpose Coatings RSS Feed RSS

In an Ideal World, Every Coating is Green

In an Ideal World, Every Coating is Green

Jeff Alexander
September 1, 2016
No Comments

It is imperative for coatings manufacturers to set an example for the entire industry and produce more sustainable products and technologies that address the many problems facing our earth.


Read More
Copper in Antifoulings: Going from Strength to Strength

Copper in Antifoulings: Going from Strength to Strength

August 1, 2016
No Comments

It is fortuitous for ship owners that compliance with the two pieces of IMO legislation can both be achieved by use of an effective copper-based antifouling coating on the underwater hull, along with careful in water cleaning when necessary, based on vessel type, usage and coating schedule.


Read More
pci top 10 and 25

2016 Global Top 10 and PCI 25: Top Paint and Coatings Companies

Karen Parker
July 5, 2016
2 Comments

The Global Top 10 and PCI 25 is a ranking of the top global and North American coatings manufacturers. Rankings are based on 2015 coatings sales. Sales of other, non-coating products are not included.


Read More
Aston Martin Racing (AMR)

Aston Martin Racing Unveils Iconic Green Livery

June 2, 2016
No Comments

Working closely with clients such as Aston Martin Racing, HMG’s Advanced Color Design team offers customers the chance to match or design their own shades, using sparkled, fluorescent or metallic pigment technology to create their own unique colours.


Read More
Reducing the Environmental Footprint of Coatings with Lactide Technology

Reducing the Environmental Footprint of Coatings with Lactide Technology

Armin Michel
May 1, 2016
No Comments

Lactide-based alkyd resins can help coatings formulators to meet new targets for lower VOC content and produce coatings with a reduced carbon footprint.


Read More
klm

Living the Dream with KLM

April 5, 2016
No Comments

The base coat/clearcoat system is typically lighter than conventional systems, while its smoother surface means there is less dirt adhesion. Additional benefits include UV protection for colors, extending the time required between repainting and reduced drying times.


Read More
Upcycling from Water Bottles to Protective Coatings

Upcycling from Water Bottles to Protective Coatings

A New Approach and a New Life – Part II
April 4, 2016
No Comments

This work has validated a place for some novel new polyols with high recycle content combined with high performance for specialty coating applications, where protection of metal surfaces is paramount.


Read More
Minimal Eco Impact. Maximal Color Effect.

Minimal Eco Impact. Maximal Color Effect.

Stephan Spiegelhauer
April 1, 2016
No Comments

In addition to highly sustainable production, the Ningbo process provides iron oxide red pigments with exceptional coloristic behavior that exceeds any currently available iron oxide pigment in the market.


Read More
Solving Film Defects with Surface Tension Modifiers

Solving Film Defects with Surface Tension Modifiers

Taking the Mystery Out of “Pixie Dust”
Dietmar Oberste Richard Najdusak
April 1, 2016
One Comment

Focusing on using the right type of additive to address a specific film defect will reduce the number of materials to test and not rely on trying many different chemicals in the hope of finding just the right pixie dust.


Read More
Maintaining Critical Road, Rail and Bridge Infrastructure

Maintaining Critical Road, Rail and Bridge Infrastructure

Del Williams
March 1, 2016
No Comments

This new category of spray-applied waterproofing coatings are seamless, rugged, fast curing, impervious to water, able to bridge cracks, and capable of lasting decades without extensive maintenance.


Read More
Previous 1 2 … 31 32 33 34 35 36 37 38 39 40 41 42 Next
Manage My Account
  • eMagazine
  • Newsletters
  • Online Registration
  • Subscription Customer Service

More Videos

Sponsored Content

Sponsored Content is a special paid section where industry companies provide high quality, objective, non-commercial content around topics of interest to the PCI audience. All Sponsored Content is supplied by the advertising company and any opinions expressed in this article are those of the author and not necessarily reflect the views of PCI or its parent company, BNP Media. Interested in participating in our Sponsored Content section? Contact your local rep!

close
  • wooden kitchen set and shelving
    Sponsored bySirca North America

    Leveraging Coatings to Meet ESG Goals in Manufacturing

Popular Stories

Breaking News

Yenkin-Majestic Pleads Guilty in Fatal Resin Plant Explosion Case

Evonik Logo

Evonik to Close Two German Sites

Plaque sign on the outside of the United States Environmental Protection Agency

EPA Draft Finds Worker Risks From trans-1,2-Dichloroethylene

Webinar custom content box

Events

September 29, 2026

Innovations in Production Dispersing and Milling

Discover how the latest advancements in high-efficiency dissolvers, basket mills, and bead mills can help you overcome real-world production challenges such as throughput bottlenecks, energy consumption, and maintenance downtime.

October 8, 2026

AI-Powered Reformulation: Finding PFAS-Free, Lower-VOC Formulations Faster

In this webinar, we will use case studies from industry to illustrate how AI can be used to identify PFAS-free formulations and select surfactant blends for water-based products.

View All Submit An Event

Products

Advanced Coating Materials

Advanced Coating Materials

See More Products
Webinar custom content box

Keep the info flowing with our eNewsletters!

Get the latest industry updates tailored your way.

JOIN TODAY!
  • RESOURCES
    • Advertise
    • Contact Us
    • Directories
    • Store
    • Want More
    • Manufacturing Division
  • SIGN UP TODAY
    • Create Account
    • eMagazine
    • Newsletters
    • Customer Service
    • Manage Preferences
  • SERVICES
    • Marketing Services
    • Reprints
    • Market Research
    • List Rental
    • Survey & Sample
  • STAY CONNECTED
    • LinkedIn
    • Facebook
    • Youtube
    • X (Twitter)
  • PRIVACY
    • PRIVACY POLICY
    • TERMS & CONDITIONS
    • DO NOT SELL MY PERSONAL INFORMATION
    • PRIVACY REQUEST
    • ACCESSIBILITY

Copyright ©2026. All Rights Reserved BNP Media, Inc. and BNP Media II, LLC.

Design, CMS, Hosting & Web Development :: ePublishing