Painting & Coating Industry (PCI) logo Powder coating summit logo
search
cart
facebook twitter linkedin youtube
  • Sign In
  • Join Today
  • Sign Out
  • My Account
Painting & Coating Industry (PCI) logo Powder coating summit logo
  • NEWS
    • Latest News
    • PCI News Now
    • Market Trends & Reports
    • Finishing News
    • Price Alerts
    • Global Top 10/ PCI 25
  • PRODUCTS
    • Product News
    • Featured Products
    • Must See Products and Services
  • MATERIALS
    • Additives
    • Resins/Polymers
    • Pigments
    • Equipment
    • Distributors
  • TECHNOLOGIES
    • Adhesives
    • Architectural Coatings
    • Finishing Articles
    • Finishing Technologies
    • Finishing Equipment
    • Industrial Coatings
    • Nanotechnology
    • Powder Coatings
    • Solventborne
    • Special Purpose Coatings
    • Sustainability
    • UV Coatings
    • Waterborne
  • EVENTS
    • Coatings Trends & Technologies Summit
    • Paint and Coatings Academy
    • Webinars
    • Calendar of Events
    • Lifetime Achievement Award
  • DIRECTORIES
    • Buyer's Guide
    • Equipment Directory
    • Materials Directory
  • RESOURCES
    • Columns
      • Did you know?
      • Distribution Dive
      • Formulating With Mike
      • Innovation Insights
      • Powder Coating Perspectives
      • TiO2 Insider
    • Blogs
      • Editor's Viewpoint
      • Industry Insights
    • Coatings Supplier Handbook
    • COAT-IT! Podcast
    • Videos
    • PCI Store
    • eBooks
    • Sponsor Insights
  • EMAGAZINE
    • eMagazine
    • Archive Issues
    • Editorial Advisory Board
    • CONTACT
    • Advertise
  • JOIN!
Home » Publications » PCI eMagazine

PCI eMagazine

pce feb 2020

2020 February

The February issue focuses on waterborne and UV/EB technology, with additional information on a greener solution to deter marine biofouling.
  • Feature Articles
  • News
  • Products

Feature Articles

Back to Top
PPG Protects World’s Largest Airport Terminal with Fire-Resistant, Sustainably Advantaged Coatings

PPG Protects World’s Largest Airport Terminal with Fire-Resistant, Sustainably Advantaged Coatings

February 10, 2020
No Comments
PPG announced that its interior and exterior coatings are enhancing protection, safety and sustainability for the new Beijing Daxing International Airport terminal building.
Read More
pci0220-Adaptive-175539860-900.jpg

A Greener Solution to Deter Marine Biofouling

Philseok Kim Teluka Galhenage
February 11, 2020
One Comment
SLIPS Foul Protect N1x has successfully demonstrated the pathway to reducing marine fouling with a non-toxic, environmentally friendly approach combining the smooth and slippery liquid-based surface (Physical module) and highly branched amphiphilic SAPs (Chemical module).
Read More

Powder Coatings Demand Continues to Rise in O&G and Automotive Sectors

Shreshtha Dhatrak
February 7, 2020
One Comment
Powder coatings market share has experienced a veritable expansion over the years owing to the benefits associated with the products, including durability, superior quality and enhanced efficiencies on virtually any type of material. Powder coatings market share has experienced a veritable expansion over the years owing to the benefits associated with the products, including durability, superior quality and enhanced efficiencies on virtually any type of material.
Read More
Diamond-Like Carbon Coatings Meet the Challenges of Demanding Applications

Diamond-Like Carbon Coatings Meet the Challenges of Demanding Applications

February 6, 2020
No Comments
Within the universe of wear-resistant thin films, diamond-like carbon (DLC) coatings have emerged as the ideal solution for demanding physical applications where components are under high loads or subject to extreme friction, wear and contact with other parts.
Read More
pci0220-Allnex-468495842-900.jpg

UV Coatings on Plastics

Bringing Value to the Market
Paul Gevaert
February 5, 2020
One Comment

Recent energy-curable resin developments respond to the increasing demand for suitable oligomers for coatings on plastics in different segments such as consumer electronics, cosmetic packaging and automotive interiors for different specifications and aesthetic requirements.


Read More
did you know column

Creating Core-Shell Latex Particles is Sometimes More a Dream than Reality

Emulsion Polymers Consulting and Education (EPCEd)
February 3, 2020
No Comments
We have been working on morphology control in latex particles for many years and have come to learn that achieving desired structures in composite particles is dependent not only upon the emulsion polymerization recipe, but also strongly upon the reaction process conditions.
Read More
pci0220-BYK--1163891251-900.jpg

Novel Silicone Surfactants for Waterborne Wood Coatings

Excellent Performance at Highest Application Speeds
Michael Toth Marcus Wessel Marcel Krohnen
February 4, 2020
3 Comments
Due to their tailored system compatibility, the new sili¬cone surfactants are suitable for use in both aqueous one-component systems as well as in aqueous two-com¬ponent polyurethane and radiation-curable systems.
Read More
pci0220-Alberdingk-1009381622-900.jpg

Waterborne UV-Curable Resins for Industrial Wood Applications

Laurie Morris
February 3, 2020
No Comments

In this study, polyurethane-acrylic resins with UV functionality have been evaluated according to industry specifications for both interior and exterior industrial wood applications.


Read More

News

Back to Top

Innovative Chemical Products Group Acquires Hi-Tech Coatings

December 6, 2019
No Comments
Innovative Chemical Products Group announced that it has acquired Hi-Tech Coatings, a developer and manufacturer of high-performance coatings for the packaging and commercial printing industries, from Heidelberger Druckmaschinen AG.
Read More
coatings manufacturers, acquisitions, Africa

AkzoNobel Strengthens Position in Sub-Saharan African Paint Market

December 13, 2019
No Comments
AkzoNobel has entered into an agreement to acquire 100% of the shares of Mauvilac Industries Limited, a leading paint and coatings company in Mauritius.
Read More

EU Project Focuses on Renewable Alternatives to Solvents

January 3, 2020
No Comments
Biotechnology company Circa Group announced it is leading the consortium for a new EU project, ReSolute, a flagship Horizon 2020 project set to develop the first commercial plant to produce a sustainably sourced, safer alternative to traditional fossil-based solvents.
Read More

Clariant Agrees to Sell Masterbatches Business

December 20, 2019
No Comments
Specialty chemical company Clariant has agreed to sell its entire Masterbatches business to PolyOne.
Read More
sustainable business practices

SONGWON Strengthens Sustainability Efforts

January 13, 2020
No Comments
SONGWON Industrial Co. Ltd. reported some of its successful in-house sustainability efforts relating to both energy conservation and efficiency and emphasized its commitment to the environment across the organization.
Read More
printing inks

Siegwerk Opens Fully Automated Printing Inks Production Facility

January 5, 2020
No Comments
Siegwerk, a leading provider of printing inks for packaging applications and labels, has opened a new fully automated facility for the production of inks at its headquarters in Siegburg, Germany.
Read More
methacrylate monomers

Röhm Introduces New Brand for Methacrylate Monomers

January 13, 2020
No Comments
Röhm GmbH announced that the company will be selling its methacrylate monomers under a new brand name.
Read More

LANXESS Buys Brazilian Biocide Manufacturer

December 6, 2019
No Comments
Specialty chemicals company LANXESS is strengthening its position as a leading manufacturer of active biocidal ingredients and formulations with the acquisition of Itibanyl Produtos Especiais Ltda.
Read More

SurfactGreen Meets 2019 Goals, Books First Order

January 3, 2020
No Comments
SurfactGreen, a specialist in the production of bio-sourced surfactants, has completed its first industrial-scale production and booked its first order.
Read More

Northspec Chemicals Corp. to Distribute Stahl Polymers Portfolio

December 29, 2019
No Comments
Northspec Chemicals Corp. is now distributing the Stahl Polymers portfolio in Canada.
Read More
sustainable business practices

Vencorex Receives EcoVadis Gold Medal for Corporate Social Responsibility

January 3, 2020
No Comments
Vencorex has obtained the CSR Gold Rating from EcoVadis for the fourth year in a row.
Read More
capacity expansions, resins for coatings

IGM Resins Breaks Ground on Production Facility in China

December 6, 2019
No Comments
The official groundbreaking ceremony for IGM's new greenfield site in Anqing, Anhui Province in China took place on Oct 23.
Read More
pilot plants, expansions

MFG Chemical Upgrades Pilot Plant in Georgia

December 13, 2019
No Comments
MFG Chemical, a global leader in specialty and custom chemical manufacturing, has completed an upgrade of its pilot plant in Dalton, Georgia.
Read More
sustainable chemicals

New Anellotech Technology Tackles Plastics Pollution

January 5, 2020
No Comments
Sustainable technology company Anellotech is expanding its program with Plas-TCat™, a new process technology, aiming to convert a wide range of plastic waste directly into chemicals.
Read More
sustainable business practices

Sun Chemical Releases 2018 Sustainability Report

December 13, 2019
No Comments
Sun Chemical has released its 2018 Corporate Sustainability Report, which focuses on how its commitment to sustainability has led to new products and services that help customers improve their eco-efficiency goals.
Read More

RadTech 2020 Technical Conference to Highlight the Latest in UV and EB Technology

December 29, 2019
No Comments

With UV and EB technology poised for continued rapid growth, the RadTech 2020 Conference Committee has assembled an extraordinary technical conference. The conference offers a complete set of informative sessions important to technical and business opportunities, including interactive panels featuring industry experts addressing needs and trends on 3D printing/additive manufacturing, UV LEDs, end user sustainability, photoinitiators, lightweighting, inkjet, printing and packaging.


Read More

NACD Welcomes Passage of USMCA Trade Deal

December 29, 2019
No Comments
The National Association of Chemical Distributors (NACD) has weighed in on the passage of the United States-Mexico-Canada Agreement (USMCA) that replaces the North American Free Trade Agreement.
Read More
powder coatings

Russian Building With Interpon Eco Coatings Receives Architzer A+ Award

November 7, 2019
No Comments
A futuristic "pyramid" in Moscow that uses low solar absorption powder coatings supplied by AkzoNobel has won a major architecture award.
Read More
British coatings industry

BCF Weighs in on UK Election Results

December 29, 2019
No Comments
Following the result of the UK's General Election, the British Coatings Federation (BCF) has expressed relief over the apparent political stability from Boris Johnson’s 80-seat majority.
Read More

Products

Back to Top

Liquid Resins from Sartomer

February 3, 2020
No Comments
N3xtDimension engineered liquid resins for UV-curable 3D printing help advance performance characteristics like impact resistance, flexibility, high-resolution prototyping and castability.
Read More

Foam-Control Agents from Ashland

February 3, 2020
No Comments
Formulated with novel hydrophobic polymers, Drewplus L-3500 and L-3510 foam-control agents help control macro- and micro-foam
Read More

Anti-Fingerprint Coating from Metashield

February 3, 2020
No Comments
Nanotechnology-based NANOPRINT provides added flexibility and durability with a simple, one-coat spray.
Read More

Double Planetary Mixer from Charles Ross & Son Co.

February 3, 2020
No Comments
This sanitary 4-gallon Double Planetary Mixer and Discharge System Model DPM/DS-4S features both interior and exterior type-316 stainless steel surfaces with a 150-grit (#4) finish and electro-polish.
Read More

Pressure Transmitter from Krohne

February 3, 2020
No Comments
OPTIBAR PM 3050 is a pressure transmitter for general pressure and level applications.
Read More

Dispensing Systems from Sulzer Mixpac USA Inc.

February 3, 2020
No Comments
MIXPAC MixCoat Flex and MixCoat Spray cartridge-based two-component dispensing systems are ideal for touch-up and repair work
Read More

Perfluoropolymer Coating from AGC Chemicals Americas

February 3, 2020
No Comments
Fluon+ PFA EA-2000 is a printed circuit board coating for copper clad laminate that improves inter-car communication across 5G networks.
Read More

Nonionic Dispersing Monomers from Perstorp

February 3, 2020
No Comments
Ymer N90, with a longer EO chain, and N180, with a shorter EO chain, allow customers to formulate solvent-free PUDs and minimize the level of harmful amines in production and during application.
Read More

Direct to Metal Polymer from Engineered Polymer Solutions

February 3, 2020
No Comments
A waterborne acrylic, EPS 2580 provides the capability to formulate direct-to-metal coatings at <50g/L VOC.
Read More
Manage My Account
  • Join Paint & Coatings Industry
  • Manage My Preferences
  • Customer Service

More Videos

Popular Stories

industry news

Dozens Treated After Toledo Chemical Release

Mergers and aquisitions

Evonik Holds Off on BASF Takeover Talks

AkzoNobel Axalta

EU Clears $25B Akzo-Axalta Merger with One Big Condition

Events

November 11, 2026

ChinaCoat

CHINACOAT2026 returns to Guangzhou this year. Welcome to exhibit, visit and join the annual industry gathering!

November 12, 2026

Premium Leveling, Broad Compatibility: A Cost-Effective Flow and Leveling Additive

This new workhorse additive is recommended in all types of coatings. This highly compatible, 100% active siloxane product prevents defects and maintains good defoamer synergy.

View All Submit An Event

Products

Powder Coatings - Foundation for the Novice Formulator (ebook)

Powder Coatings - Foundation for the Novice Formulator (ebook)

See More Products
PCI news now promo ad

Keep the info flowing with our eNewsletters!

Get the latest industry updates tailored your way.

JOIN TODAY!
  • RESOURCES
    • Advertise
    • Contact Us
    • Directories
    • Store
    • Manufacturing Division
  • JOIN TODAY
    • Create Account
    • eMagazine
    • Newsletters
    • Customer Service
    • Manage Preferences
  • SERVICES
    • Marketing Services
    • Reprints
    • Market Research
    • List Rental
    • Survey & Sample
  • STAY CONNECTED
    • LinkedIn
    • Facebook
    • Youtube
    • X (Twitter)
  • PRIVACY
    • PRIVACY POLICY
    • TERMS & CONDITIONS
    • DO NOT SELL MY PERSONAL INFORMATION
    • PRIVACY REQUEST
    • ACCESSIBILITY

Copyright ©2026. All Rights Reserved BNP Media, Inc. and BNP Media II, LLC.

Design, CMS, Hosting & Web Development :: ePublishing