Painting & Coating Industry (PCI) logo Powder coating summit logo
search
cart
facebook twitter linkedin youtube
  • Sign In
  • Create Account
  • Sign Out
  • My Account
Painting & Coating Industry (PCI) logo Powder coating summit logo
  • NEWS
    • Latest News
    • Market Trends & Reports
    • Finishing News
    • Price Alerts
    • Subscribe to Newsletters
    • Global Top 10/ PCI 25
    • Weekly Featured Article
  • PRODUCTS
    • Product News
    • Featured Products
    • Must See Products and Services
  • MATERIALS
    • Additives
    • Resins/Polymers
    • Pigments
    • Equipment
    • Distributors
  • TECHNOLOGIES
    • Adhesives
    • Architectural Coatings
    • Finishing Articles
    • Finishing Technologies
    • Finishing Equipment
    • Industrial Coatings
    • Nanotechnology
    • Powder Coatings
    • Solventborne
    • Special Purpose Coatings
    • Sustainability
    • UV Coatings
    • Waterborne
  • RESOURCES
    • Columns
      • Did you know?
      • Distribution Dive
      • Formulating With Mike
      • Innovation Insights
      • Powder Coating Perspectives
      • TiO2 Insider
    • Blogs
      • Editor's Viewpoint
      • Industry Insights
    • Coatings Supplier Handbook
    • Podcasts and Videos
      • COAT-IT! Podcast
      • Videos/PCI TV
    • PCI Store
    • Classifieds
    • eBooks
    • Sponsor Insights
    • White Papers
    • COATLE Word Game
  • EVENTS
    • Coatings Trends & Technologies Summit
    • Paint and Coatings Academy
    • Webinars
    • Calendar of Events
    • Lifetime Achievement Award
  • DIRECTORIES
    • Buyer's Guide
    • Equipment Directory
    • Materials Directory
  • EMAGAZINE
    • Current Issue
    • eMagazine Archive
    • China Issue Archive
    • Editorial Advisory Board
  • CONTACT
    • Contact Us
    • Advertise
    • Subscribe to eMagazine
    • Subscribe to Newsletters
  • SIGN UP!
Paint and Coating EquipmentTesting, Monitoring &Tools

Flexible, Non-Contact Film Thickness Measurement

By Martin Rola
pci0719-Sapience-1133235360-900.jpg
August 9, 2019

A new measurement and control technology designed to quickly and accurately measure uncured powder thickness has enabled quality and process engineers in Europe over the past several years to rapidly optimize their powder coating applications. The system has allowed them to minimize the need for the safety margins commonly applied to the powder quantity settings, resulting in large reductions in material consumption. In addition, the continuous measurement of coating thickness immediately after it is applied provides another layer of protection to detect quality problems before the parts are cured. Called Advanced Thermal Optics (ATO), the sensing means behind the system enables for highly accurate film thickness to be measured with a non-contact means on cured or uncured organic powder and powder enamel in a way that is extremely adaptable to the production environment. The data captured by the ATO system is processed with state-of-the-art signal processing to quickly generate very precise film thickness measurement data.

This patented technology was developed by Winterthur Instruments AG (Winterthur, Switzerland), and their flagship product, the Coatmaster, is now being used in a variety of industrial coating thickness measurement applications with over 220 units installed (Figure 1). The nature of the technology allows it to measure almost any type of coating on virtually any substrate, so in addition to powder materials, its application base includes liquid paints, adhesives, lubricants and thermal spray coatings. However, since powder materials are highly sensitive to the heating and cooling effects that are core to the system, the Coatmaster is extremely powerful when used to measure uncured powder film thickness. For example, the latest version of the system can produce a film thickness “heat map” of the uncured powder coating thickness for a 32-inch by 70-inch area only 15 seconds after the powder is applied.

Coatmaster installation
FIGURE 1 » Coatmaster installation.

The ATO technology behind the Coatmaster works in the following way. A light pulse is emitted that very slightly warms the surface. Then, high-speed infrared sensors detect the rate at which the material cools. Using proprietary algorithms, the Coatmaster is able to translate this rate of cooling to a highly accurate film thickness measurement. The time to take a reading varies by application, but is typically 100-300 ms, and individual point readings can occur as quickly as once every 1.5 seconds. Depending on the application, the standard deviation is typically between 0.1% and 2% of the actual film thickness. The Coatmaster’s LED positioning system offers a single-point marking with a diameter between 1 and 50 mm. In this way, the measuring point can be precisely positioned even on the smallest objects, curves or complex shaped parts. From this, the Coatmaster calculates the average value of the measured range and displays it as a measurement result. Since the measurement is based on this heating-cooling effect, which is detectable in almost all coatings, it is for the most part material and substrate independent, which means that the system can measure a wide range of coating-substrate combinations. Organic powder over metal or MDF and powder enamel over metal are common applications, and it is possible to measure thicknesses of 1,000 microns or higher.

One of the unique aspects of the ATO technology used in the Coatmaster compared to approaches of other systems used for non-contact film thickness measurement is the implementation flexibility it allows in a manufacturing environment. The system is very forgiving in terms of its location with respect to the part and the speed of the part being measured. It can read from distances as close as 2 inches or as far as 48 inches, and has a measurement area that ranges from 1 to 50 mm. It can read parts moving on a conveyor up to 350 ft/min and can read off angle as much as 70 degrees. This flexibility allows it to measure parts that rotate or shift when moving on the conveyor with minimal loss of accuracy. The Coatmaster can also measure coatings on components with highly complex shapes including threaded rods, corners and angles on narrow edges, and internal and curved surfaces.

The data-capturing capability of the system is impressive, but this is only of value if this data can be used effectively. To this point, the system comes with built-in quality control software that will track the measurements and identify trends, providing warnings or alarms when readings are out of a tolerance range. The system can be used only with the industrial PC interface, or can be integrated with a PLC. The open-architecture nature of the product allows it to be easily integrated into either plant monitoring systems or directly into the application equipment to enable closed-loop control of the coating process. Manufacturers of automotive components, architectural components and other products have all used this closed-loop approach to substantially reduce their film thickness variation. This not only reduces defects, but also allows for substantial reduction in material consumption by enabling a target set point.

This ability to reduce variation in thickness is especially beneficial in powder. Since powder application tends to drift over time due to batch-to-batch material variation, environmental changes or powder gun wear, having the ability to detect this and adjust in real time allows the system to be dialed in much more precisely. Since powder materials tend to be fairly forgiving in terms of film thickness, many applications may run either with only a minimum film thickness requirement or with a broad film thickness range, such as 3 mils +/- 1 mil. If by controlling the process better with real-time film thickness feedback, a variation of +/- 0.4 mils is achievable, the process can be adjusted to target a film thickness of 2.4 mil, which is a 20% material savings (Figure 2). In fact, plants in Europe have realized savings as high as 28% as observed in the following case study. “The Coatmaster provides us with quantitative and immediate feedback on investment decisions. In this way, we can selectively and safely reduce layer thicknesses to the lower tolerance threshold. Last year, thanks to the Coatmaster, we reduced our powder consumption by a total of 28%, clearly exceeding our expectations.” Says Kai Altenburg, Head of Surface Technology at Ernst Schweizer Metallbau, a manufacturer of architectural components.

Adjustments based on feedback from the Coatmaster allow for the process to quickly be brought into the control range
FIGURE 2 » Adjustments based on feedback from the Coatmaster allow for the process to quickly be brought into the control range.

The Coatmaster is now being introduced in North America and is available in multiple configurations. There is a version designed for systems where the measurement system is static or requires minimal movement, a version designed to be integrated into a robot or more complex automation, and a handheld, battery-operated version called the Flex that is now available (Figure 3). For uncured powder over metal, a version called the Coatmaster 3D is available. With this system, the part is tracked and measured for 1-2 seconds after being slightly warmed by lights. The data is processed for 10-12 seconds and a heat map of the film thickness is created, showing variations in coating thickness for areas as large as 32” x 60” (Figure 4). This can be used to provide immediate feedback to manual applicators or as a means to more rapidly and thoroughly adjust and automated coating process.

The Flex handheld, battery-operated unit
FIGURE 3 » The Flex handheld, battery-operated unit.
Film thickness map of the Coatmaster 3D
FIGURE 4 » Film thickness map of the Coatmaster 3D.

The flexibility, responsiveness and accuracy of the new technology implemented in the Coatmaster allows for process control of powder applications that have never previously been achievable. 

 

For more information, email info@coatmasterus.com or visit www.coatmasterus.com.

KEYWORDS: coating thickness gauge Testing Equipment

Share This Story

Looking for a reprint of this article?
From high-res PDFs to custom plaques, order your copy today!

Martin Rola, President, Sapience Automation, Charleston, SC

Recommended Content

JOIN TODAY
to unlock your recommendations.

Already have an account? Sign In

  • Double exposure of creative chemistry concept on laptop background, research and development concept

    Inside the AI Shift in Coatings

    Industry leaders share real-world examples of how AI is...
    Sustainable
    By: PCI Editorial Staff
  • Global Top 10 and PCI Logo

    2026 Global Top 10: Top Paint and Coatings Companies

    See how the world’s largest paint and coatings companies...
    Global Top 10 and PCI 25
    By: Courtney Bassett
  • The 2026 PCI 25

    2026 PCI 25: Top Paint and Coatings Companies

    See how North America's largest paint and coatings...
    Global Top 10 and PCI 25
    By: Courtney Bassett
You must login or register in order to post a comment.

Report Abusive Comment

Manage My Account
  • eMagazine
  • Newsletters
  • Online Registration
  • Subscription Customer Service

More Videos

Sponsored Content

Sponsored Content is a special paid section where industry companies provide high quality, objective, non-commercial content around topics of interest to the PCI audience. All Sponsored Content is supplied by the advertising company and any opinions expressed in this article are those of the author and not necessarily reflect the views of PCI or its parent company, BNP Media. Interested in participating in our Sponsored Content section? Contact your local rep!

close
  • wooden kitchen set and shelving
    Sponsored bySirca North America

    Leveraging Coatings to Meet ESG Goals in Manufacturing

  • man woodworking in workshop
    Sponsored byGemini Industries, Inc.

    Waterborne Coatings Aren't the Future -- They're the New Performance Benchmark

Popular Stories

Breaking News

16 Taken to Hospitals After Incident at Massachusetts Coating Facility

USA election voters in red and blue to represent democrats and republicans

The AkzoNobel-Axalta Vote is Over. What Will Regulators Ask Next?

3d rendering of exclamation mark on speech bubble.

PFAS Update 2026

Webinar custom content box

Events

September 15, 2026

Coatings Trends & Technologies Summit

The Coatings Trends & Technologies (CTT) Summit is an annual conference for both liquid and powder coatings formulators and manufacturers to discuss innovations in coatings technology. This event combines high-quality technical presentations, a resource-rich exhibit hall, and dedicated networking opportunities to connect scientific minds, foster innovation, and cultivate game-changing new ideas!

January 1, 2030

Webinar Sponsorship Information

For webinar sponsorship information, visit www.bnpevents.com/webinars or email webinars@bnpmedia.com.

View All Submit An Event

Products

Advanced Coating Materials

Advanced Coating Materials

See More Products
Webinar custom content box

Related Articles

  • LITERATURE: Film Thickness Measurement Brochure

    See More
  • Coating Thickness Measurement Tool

    See More
  • Coating Thickness Measurement Tool

    See More

Related Products

See More Products
  • thin film.jpg

    Thin Film Coatings Properties, Deposition, and Applications

See More Products
×

Keep the info flowing with our eNewsletters!

Get the latest industry updates tailored your way.

JOIN TODAY!
  • RESOURCES
    • Advertise
    • Contact Us
    • Directories
    • Store
    • Want More
    • Manufacturing Division
  • SIGN UP TODAY
    • Create Account
    • eMagazine
    • Newsletters
    • Customer Service
    • Manage Preferences
  • SERVICES
    • Marketing Services
    • Reprints
    • Market Research
    • List Rental
    • Survey & Sample
  • STAY CONNECTED
    • LinkedIn
    • Facebook
    • Youtube
    • X (Twitter)
  • PRIVACY
    • PRIVACY POLICY
    • TERMS & CONDITIONS
    • DO NOT SELL MY PERSONAL INFORMATION
    • PRIVACY REQUEST
    • ACCESSIBILITY

Copyright ©2026. All Rights Reserved BNP Media, Inc. and BNP Media II, LLC.

Design, CMS, Hosting & Web Development :: ePublishing