Painting & Coating Industry (PCI) logo Powder coating summit logo
search
cart
facebook twitter linkedin youtube
  • Sign In
  • Join Today
  • Sign Out
  • My Account
Painting & Coating Industry (PCI) logo Powder coating summit logo
  • NEWS
    • Latest News
    • PCI News Now
    • Market Trends & Reports
    • Finishing News
    • Price Alerts
    • Global Top 10/ PCI 25
  • PRODUCTS
    • Product News
    • Featured Products
    • Must See Products and Services
  • MATERIALS
    • Additives
    • Resins/Polymers
    • Pigments
    • Equipment
    • Distributors
  • TECHNOLOGIES
    • Adhesives
    • Architectural Coatings
    • Finishing Articles
    • Finishing Technologies
    • Finishing Equipment
    • Industrial Coatings
    • Nanotechnology
    • Powder Coatings
    • Solventborne
    • Special Purpose Coatings
    • Sustainability
    • UV Coatings
    • Waterborne
  • EVENTS
    • Coatings Trends & Technologies Summit
    • Paint and Coatings Academy
    • Webinars
    • Calendar of Events
    • Lifetime Achievement Award
  • DIRECTORIES
    • Buyer's Guide
    • Equipment Directory
    • Materials Directory
  • RESOURCES
    • Columns
      • Did you know?
      • Distribution Dive
      • Formulating With Mike
      • Innovation Insights
      • Powder Coating Perspectives
      • TiO2 Insider
    • Blogs
      • Editor's Viewpoint
      • Industry Insights
    • Coatings Supplier Handbook
    • COAT-IT! Podcast
    • Videos
    • PCI Store
    • eBooks
    • Sponsor Insights
  • EMAGAZINE
    • eMagazine
    • Archive Issues
    • Editorial Advisory Board
    • CONTACT
    • Advertise
  • JOIN!
Powder CoatingsPowder Coating Perspectives

FBE Powder Coatings Remain a Cornerstone of Pipeline Protection Strategies

By Eric Casebolt
Web-Poster-GI-1253225696-1170x658.jpg

Image credit: cgtoolbox / Creatas Video via Getty Images.

June 4, 2025

Battling corrosion is a costly but critical requirement for the oil and gas industry. Billions of dollars are spent each year to protect and repair high-value infrastructure from corrosion. When it comes to pipelines, fusion-bonded epoxy (FBE) powder coatings play a central role.

FBE coatings have become a staple in pipeline protection, dominating as the primary coating solution for buried and subsea applications. These pipelines, often stretching thousands of miles, face continuous exposure to aggressive environmental conditions. FBE coatings form a durable barrier against moisture, soil electrolytes and corrosive chemicals, extending asset life while minimizing leaks and costly downtime.


Corrosion Prevention Strategies

Two key strategies, which are often used synergistically, can combat corrosion in pipeline applications: cathodic protection systems and anticorrosive coatings.

Cathodic protection systems work by converting the pipeline into the cathode of a galvanic cell. This is achieved by coupling it with a less noble metal, which serves as the anode and corrodes in place of the steel. When used in this manner, this less noble metal is commonly referred to as a “sacrificial anode,” thus offering “cathodic protection” to the pipeline. While more sophisticated cathodic protection systems exist, such as impressed current systems, the fundamental principle remains the same.

Complementing the cathodic protection systems are anticorrosive coatings, which form a physical barrier between the steel and the environment. These coatings may be solvent-based or powder coatings, and they can range from single to multilayer depending on pipeline location, environmental exposure and mechanical stress requirements. The main principle being employed here is to inhibit moisture and electrolytes from reaching the surface of the metal, thus preventing the initiation of corrosion.


Fundamentals of FBE Powder Coatings

FBE coatings are thermosetting powder coatings designed specifically to perform in the highly aggressive environments that pipelines are subjected to. The main binder consists of epoxy resin and curing agents that are formulated to form a tough, chemically resistant layer that bonds tightly to the substrate. These coatings typically utilize specialty materials and functional fillers, such as wollastonite, to improve mechanical strength, thermal stability and corrosion resistance to ensure optimal protection.

The application process is highly controlled. First, the surface of the pipeline undergoes abrasive blasting to remove contaminants and provide a roughened surface profile to maximize mechanical adhesion. The pipe is then preheated to 180–250 °C prior to coating application, a technique that ensures maximum bonding once the powder is applied.

Next, the FBE coating is electrostatically applied onto the hot surface, where it immediately flows and begins to cure, eventually forming a highly crosslinked film with a typical dry film thickness of 250–500 µm (10–20 mils). In some cases, the pipe may undergo a post-curing process to ensure the coating is fully crosslinked. Once sufficiently cooled via air or water jets, the coating is inspected for dry film thickness, continuity (holiday detection) and other parameters that are critical to performance in the field.


A Cornerstone in Pipeline Protection

FBE powder coatings owe their popularity to a variety of factors when compared to solvent-based coatings. The application process of FBE coatings is more efficient, as they only require one layer as opposed to the two or even three layers that are often required to adequately protect the pipeline with solvent-based coatings.

Durability is another key advantage. FBE coatings resist damage from abrasion and mechanical stresses that can be encountered during pipeline handling and installation. Their strong adhesion to steel (achieved during the fusion process) minimizes the risk of delamination, even under thermal cycling conditions. The strong bond also provides excellent resistance to cathodic disbondment, which is one of the more difficult requirements for pipeline applications.

Environmentally, FBE coatings have a significant advantage. They are 100% solids systems and thus emit virtually zero volatile organic compounds (VOCs) during the application and curing processes. Their high level of durability offers long service life, reducing the need for frequent maintenance or recoating, which lowers both the environmental impact and lifecycle costs of pipeline operations. Altogether, FBE coatings offer an attractive balance of cost, performance and sustainability profile for pipeline applications.


Challenges and Limitations of FBE Coatings

Despite their advantages, FBE coatings are not without challenges. The application process demands precision, as inadequate surface preparation or curing can compromise performance and lead to premature field failure. FBE coatings also lack flexibility at higher film builds and can be susceptible to cracking if the coated pipes are bent too aggressively. Additionally, because the system relies on high temperatures for application and curing, field repairs and coating of weld joints typically require the use of liquid coatings or other specialized repair materials.


Optimal Balance of Properties

Fusion-bonded epoxy powder coatings continue to play a central role in pipeline protection strategies. Their unmatched combination of corrosion resistance, mechanical durability and environmental performance makes them an ideal solution for buried and subsea pipelines. While they require careful application and have limitations in flexibility and repairability, their long-term benefit to service life makes FBE coatings a trusted choice in safeguarding critical pipeline infrastructure.

For more information, contact the author at ecasebolt@chemquest.com or visit https://chemquest.com.

KEYWORDS: Corrosion Control Epoxy Resins pipeline coatings

Share This Story

Looking for a reprint of this article?
From high-res PDFs to custom plaques, order your copy today!

By Eric Casebolt, Vice President, The ChemQuest Group, Inc.

Recommended Content

JOIN TODAY
to unlock your recommendations.

Already have an account? Sign In

  • Double exposure of creative chemistry concept on laptop background, research and development concept

    Inside the AI Shift in Coatings

    Industry leaders share real-world examples of how AI is...
    Paint and Coating Resins & Polymers
    By: PCI Editorial Staff
  • Global Top 10 and PCI Logo

    2026 Global Top 10: Top Paint and Coatings Companies

    See how the world’s largest paint and coatings companies...
    Global Top 10 and PCI 25
    By: Courtney Bassett
  • The 2026 PCI 25

    2026 PCI 25: Top Paint and Coatings Companies

    See how North America's largest paint and coatings...
    Global Top 10 and PCI 25
    By: Courtney Bassett
You must login or register in order to post a comment.

Report Abusive Comment

Manage My Account
  • Join Paint & Coatings Industry
  • Manage My Preferences
  • Customer Service

More Videos

Popular Stories

Mergers and aquisitions

BASF Ends Evonik Takeover Pursuit

Breaking News

H.B. Fuller to Close Seven Sites in Supply-Chain Overhaul

AkzoNobel Axalta

EU Clears $25B Akzo-Axalta Merger with One Big Condition

Events

December 2, 2026

Self-Activated Binder Technology: A New Path to Tin-Free Polyurethane Coatings

Through examples from protective and general industrial coating applications, attendees will learn how these innovative technologies can help maintain, and in some cases improve, coating performance while supporting safer, more sustainable formulations that align with evolving regulatory expectations

December 10, 2026

PC Academy: Waterborne Polymers and Film Formation

The trend towards waterborne polymers in the paint and coatings industry is clear; highlighting their environmentally friendly nature, regulatory considerations, growing market demand, and meeting sustainability goals.

View All Submit An Event

Products

Powder Coatings - Foundation for the Novice Formulator (ebook)

Powder Coatings - Foundation for the Novice Formulator (ebook)

See More Products
PCI news now promo ad

Related Articles

  • Development of Novel Toughening Technology for Fusion-Bonded-Epoxy (FBE) Powder Coatings

    See More
  • Market for Pipeline Protection Expands as Needs Grow

    See More
  • An image taken during application, where salt crust, the water table and intermediate soil layers are clearly visible.

    Visco-Elastic Technology Enhances Pipeline Protection and Market Growth

    See More

Related Directories

  • Micro Powders

    Micro Powders' additives solve problems and achieve unique coating surface effects including: slip; rub, abrasion, and scratch resistance; gloss reduction, burnish resistance; water repellency; texture, tactile, and soft touch effects. We are leaders in creating innovative particle technologies, including natural/biodegradable grades and nanocomposite wax PTFE alternatives.
×

Keep the info flowing with our eNewsletters!

Get the latest industry updates tailored your way.

JOIN TODAY!
  • RESOURCES
    • Advertise
    • Contact Us
    • Directories
    • Store
    • Manufacturing Division
  • JOIN TODAY
    • Create Account
    • eMagazine
    • Newsletters
    • Customer Service
    • Manage Preferences
  • SERVICES
    • Marketing Services
    • Reprints
    • Market Research
    • List Rental
    • Survey & Sample
  • STAY CONNECTED
    • LinkedIn
    • Facebook
    • Youtube
    • X (Twitter)
  • PRIVACY
    • PRIVACY POLICY
    • TERMS & CONDITIONS
    • DO NOT SELL MY PERSONAL INFORMATION
    • PRIVACY REQUEST
    • ACCESSIBILITY

Copyright ©2026. All Rights Reserved BNP Media, Inc. and BNP Media II, LLC.

Design, CMS, Hosting & Web Development :: ePublishing