Painting & Coating Industry (PCI) logo Powder coating summit logo
search
cart
facebook twitter linkedin youtube
  • Sign In
  • Create Account
  • Sign Out
  • My Account
Painting & Coating Industry (PCI) logo Powder coating summit logo
  • NEWS
    • Latest News
    • Market Trends & Reports
    • Finishing News
    • Price Alerts
    • Subscribe to Newsletters
    • Global Top 10/ PCI 25
    • Weekly Featured Article
  • PRODUCTS
    • Product News
    • Featured Products
    • Must See Products and Services
  • MATERIALS
    • Additives
    • Resins/Polymers
    • Pigments
    • Equipment
    • Distributors
  • TECHNOLOGIES
    • Adhesives
    • Architectural Coatings
    • Finishing Articles
    • Finishing Technologies
    • Finishing Equipment
    • Industrial Coatings
    • Nanotechnology
    • Powder Coatings
    • Solventborne
    • Special Purpose Coatings
    • Sustainability
    • UV Coatings
    • Waterborne
  • RESOURCES
    • Columns
      • Did you know?
      • Distribution Dive
      • Formulating With Mike
      • Innovation Insights
      • Powder Coating Perspectives
      • TiO2 Insider
    • Blogs
      • Editor's Viewpoint
      • Industry Insights
    • Coatings Supplier Handbook
    • Podcasts and Videos
      • COAT-IT! Podcast
      • Videos/PCI TV
    • PCI Store
    • Classifieds
    • eBooks
    • Sponsor Insights
    • White Papers
    • COATLE Word Game
  • EVENTS
    • Coatings Trends & Technologies Summit
    • Paint and Coatings Academy
    • Webinars
    • Calendar of Events
    • Lifetime Achievement Award
  • DIRECTORIES
    • Buyer's Guide
    • Equipment Directory
    • Materials Directory
  • EMAGAZINE
    • Current Issue
    • eMagazine Archive
    • China Issue Archive
    • Editorial Advisory Board
  • CONTACT
    • Contact Us
    • Advertise
    • Subscribe to eMagazine
    • Subscribe to Newsletters
  • SIGN UP!
Paint and Coating Market ReportsIndustry News

New Report Examines Epoxy Resin Demand

Magnifying glass and documents with analytics data lying on tablet
Credit: tonefotografia / iStock via Getty Images Plus
November 14, 2025

In a report by Polaris Market Research, the global epoxy resins market continues to expand as demand increases across construction, electronics, automotive, aerospace, marine, and emerging renewable energy applications. The report notes that epoxy resins are widely used for their strong adhesion, durability, and versatility in bonding, coating, and sealing.

The analysis details how epoxy resins support a range of applications in construction and infrastructure, such as concrete repair and epoxy-based floor coatings used in industrial, warehouse, and garage environments. In electronics, epoxy resins are critical for potting and encapsulating sensitive components to protect against moisture, heat, and dust. These materials help prevent short circuits and extend the lifespan of electronic products.

Epoxy Resin MarketCredit: Polaris Market Research and Consulting


The report highlights the importance of epoxy resins in automotive and aerospace applications due to their strength and lightweight performance. Epoxy-based composites are used in components such as car panels and aircraft structures, and the materials also support high-temperature bonding in engine parts.

Demand for epoxy resins is also growing in art and consumer applications. Artists and makers use epoxy formulations for glossy, durable finishes on tables, paintings, and countertops. Jewelry-makers use resin for cast pieces and embedded designs. The material’s clarity and protective properties continue to support widespread DIY adoption.

Marine applications remain a significant category due to the resin’s water resistance and long-term durability. Epoxy formulations protect hulls from corrosion and maintain essential functions across various vessel components.

Regionally, Asia Pacific leads demand due to rapid industrialization and strong automotive, construction, and electronics sectors. China plays a major role with expanding infrastructure and renewable energy projects. North America is experiencing increased demand through aerospace, automotive, and clean energy investments. The United States market continues to grow in electronics, EV manufacturing, and infrastructure development. Europe’s demand reflects an emphasis on lightweight materials for automotive and aerospace uses as well as offshore wind energy projects.

The report notes that future growth will be supported by electric vehicles, renewable energy, advanced manufacturing technologies, and the development of environmentally friendly epoxy formulations. Epoxy resins are expected to remain essential in applications where strength, durability, and lightweight performance are critical.

Access the full report here.

KEYWORDS: epoxy Epoxy Resins Market Forecasts market reports

Share This Story

Looking for a reprint of this article?
From high-res PDFs to custom plaques, order your copy today!

Recommended Content

JOIN TODAY
to unlock your recommendations.

Already have an account? Sign In

  • Double exposure of creative chemistry concept on laptop background, research and development concept

    Inside the AI Shift in Coatings

    Industry leaders share real-world examples of how AI is...
    Sustainable
    By: PCI Editorial Staff
  • Global Top 10 and PCI Logo

    2026 Global Top 10: Top Paint and Coatings Companies

    See how the world’s largest paint and coatings companies...
    Global Top 10 and PCI 25
    By: Courtney Bassett
  • The 2026 PCI 25

    2026 PCI 25: Top Paint and Coatings Companies

    See how North America's largest paint and coatings...
    Global Top 10 and PCI 25
    By: Courtney Bassett
You must login or register in order to post a comment.

Report Abusive Comment

Manage My Account
  • eMagazine
  • Newsletters
  • Online Registration
  • Subscription Customer Service

More Videos

Sponsored Content

Sponsored Content is a special paid section where industry companies provide high quality, objective, non-commercial content around topics of interest to the PCI audience. All Sponsored Content is supplied by the advertising company and any opinions expressed in this article are those of the author and not necessarily reflect the views of PCI or its parent company, BNP Media. Interested in participating in our Sponsored Content section? Contact your local rep!

close
  • wooden kitchen set and shelving
    Sponsored bySirca North America

    Leveraging Coatings to Meet ESG Goals in Manufacturing

  • man woodworking in workshop
    Sponsored byGemini Industries, Inc.

    Waterborne Coatings Aren't the Future -- They're the New Performance Benchmark

Popular Stories

Breaking News

16 Taken to Hospitals After Incident at Massachusetts Coating Facility

USA election voters in red and blue to represent democrats and republicans

The AkzoNobel-Axalta Vote is Over. What Will Regulators Ask Next?

3d rendering of exclamation mark on speech bubble.

PFAS Update 2026

Webinar custom content box

Events

September 15, 2026

Coatings Trends & Technologies Summit

The Coatings Trends & Technologies (CTT) Summit is an annual conference for both liquid and powder coatings formulators and manufacturers to discuss innovations in coatings technology. This event combines high-quality technical presentations, a resource-rich exhibit hall, and dedicated networking opportunities to connect scientific minds, foster innovation, and cultivate game-changing new ideas!

January 1, 2030

Webinar Sponsorship Information

For webinar sponsorship information, visit www.bnpevents.com/webinars or email webinars@bnpmedia.com.

View All Submit An Event

Products

Advanced Coating Materials

Advanced Coating Materials

See More Products
Webinar custom content box

Related Articles

  • Market Reports.jpg

    Report Highlights Future Growth in Epoxy Resin Market

    See More
  • Report Examines Trends in Specialty Silica Market

    See More
  • ‘Coatings 100' Report Examines Changing Face of Industry Worldwide

    See More

Related Products

See More Products
  • marketsandmarketslogo.jpg

    Protective Coatings Market by Resin Type...

See More Products

Related Directories

  • Epic Resins

    Epic Resins is a formulator of one- and two-component epoxy and polyurethane adhesives for use with natural, nylon, polyester, olefin and vinyl filaments. We have served the paint applicator industry with a complete line of standard products, as well as the ability to custom formulate. ISO 9001 and ISO 14001 Certified.
  • IGM Resins

    IGM Resins provides a broad range of photoinitiators, oligomers (epoxy, polyester and urethane), acrylate monomers and additives to address every formulating need.
×

Keep the info flowing with our eNewsletters!

Get the latest industry updates tailored your way.

JOIN TODAY!
  • RESOURCES
    • Advertise
    • Contact Us
    • Directories
    • Store
    • Want More
    • Manufacturing Division
  • SIGN UP TODAY
    • Create Account
    • eMagazine
    • Newsletters
    • Customer Service
    • Manage Preferences
  • SERVICES
    • Marketing Services
    • Reprints
    • Market Research
    • List Rental
    • Survey & Sample
  • STAY CONNECTED
    • LinkedIn
    • Facebook
    • Youtube
    • X (Twitter)
  • PRIVACY
    • PRIVACY POLICY
    • TERMS & CONDITIONS
    • DO NOT SELL MY PERSONAL INFORMATION
    • PRIVACY REQUEST
    • ACCESSIBILITY

Copyright ©2026. All Rights Reserved BNP Media, Inc. and BNP Media II, LLC.

Design, CMS, Hosting & Web Development :: ePublishing