Painting & Coating Industry (PCI) logo Powder coating summit logo
search
cart
facebook twitter linkedin youtube
  • Sign In
  • Create Account
  • Sign Out
  • My Account
Painting & Coating Industry (PCI) logo Powder coating summit logo
  • NEWS
    • Latest News
    • Market Trends & Reports
    • Finishing News
    • Price Alerts
    • Subscribe to Newsletters
    • Global Top 10/ PCI 25
    • Weekly Featured Article
    • COATLE Word Game
  • PRODUCTS
    • Product News
    • Featured Products
    • Must See Products and Services
  • MATERIALS
    • Additives
    • Resins/Polymers
    • Pigments
    • Equipment
    • Distributors
  • TECHNOLOGIES
    • Adhesives
    • Architectural Coatings
    • Finishing Articles
    • Finishing Technologies
    • Finishing Equipment
    • Industrial Coatings
    • Nanotechnology
    • Powder Coatings
    • Solventborne
    • Special Purpose Coatings
    • Sustainability
    • UV Coatings
    • Waterborne
  • RESOURCES
    • Columns
      • Did you know?
      • Distribution Dive
      • Formulating With Mike
      • Innovation Insights
      • Powder Coating Perspectives
      • TiO2 Insider
    • Blogs
      • Editor's Viewpoint
      • Industry Insights
    • Coatings Supplier Handbook
    • Podcasts and Videos
      • COAT-IT! Podcast
      • Videos/PCI TV
    • PCI Store
    • Classifieds
    • eBooks
    • Sponsor Insights
    • White Papers
    • COATLE Word Game
  • EVENTS
    • Coatings Trends & Technologies Summit
    • Paint and Coatings Academy
    • Webinars
    • Calendar of Events
    • Lifetime Achievement Award
  • DIRECTORIES
    • Buyer's Guide
    • Equipment Directory
    • Materials Directory
  • EMAGAZINE
    • Current Issue
    • eMagazine Archive
    • China Issue Archive
    • Editorial Advisory Board
  • CONTACT
    • Contact Us
    • Advertise
    • Subscribe to eMagazine
    • Subscribe to Newsletters
  • SIGN UP!
Home » Topics » Featured Stories

Featured Stories
Featured Stories RSS Feed RSS

Building Façades with an Eye for Color and the Environment

Falk Timo Tragor
October 1, 2008
No Comments
Modern façade paints must be weather resistant, diffusible and feature long-lasting fastness.
Read More

How to Formulate "Eco-Friendly" Anticorrosive Coatings

Lluis Justo
October 1, 2008
No Comments
“Eco-friendly corrosion inhibitors” should not contain heavy metals, non reportable compounds or ingredients, and be green-label compliant and also zinc free.
Read More

Crystallinity of Coatings Based on Polyvinylidene Fluoride

Dr. Robert Iezzi
October 1, 2008
No Comments
The degree of crystallinity and crystal size of coatings based on semi-crystalline polymers such as PVDF can be controlled by controlling the thermal history of the coating, and the cooling rate after baking.
Read More

2-Component Polyurethane Topcoats

Kurt Best Dr. Edward Squiller
October 1, 2008
8 Comments
Polyurethane coatings are used today as architectural coatings, product finishes, automotive coatings and industrial maintenance coatings, making them among the most versatile coating types available.(1)Polyurethane topcoats were introduced to the
Read More

Beyond the Zahn Cup

Vincent Hebert
October 1, 2008
No Comments
Formulation, performance and production costs all reap the benefit gained through quick, easy and accurate flow property testing.
Read More

Novel High-Solids Systems Based On Silicone-Epoxy Resins

Anke Bartek Markus Hallack Christopher Howard Dr. Udo Schiemann
October 1, 2008
No Comments
Exploring inorganic silicone-based chemistry has led to the development of a silicone-epoxy hybrid polymer, which combines the properties of both organic and inorganic compounds in a new class of resins for protective coatings.
Read More

Trimethylol Propane Monoallyl Ether as Hydroxyl-Functional Co-Monomer

Mircea Manea Sri Pauliana Mayke Winarti
October 1, 2008
No Comments
The interest for hydroxyl-functional acrylic resins as a component in polyurethane coatings has increased not only because of improved performance through crosslinking, but also because of higher non-volatile content. Hydroxyl
Read More

Distributors Play a Critical Role in the Supply Chain

Mike McKenna
September 1, 2008
No Comments
In the ever-changing coatings industry, distributors play an important role in the supply chain.
Read More

Uncle Sam Wants U...V.

Paul Mills
September 1, 2008
No Comments
Recently, my world and the military world have collided around something in common – my favorite acronym – UV.
Read More

Engineered Polymer Nanoparticle Composites for Flexible Transparent Films

Omar Buazza Thad Druffel Scott Farmer Matthew Lattis
September 1, 2008
No Comments
This paper won the Best Paper Award at the 11th Annual Coatings for Plastics Symposium, Chicago, April 2008.
Read More
Previous 1 2 … 76 77 78 79 80 81 82 83 84 … 157 158 Next
Manage My Account
  • eMagazine
  • Newsletters
  • Online Registration
  • Subscription Customer Service

More Videos

Sponsored Content

Sponsored Content is a special paid section where industry companies provide high quality, objective, non-commercial content around topics of interest to the PCI audience. All Sponsored Content is supplied by the advertising company and any opinions expressed in this article are those of the author and not necessarily reflect the views of PCI or its parent company, BNP Media. Interested in participating in our Sponsored Content section? Contact your local rep!

close
  • wooden kitchen set and shelving
    Sponsored bySirca North America

    Leveraging Coatings to Meet ESG Goals in Manufacturing

  • man woodworking in workshop
    Sponsored byGemini Industries, Inc.

    Waterborne Coatings Aren't the Future -- They're the New Performance Benchmark

Popular Stories

Akzo, SW, Nippon Logos

AkzoNobel Rejects Cash Offer From Nippon Paint, Sherwin-Williams

BASF SE Logo

BASF Announces Strategic Business Sale

AkzoSWNipponEndTalks

Nippon Paint, Sherwin-Williams End AkzoNobel Pursuit

POB-Point-and-Shoot

PCI Buyers Guide

Submit a Request for Proposal (RFP) to suppliers of your choice with details on what you need with a click of a button

Start your RFP

Browse our Buyers Guide for manufacturers and distributors of all types of coatings products and much more!

Find Suppliers

Events

September 4, 2025

N-Butylpyrrolidone (NBP) as a Green Solvent to Replace N-Methylpyrrolidone (NMP) in Industrial Coating Applications

ON DEMAND: EPA published a regulation proposal around N-methylpyrrolidone (NMP) in June 2024 to ban or limit NMP in many applications, such as paints and coatings and their removers. N-butylpyrrolidone (NBP) is a powerful and versatile solvent for a variety of industries looking for alternatives to substance of very high concern (SVHC)-listed solvents.

September 15, 2026

Coatings Trends & Technologies Summit

The Coatings Trends & Technologies (CTT) Summit is an annual conference for both liquid and powder coatings formulators and manufacturers to discuss innovations in coatings technology. This event combines high-quality technical presentations, a resource-rich exhibit hall, and dedicated networking opportunities to connect scientific minds, foster innovation, and cultivate game-changing new ideas!

View All Submit An Event

Poll

Longest-running laboratory experiment

What is the longest-running laboratory experiment?
View Results Poll Archive

Products

Automotive Paints and Coatings, 2nd Edition

Now in its second edition and still the only book of its kind, this is an authoritative treatment of all stages of the coating process.

See More Products
Inside the AI Shift in Coatings - See the article now

Keep the info flowing with our eNewsletters!

Get the latest industry updates tailored your way.

JOIN TODAY!
  • RESOURCES
    • Advertise
    • Contact Us
    • Directories
    • Store
    • Want More
    • Manufacturing Division
  • SIGN UP TODAY
    • Create Account
    • eMagazine
    • Newsletters
    • Customer Service
    • Manage Preferences
  • SERVICES
    • Marketing Services
    • Reprints
    • Market Research
    • List Rental
    • Survey & Sample
  • STAY CONNECTED
    • LinkedIn
    • Facebook
    • Youtube
    • X (Twitter)
  • PRIVACY
    • PRIVACY POLICY
    • TERMS & CONDITIONS
    • DO NOT SELL MY PERSONAL INFORMATION
    • PRIVACY REQUEST
    • ACCESSIBILITY

Copyright ©2026. All Rights Reserved BNP Media, Inc. and BNP Media II, LLC.

Design, CMS, Hosting & Web Development :: ePublishing