Painting & Coating Industry (PCI) logo Powder coating summit logo
search
cart
facebook twitter linkedin youtube
  • Sign In
  • Join Today
  • Sign Out
  • My Account
Painting & Coating Industry (PCI) logo Powder coating summit logo
  • NEWS
    • Latest News
    • PCI News Now
    • Market Trends & Reports
    • Finishing News
    • Price Alerts
    • Global Top 10/ PCI 25
  • PRODUCTS
    • Product News
    • Featured Products
    • Must See Products and Services
  • MATERIALS
    • Additives
    • Resins/Polymers
    • Pigments
    • Equipment
    • Distributors
  • TECHNOLOGIES
    • Adhesives
    • Architectural Coatings
    • Finishing Articles
    • Finishing Technologies
    • Finishing Equipment
    • Industrial Coatings
    • Nanotechnology
    • Powder Coatings
    • Solventborne
    • Special Purpose Coatings
    • Sustainability
    • UV Coatings
    • Waterborne
  • EVENTS
    • Coatings Trends & Technologies Summit
    • Paint and Coatings Academy
    • Webinars
    • Calendar of Events
    • Lifetime Achievement Award
  • DIRECTORIES
    • Buyer's Guide
    • Equipment Directory
    • Materials Directory
  • RESOURCES
    • Columns
      • Did you know?
      • Distribution Dive
      • Formulating With Mike
      • Innovation Insights
      • Powder Coating Perspectives
      • TiO2 Insider
    • Blogs
      • Editor's Viewpoint
      • Industry Insights
    • Coatings Supplier Handbook
    • COAT-IT! Podcast
    • Videos
    • PCI Store
    • eBooks
    • Sponsor Insights
  • EMAGAZINE
    • eMagazine
    • Archive Issues
    • Editorial Advisory Board
    • CONTACT
    • Advertise
  • JOIN!
Home » Topics » Paint and Coatings Additives

Paint and Coatings Additives
Paint and Coatings Additives RSS Feed RSS

pci0220-Adaptive-175539860-900.jpg

A Greener Solution to Deter Marine Biofouling

Philseok Kim Teluka Galhenage
February 11, 2020
One Comment
SLIPS Foul Protect N1x has successfully demonstrated the pathway to reducing marine fouling with a non-toxic, environmentally friendly approach combining the smooth and slippery liquid-based surface (Physical module) and highly branched amphiphilic SAPs (Chemical module).
Read More
pci0220-BYK--1163891251-900.jpg

Novel Silicone Surfactants for Waterborne Wood Coatings

Excellent Performance at Highest Application Speeds
Michael Toth Marcus Wessel Marcel Krohnen
February 4, 2020
3 Comments
Due to their tailored system compatibility, the new sili¬cone surfactants are suitable for use in both aqueous one-component systems as well as in aqueous two-com¬ponent polyurethane and radiation-curable systems.
Read More
pci1220-Bitrez-627864824-Lead-900.jpg

A New Generation of REACH-Compliant Ketamine Epoxy Curing Agents

Paul Jones
January 9, 2020
No Comments
Laboratory tests prove that the new generation of ketamines are unique - not only are they REACH compliant, but technically they also outperform their conventional counterparts both during and after cure, as well as offering both long pot-life and reduced hazard, making them the ideal curing agents for the paint and coatings industry.
Read More
pci1019-Corning-AMpowderOnly35134-Lead-900.jpg

Copper-Containing Glass Ceramic with High Antimicrobial Efficacy

Timothy M. Gross Joydeep Lahiri Avantika Golas Jian Luo Florence Verrier Jackie L. Kurzejewski David E. Baker Jie Wang Paul F. Novak Michael J. Snyder
October 9, 2019
One Comment
This article describes an alkali copper aluminoborophosphosilicate glass ceramic material that acts as a sustainable delivery system for Cu+1 ions with high antimicrobial efficacy.
Read More
pci1019-BYK-187003402-900.jpg

When the Film Thickness Does Not Determine the Leveling

Kerstin Vennhoff
October 8, 2019
No Comments
With RHEOBYK-7610, BYK has succeeded in developing a rheology additive which, in addition to the familiar properties, generates a specific viscosity profile.
Read More
pci1019-Sibelco-Lead-900.jpg

Gloss Control of Powder Coatings

by Engineered Mineral Fillers
William Mertens
October 3, 2019
No Comments
The use of barites is a proven method for accurate control of gloss in the high- to medium-gloss range. ATH is the product of choice for gloss control when the relatively high density of barite is undesired, or in applications where improved resistance to water spotting is an issue.
Read More
specialty chemicals

Specialty Chemicals Snapshot

Kristin Johansson
September 12, 2019
No Comments
Specialty chemicals are used throughout many industries, including coatings. PCI recently asked Jonathan Craig, Vice President Specialty Chemicals at Ascend Performance Materials, to discuss these performance products and the current state of the market.
Read More
pci0919-Clariant-483702288-900.jpg

Improving Outdoor Durability of Wood Coatings

Dr. Mouhcine Kanouni Jean-Yves Desrats
September 10, 2019
No Comments
These new dispersion additives provide excellent outdoor protection for all water-based polymeric binders used in exterior applications such as coatings, grouts and plasters.
Read More
pci0819-FP-181132871-900.jpg

UV-Vis-Resistant Acrylic Latexes for Wood Coating Applications

by Encapsulation of Inorganic NPs Using Mini-Emulsion Polymerization
Gabrielle Boivin Anna M. Ritcey Véronic Landry
September 9, 2019
No Comments
In this work, mini-emulsion polymerization was used to prepare formulations containing various sizes of ZnO nanoparticles in order to increase photostabilization of exterior clear coatings for wood.
Read More
perstop

Green Buildings and Sustainable Fire Safety Technology – Moving Ahead

Ryan Schoonmaker
September 4, 2019
One Comment
Green building is rapidly starting to scale up, bringing to light emerging issues such as the nexus between sustainable building design and fire safety - a challenge addressed by Perstorp's bio-based pentaerythritol for intumescent coatings.
Read More
Previous 1 2 … 25 26 27 28 29 30 31 32 33 … 52 53 Next
Manage My Account
  • Join Paint & Coatings Industry
  • Manage My Preferences
  • Customer Service

More Videos

Popular Stories

industry news

Dozens Treated After Toledo Chemical Release

Mergers and aquisitions

Evonik Holds Off on BASF Takeover Talks

AkzoNobel Axalta

EU Clears $25B Akzo-Axalta Merger with One Big Condition

Events

November 19, 2026

Reformulating Paints with AI: Turn Change into a Competitive Advantage

Join industry leaders and experts for real case studies showing how AI helps R&D teams use existing paint formulation and test data to evaluate alternatives, predict trade-offs, and prioritize experiments.

December 10, 2026

PC Academy: Waterborne Polymers and Film Formation

The trend towards waterborne polymers in the paint and coatings industry is clear; highlighting their environmentally friendly nature, regulatory considerations, growing market demand, and meeting sustainability goals.

View All Submit An Event

Products

Powder Coatings - Foundation for the Novice Formulator (ebook)

Powder Coatings - Foundation for the Novice Formulator (ebook)

See More Products
PCI news now promo ad

Keep the info flowing with our eNewsletters!

Get the latest industry updates tailored your way.

JOIN TODAY!
  • RESOURCES
    • Advertise
    • Contact Us
    • Directories
    • Store
    • Manufacturing Division
  • JOIN TODAY
    • Create Account
    • eMagazine
    • Newsletters
    • Customer Service
    • Manage Preferences
  • SERVICES
    • Marketing Services
    • Reprints
    • Market Research
    • List Rental
    • Survey & Sample
  • STAY CONNECTED
    • LinkedIn
    • Facebook
    • Youtube
    • X (Twitter)
  • PRIVACY
    • PRIVACY POLICY
    • TERMS & CONDITIONS
    • DO NOT SELL MY PERSONAL INFORMATION
    • PRIVACY REQUEST
    • ACCESSIBILITY

Copyright ©2026. All Rights Reserved BNP Media, Inc. and BNP Media II, LLC.

Design, CMS, Hosting & Web Development :: ePublishing