The performance of field-applied UV-curable floor finishes based on new UV-curable polyurethane dispersions has been compared to that of conventional floor finishes.
This article discusses the three types of OPVs and emphasizes the use of cellulose esters as additives to improve flow and leveling, and in many cases adhesion.
A unique acrylic/polyurethane technology has been described that offers a new mechanism for the faster release of coalescent from industrial wood coatings.
Newer ultrafine nepheline syenite sizes have refractive index and physical properties that are particularly well suited for use as a performance additive in radiation-curable coatings, inks and adhesives.
This paper will review the current use of silica nanoparticles in UV-curable coatings and introduce effective approaches for delivering silica nanoparticles to UV-curable resin formulations without the drawbacks of current solvent- or monomer-based silica nanoparticle dispersions.