Sachtleben has expanded its Sachtoperse family of barium sulphate pigments to include new patented, functionalized pigments designed to optimize paint properties and meet new requirements in the coatings market.
Troy Corp.’s exhibit, through performance data and extensive product details, highlighted how Troy can help customers reach performance and cost targets through advanced, high-performance products with exceptional technical service.
At this year’s American Coatings Show, specialty chemicals group LANXESS presented material protection products as well as organic and inorganic pigments that fulfill the most exacting of requirements.
At its booth at the American Coatings Show, Eastman Chemical Co., Kingsport, TN, featured products from its coatings, adhesives, specialty polymers and inks (CASPI) business segment, including additives for the transportation, industrial and architectural markets, and showcased the ACS debut of Eastman Optifilm™ additive OT1200.
Celanese Emulsions is presenting a range of technologies at Booth #1200 to help paint and coating manufacturers more easily formulate low-VOC and low-odor products and introduced a “drop-in” alternative emulsion for vinyl acrylic formulations with high-scrub resistance.