Painting & Coating Industry (PCI) logo Powder coating summit logo
search
cart
facebook twitter linkedin youtube
  • Sign In
  • Create Account
  • Sign Out
  • My Account
Painting & Coating Industry (PCI) logo Powder coating summit logo
  • NEWS
    • Latest News
    • Market Trends & Reports
    • Finishing News
    • Price Alerts
    • Global Top 10/ PCI 25
  • PRODUCTS
    • Product News
    • Featured Products
    • Must See Products and Services
  • MATERIALS
    • Additives
    • Resins/Polymers
    • Pigments
    • Equipment
    • Distributors
  • TECHNOLOGIES
    • Adhesives
    • Architectural Coatings
    • Finishing Articles
    • Finishing Technologies
    • Finishing Equipment
    • Industrial Coatings
    • Nanotechnology
    • Powder Coatings
    • Solventborne
    • Special Purpose Coatings
    • Sustainability
    • UV Coatings
    • Waterborne
  • EVENTS
    • Coatings Trends & Technologies Summit
    • Paint and Coatings Academy
    • Webinars
    • Calendar of Events
    • Lifetime Achievement Award
  • DIRECTORIES
    • Buyer's Guide
    • Equipment Directory
    • Materials Directory
  • RESOURCES
    • Columns
      • Did you know?
      • Distribution Dive
      • Formulating With Mike
      • Innovation Insights
      • Powder Coating Perspectives
      • TiO2 Insider
    • Blogs
      • Editor's Viewpoint
      • Industry Insights
    • Coatings Supplier Handbook
    • COAT-IT! Podcast
    • Videos
    • PCI Store
    • eBooks
    • Sponsor Insights
  • EMAGAZINE
    • eMagazine
    • Archive Issues
    • Editorial Advisory Board
    • CONTACT
    • Advertise
  • SIGN UP!
Home » Topics » Paint & Coatings Industry Top Stories

Paint & Coatings Industry Top Stories
Paint & Coatings Industry Top Stories RSS Feed RSS

ask-joe-powder-column-1170.jpg

Ask Joe Powder: Recoating Wrinkle Finishes

Kevin Biller
July 17, 2023
No Comments

We currently use a "midnight black” wrinkle powder coating supplied by a major powder producer. Can a second touchup coat be applied after the first coat has cured? Read the answer to this question and more in this edition of Ask Joe Powder. 


Read More
pci0423-Distributor-1353785280-1170.jpg

Safely Transporting Essential Ingredients

Eric Byer
July 13, 2023
No Comments

This article explores the expertise, steadfast commitment to safety, and overarching mindset of responsibility that is invested to get chemical ingredients where they need to go.


Read More
pci0723-Cov-672906220-1440.jpg

2023 PCI 25: Top Paint and Coatings Companies

Annual Ranking of Top Paint and Coatings Companies
Courtney Bassett
July 11, 2023
5 Comments
PCI’s annual ranking of the top 25 North American paint and coatings manufacturers, based on 2022 coatings sales. Sales of non-coating products are not included.
Read More
pci1222-TIO2-669596876-1170.jpg

TiO2 Industry: Where is the Light at the End of the Tunnel?

Gerald Colamarino
July 8, 2023
No Comments

The TiO2 industry continues to experience difficult times. Multi-national producer volume in 1Q23 was 31% lower than 1Q22, while net exports from China increased 22%. This followed a fourth quarter that was down 35% compared to the previous year. Is there a light at the end of the tunnel, and if so, how long is the tunnel?


Read More
Neptune Image 2.jpg

Key Considerations for Selecting a Portable Mixer

Eulis Ester
July 8, 2023
No Comments

The needs of fluid-handling operations are as varied as the kinds of liquids they handle. For those that mix fluids together, some might require small-batch blending, while others need to mix large quantities. Some operations need only gentle mixing, while others may require vigorous agitation. So, how do you know what the right mixer is for your operation?


Read More
GettyImages-1421709258.jpg

Amorphous vs. Crystalline Polymers

Ibrahim El-Hedok
July 8, 2023
One Comment

Polymers are unlike other types of compounds because of their extremely large size, which has a great impact on their unique properties and how they behave in different phase states. Many applications of polymers and polymer coatings need flexibility at low to ambient temperatures. This article explores the difference between amorphous and crystalline polymers.


Read More
pci0723-Cov-672906220-1440.jpg

2023 Global Top 10: Top Paint and Coatings Companies

Annual Ranking of Top Paint and Coatings Companies
Courtney Bassett
July 6, 2023
19 Comments
Who ranks on top? PCI’s annual ranking of the top 10 global paint and coatings manufacturers reveals who had the highest coatings sales in 2022.
Read More
GettyImages-1450272068.jpg

Solar Glass Coatings Enhance Electricity Production

Strategic Market Research
July 3, 2023
No Comments

The United States has increased the use of solar and wind power for electricity production. The U.S. Department of Energy claims that preserving your panels' surface with a glass coating can boost the photoelectric effect by up to 3-6%, therefore boosting potential demand in the glass coatings market. 


Read More
ION Science Lead Image.jpg

High-Performance Sensors Underpin the Quality of Occupational Safety Equipment

ION Science Ltd.
June 22, 2023
One Comment

Employers have a duty of care to protect the health, safety, and welfare of employees, so it is vitally important to keep workers’ occupational exposure to harmful gases within permissible limits. For this reason, providing highly accurate sensors that are reliable is a must. 


Read More
Wagner Lead Image.jpg

Resource-Saving Coating Technology for Rail Vehicle Wheels

Walther Spritz- und Lackiersysteme GmbH
June 20, 2023
No Comments

In order to adapt to the increasing demand in rail transport, a wheelset system production plant was modernized to include use of a highly efficient coating line that emphasizes sustainability and resource-saving production value. 


Read More
Previous 1 2 … 49 50 51 52 53 54 55 56 57 … 142 143 Next
Manage My Account
  • eMagazine
  • Newsletters
  • Online Registration
  • Subscription Customer Service

More Videos

Popular Stories

Evonik Logo

Evonik to Close Two German Sites

Mergers-and-Company-Strategies.jpg

BASF Confirms Exploratory Talks on Potential Evonik Takeover

Sherwin-Williams

Sherwin-Williams Opens Largest North American Plant

Webinar custom content box

Events

November 5, 2026

Advancing Polyester Powder Coatings: Breakthroughs in Flexibility and Low-Cure Performance

Join us to learn how to improve coating durability while keeping your manufacturing process efficient. Explore the latest advancements in polyester powder coating technology.

January 1, 2030

Webinar Sponsorship Information

For webinar sponsorship information, visit www.bnpevents.com/webinars or email webinars@bnpmedia.com.

View All Submit An Event

Products

Advanced Coating Materials

Advanced Coating Materials

See More Products
Webinar custom content box

Keep the info flowing with our eNewsletters!

Get the latest industry updates tailored your way.

JOIN TODAY!
  • RESOURCES
    • Advertise
    • Contact Us
    • Directories
    • Store
    • Want More
    • Manufacturing Division
  • SIGN UP TODAY
    • Create Account
    • eMagazine
    • Newsletters
    • Customer Service
    • Manage Preferences
  • SERVICES
    • Marketing Services
    • Reprints
    • Market Research
    • List Rental
    • Survey & Sample
  • STAY CONNECTED
    • LinkedIn
    • Facebook
    • Youtube
    • X (Twitter)
  • PRIVACY
    • PRIVACY POLICY
    • TERMS & CONDITIONS
    • DO NOT SELL MY PERSONAL INFORMATION
    • PRIVACY REQUEST
    • ACCESSIBILITY

Copyright ©2026. All Rights Reserved BNP Media, Inc. and BNP Media II, LLC.

Design, CMS, Hosting & Web Development :: ePublishing