Painting & Coating Industry (PCI) logo Powder coating summit logo
search
cart
facebook twitter linkedin youtube
  • Sign In
  • Create Account
  • Sign Out
  • My Account
Painting & Coating Industry (PCI) logo Powder coating summit logo
  • NEWS
    • Latest News
    • PCI News Now
    • Market Trends & Reports
    • Finishing News
    • Price Alerts
    • Global Top 10/ PCI 25
  • PRODUCTS
    • Product News
    • Featured Products
    • Must See Products and Services
  • MATERIALS
    • Additives
    • Resins/Polymers
    • Pigments
    • Equipment
    • Distributors
  • TECHNOLOGIES
    • Adhesives
    • Architectural Coatings
    • Finishing Articles
    • Finishing Technologies
    • Finishing Equipment
    • Industrial Coatings
    • Nanotechnology
    • Powder Coatings
    • Solventborne
    • Special Purpose Coatings
    • Sustainability
    • UV Coatings
    • Waterborne
  • EVENTS
    • Coatings Trends & Technologies Summit
    • Paint and Coatings Academy
    • Webinars
    • Calendar of Events
    • Lifetime Achievement Award
  • DIRECTORIES
    • Buyer's Guide
    • Equipment Directory
    • Materials Directory
  • RESOURCES
    • Columns
      • Did you know?
      • Distribution Dive
      • Formulating With Mike
      • Innovation Insights
      • Powder Coating Perspectives
      • TiO2 Insider
    • Blogs
      • Editor's Viewpoint
      • Industry Insights
    • Coatings Supplier Handbook
    • COAT-IT! Podcast
    • Videos
    • PCI Store
    • eBooks
    • Sponsor Insights
  • EMAGAZINE
    • eMagazine
    • Archive Issues
    • Editorial Advisory Board
    • CONTACT
    • Advertise
  • SIGN UP!
Home » Low-VOC Paint and Coatings

Articles Tagged with ''Low-VOC Paint and Coatings''

pci1221-Cardolite-1219311003-1170.jpg

Novel CNSL-Based Epoxy Curing Agents for Zero-VOC Floor Coatings and Underwater Cure Applications

Hong Xu Ph.D.
December 8, 2021
No Comments
These epoxy curing agents can achieve zero-VOC floor coatings, excellent adhesion to poorly prepared concrete, good water resistance and fast return-to-service.
Read More
pci0321-Synthomer-815230126-900.jpg

New Binder for Weather- and Surface-Tolerant Wood Trim Paints

M. Secher A. Fream C. Baude N. Martins
March 11, 2021
No Comments
A new binder for water-based wood trim paints is based on a heterogeneous acrylic polymer structure. It combines excellent flexibility and high blocking resistance, while maintaining low VOC content.
Read More
pci0520-MarketReport-1161883713-900.jpg

Demand for Low-VOC Coatings Continues to Rise

Vikash Kumar Annirban Bhattacharya
May 5, 2020
No Comments
The low-VOC coatings market is projected to grow at a CAGR of 6.0% by 2024. Water¬borne, powder and radiation cure technologies are the major low-VOC coating technologies, and are thus gaining in popularity.
Read More
low-voc

How Will Functional Binders for Low-VOC Architectural Coatings Impact the Global Construction Industry?

Pratik Kumar
January 7, 2019
No Comments
Functional binders, when incorporated in low-VOC architectural coatings, offer a wide range of benefits in construction applications in terms of texture as well as durability.
Read More
pci0218-EPS-586694892-900.jpg

The Impact of Film Properties on Corrosion Resistance

in Waterborne Acrylics and Next-Generation Low-VOC Resin Development
Allen S. Bulick Chris R. LeFever Glenn R. Frazee Matt L. Mellott Kailong Jin
February 5, 2018
No Comments

The adhesion/corrosion balance of the previous study yielded significant new insights into resin design. Polymers with good wet adhesion and good corrosion resistance could be isolated, and those properties correlated back to their monomer compositions and particle morphologies.


Read More
pci1117-Vencorex-157396257-900.jpg

How the Design of (Poly)isocyanate Hardeners Can Impact the Properties of Aliphatic Polyurea Coatings

Rolf Klucker
November 7, 2017
No Comments

The present study shows that the reactive diluent Tolonate X FLO 100, used in blend with conventional HDI-based polyisocyanates, can bring significant advantages to 2K polyaspartic systems.


Read More
pci0917-Emerald-504067478-900.jpg

Blend Optimization of Low-VOC Benzoate Coalescents

for Increased Hardness of Waterborne Coatings
Stephen F. Foster William Arendt Brad Farrell Emily McBride Deirdre Newton
September 1, 2017
No Comments

Architectural low-VOC coatings can be formulated with dibenzoate glycol esters to have increased hardness, block resistance, gloss and scrub resistance.


Read More
Quantification of Surface Tack

Quantification of Surface Tack

of Next-Generation, High-Gloss, Low-VOC Architectural Binders
Tyler Bell Robert Sandoval Mary-Jane Hibben Mike Wildman Alexis Kipping
February 1, 2017
No Comments

This study utilized multiple hardness and tack testing procedures in order to fully understand the hardness profile of architectural paints.


Read More
Environmentally Friendly Coatings: Historical Perspectives and Future Outlook

Environmentally Friendly Coatings: Historical Perspectives and Future Outlook

Kurt G. Olson
September 1, 2016
No Comments

In order to affect true change, we must develop products that touch on several of the change drivers, including regulatory issues, total cost of painting and performance


Read More
In an Ideal World, Every Coating is Green

In an Ideal World, Every Coating is Green

Jeff Alexander
September 1, 2016
No Comments

It is imperative for coatings manufacturers to set an example for the entire industry and produce more sustainable products and technologies that address the many problems facing our earth.


Read More
Previous 1 2 3 4 5 6 7 8 9 Next
Manage My Account
  • eMagazine
  • Newsletters
  • Online Registration
  • Subscription Customer Service

More Videos

Popular Stories

AkzoNobel, Nippon

AkzoNobel to Sell Southeast Asia Decorative Paints Business to Nippon Paint for $1.35 Billion

industry news

Dozens Treated After Toledo Chemical Release

Lincoln Memorial Pool Coating

Inspection Report Finds at Least 85 Reflecting Pool Liner Failure Locations

Events

November 5, 2026

Advancing Polyester Powder Coatings: Breakthroughs in Flexibility and Low-Cure Performance

Join us to learn how to improve coating durability while keeping your manufacturing process efficient. Explore the latest advancements in polyester powder coating technology.

November 12, 2026

Premium Leveling, Broad Compatibility: A Cost-Effective Flow and Leveling Additive

This new workhorse additive is recommended in all types of coatings. This highly compatible, 100% active siloxane product prevents defects and maintains good defoamer synergy.

View All Submit An Event
PCI news now promo ad

Keep the info flowing with our eNewsletters!

Get the latest industry updates tailored your way.

JOIN TODAY!
  • RESOURCES
    • Advertise
    • Contact Us
    • Directories
    • Store
    • Want More
    • Manufacturing Division
  • SIGN UP TODAY
    • Create Account
    • eMagazine
    • Newsletters
    • Customer Service
    • Manage Preferences
  • SERVICES
    • Marketing Services
    • Reprints
    • Market Research
    • List Rental
    • Survey & Sample
  • STAY CONNECTED
    • LinkedIn
    • Facebook
    • Youtube
    • X (Twitter)
  • PRIVACY
    • PRIVACY POLICY
    • TERMS & CONDITIONS
    • DO NOT SELL MY PERSONAL INFORMATION
    • PRIVACY REQUEST
    • ACCESSIBILITY

Copyright ©2026. All Rights Reserved BNP Media, Inc. and BNP Media II, LLC.

Design, CMS, Hosting & Web Development :: ePublishing