Painting & Coating Industry (PCI) logo Powder coating summit logo
search
cart
facebook twitter linkedin youtube
  • Sign In
  • Create Account
  • Sign Out
  • My Account
Painting & Coating Industry (PCI) logo Powder coating summit logo
  • NEWS
    • Latest News
    • Market Trends & Reports
    • Finishing News
    • Price Alerts
    • Global Top 10/ PCI 25
  • PRODUCTS
    • Product News
    • Featured Products
    • Must See Products and Services
  • MATERIALS
    • Additives
    • Resins/Polymers
    • Pigments
    • Equipment
    • Distributors
  • TECHNOLOGIES
    • Adhesives
    • Architectural Coatings
    • Finishing Articles
    • Finishing Technologies
    • Finishing Equipment
    • Industrial Coatings
    • Nanotechnology
    • Powder Coatings
    • Solventborne
    • Special Purpose Coatings
    • Sustainability
    • UV Coatings
    • Waterborne
  • EVENTS
    • Coatings Trends & Technologies Summit
    • Paint and Coatings Academy
    • Webinars
    • Calendar of Events
    • Lifetime Achievement Award
  • DIRECTORIES
    • Buyer's Guide
    • Equipment Directory
    • Materials Directory
  • RESOURCES
    • Columns
      • Did you know?
      • Distribution Dive
      • Formulating With Mike
      • Innovation Insights
      • Powder Coating Perspectives
      • TiO2 Insider
    • Blogs
      • Editor's Viewpoint
      • Industry Insights
    • Coatings Supplier Handbook
    • COAT-IT! Podcast
    • Videos
    • PCI Store
    • eBooks
    • Sponsor Insights
  • EMAGAZINE
    • eMagazine
    • Archive Issues
    • Editorial Advisory Board
    • CONTACT
    • Advertise
  • SIGN UP!
Home » electric vehicles

Articles Tagged with ''electric vehicles''

Big-Innovation-light-bulb-no-laser-p-1080.jpg

Axalta Wins 2025 BIG Innovation Award

January 28, 2025
One Comment

The company announced that its been recognized for its role in enhancing the reliability and efficiency of electric vehicles.


Read More
P326_Koch_International_Osnabrueck_E-LKW.jpg

BASF and Koch Go Electric for Long-Haul Transport

January 9, 2025
2 Comments

BASF Coatings and Koch International are transitioning to electric trucks, cutting CO2 emissions and costs as part of their sustainability strategy.



Read More
1-InnovationInsights.png

Electric Avenue: The Changing Landscape of Mobility

Victoria Scarborough Ph.D.
December 10, 2024
3 Comments

Electric vehicles are transforming transportation, creating new demands for coatings that enhance durability, safety, energy efficiency and sustainability in an evolving regulatory landscape.


Read More
akzonobel ev battery.png

AkzoNobel Launches One-Spray Powder Coating for EV Battery Insulation

July 30, 2024
No Comments

AkzoNobel introduced a Resicoat powder coating for EV battery parts that delivers high dielectric strength in a single spray application.


Read More
Electric vehicle car illustration

Anti-Corrosion Finishes for EV-Fastener Applications

Dr. Björn Dingwerth
April 5, 2024
No Comments

Automotive fasteners are tasked with preventing the connected components from becoming dislodged, while also facilitating easy disassembly for servicing or repairs. Nothing poses a greater threat to their efficacy than the accumulation of rust on their surface. Zinc-nickel surface finishing offers a solution that makes minimal contributions to the carbon footprint, thus firmly advancing us along the road to a carbon-emission-free future.


Read More
BASF and Stena Recycling Partner in Recycling of Electric Vehicle Batteries.jpg

BASF and Stena Recycling Partner in Electric Vehicle Batteries

January 11, 2024
No Comments

The focus of the co-operation will be on developing improved black mass production processes to achieve high recovery rates for metals such as lithium, nickel, and cobalt to support closed loop solutions for the European electric vehicle battery market. 



Read More
PCI1223-ChemQuest-1170.jpg

Global Trends Represent Growth and Innovation Opportunities for the Coatings Industry

Victoria Scarborough Ph.D.
December 12, 2023
4 Comments

Commercialization of 3D printing, the increase in popularity of electric vehicles (EVs), and climate change-related challenges are highlighted as three major global trends affecting coatings industry growth and leading innovation efforts.


Read More
Previous 1 2 Next
Manage My Account
  • eMagazine
  • Newsletters
  • Online Registration
  • Subscription Customer Service

More Videos

Popular Stories

Evonik Logo

Evonik to Close Two German Sites

Mergers-and-Company-Strategies.jpg

BASF Confirms Exploratory Talks on Potential Evonik Takeover

Breaking News

Evonik Rejected €10.3 Billion BASF Offer, Reuters Reports

Webinar custom content box

Events

October 8, 2026

AI-Powered Reformulation: Finding PFAS-Free, Lower-VOC Formulations Faster

In this webinar, we will use case studies from industry to illustrate how AI can be used to identify PFAS-free formulations and select surfactant blends for water-based products.

January 1, 2030

Webinar Sponsorship Information

For webinar sponsorship information, visit www.bnpevents.com/webinars or email webinars@bnpmedia.com.

View All Submit An Event

Products

Advanced Coating Materials

Advanced Coating Materials

See More Products
Webinar custom content box

Keep the info flowing with our eNewsletters!

Get the latest industry updates tailored your way.

JOIN TODAY!
  • RESOURCES
    • Advertise
    • Contact Us
    • Directories
    • Store
    • Want More
    • Manufacturing Division
  • SIGN UP TODAY
    • Create Account
    • eMagazine
    • Newsletters
    • Customer Service
    • Manage Preferences
  • SERVICES
    • Marketing Services
    • Reprints
    • Market Research
    • List Rental
    • Survey & Sample
  • STAY CONNECTED
    • LinkedIn
    • Facebook
    • Youtube
    • X (Twitter)
  • PRIVACY
    • PRIVACY POLICY
    • TERMS & CONDITIONS
    • DO NOT SELL MY PERSONAL INFORMATION
    • PRIVACY REQUEST
    • ACCESSIBILITY

Copyright ©2026. All Rights Reserved BNP Media, Inc. and BNP Media II, LLC.

Design, CMS, Hosting & Web Development :: ePublishing