Painting & Coating Industry (PCI) logo Powder coating summit logo
search
cart
facebook twitter linkedin youtube
  • Sign In
  • Create Account
  • Sign Out
  • My Account
Painting & Coating Industry (PCI) logo Powder coating summit logo
  • NEWS
    • Latest News
    • PCI News Now
    • Market Trends & Reports
    • Finishing News
    • Price Alerts
    • Global Top 10/ PCI 25
  • PRODUCTS
    • Product News
    • Featured Products
    • Must See Products and Services
  • MATERIALS
    • Additives
    • Resins/Polymers
    • Pigments
    • Equipment
    • Distributors
  • TECHNOLOGIES
    • Adhesives
    • Architectural Coatings
    • Finishing Articles
    • Finishing Technologies
    • Finishing Equipment
    • Industrial Coatings
    • Nanotechnology
    • Powder Coatings
    • Solventborne
    • Special Purpose Coatings
    • Sustainability
    • UV Coatings
    • Waterborne
  • EVENTS
    • Coatings Trends & Technologies Summit
    • Paint and Coatings Academy
    • Webinars
    • Calendar of Events
    • Lifetime Achievement Award
  • DIRECTORIES
    • Buyer's Guide
    • Equipment Directory
    • Materials Directory
  • RESOURCES
    • Columns
      • Did you know?
      • Distribution Dive
      • Formulating With Mike
      • Innovation Insights
      • Powder Coating Perspectives
      • TiO2 Insider
    • Blogs
      • Editor's Viewpoint
      • Industry Insights
    • Coatings Supplier Handbook
    • COAT-IT! Podcast
    • Videos
    • PCI Store
    • eBooks
    • Sponsor Insights
  • EMAGAZINE
    • eMagazine
    • Archive Issues
    • Editorial Advisory Board
    • CONTACT
    • Advertise
  • SIGN UP!
Home » Topics » Paint and Coating Resins & Polymers

Paint and Coating Resins & Polymers
Paint and Coating Resins & Polymers RSS Feed RSS

Novel Path to Hydroxyl-Functional Emulsions

Novel Path to Hydroxyl-Functional Emulsions

for High-Performance Waterborne Two-Component Polyurethane Coatings
Marcelo Herszenhaut Steven Mao Scott Wang David Vanaken
July 6, 2021
No Comments
OH-functional acrylic emulsions can be designed with a wide range of hydroxyl values and performance characteristics to address the needs of many different applications in plastic, wood, automotive, and construction coatings.
Read More
High-Performance Coatings Protect Office Center

High-Performance Coatings Protect Office Center

From 20+ Years of Future Weathering Damage
APV Engineered Coatings
May 13, 2021
No Comments
This restoration coating is helping a building resist exterior fading and degradation for at least 20 years.
Read More
High Solids Epoxy: A Solution to the EPA’s VOC Regulations

High Solids Epoxy: A Solution to the EPA’s VOC Regulations

Tommy O’Shaughnessy
April 18, 2021
No Comments
This article discusses what VOCs are, where they come from, and why high-solids coatings are so good at reducing VOC emissions.
Read More
datacolor

Getting it Right: Formulating Color Efficiently and Sustainably

Jason Loehr
April 12, 2021
One Comment
Managing color can be challenging, but with a comprehensive digital color management system in place, it is possible to achieve accurate color quickly, sustainably and cost efficiently.
Read More
pci0421-Aditya-889570808-900.jpg

Water-Based Epoxy Technologies for Metal Coating Applications

Dr. Daniel Suckley
April 5, 2021
No Comments
Water-based epoxy resin and curing agents have been developed that can used together as a system to provide corrosion protection coatings with low VOC content, less than 100 grams per liter.
Read More
pci0321-Synthomer-815230126-900.jpg

New Binder for Weather- and Surface-Tolerant Wood Trim Paints

M. Secher A. Fream C. Baude N. Martins
March 11, 2021
No Comments
A new binder for water-based wood trim paints is based on a heterogeneous acrylic polymer structure. It combines excellent flexibility and high blocking resistance, while maintaining low VOC content.
Read More
pci0321-Roquette-469538141-900.jpg

Isosorbide: A Sustainable, Safe, High-Performance Plant-Based Feedstock for Coatings

Jiae Kim
March 10, 2021
No Comments
Perfectly safe and produced from an annually renewable feedstock, isosorbide has a unique combination of properties that offers excellent potential for a range of CASE applications.
Read More
pci0321-Nagase-LeadPhoto-900.jpg

1,5-Pentanediol Diacrylate: A Bio-Based Alternative for UV-Curable Coatings and Inks

Mike Idacavage Dr. Kevin Barnett
March 9, 2021
No Comments
A multi-step continuous process has been developed to convert renewably sourced furfural to 1,5-Pentanediol (1,5-PDO), which is a low-cost renewable replacement for 1,6-HDO, a diol intermediate currently used to produce coatings, adhesives and plastics.
Read More
pci0221-Kumar-603903118-900.jpg

Eco-Friendly Hyperbranched Polyaspartic Polyol and Polyurethane-Urea-Polyurea Hybrid Coatings

for Corrosion Mitigation and Functional Applications
Rajnish Kumar Ramanuj Narayan KVSN Raju
February 11, 2021
No Comments
Development of eco-friendly, sustainable and high-solid (low-VOC) coatings have received a lot of attention due to environmental concerns and legislative issues.
Read More
Where the Acid Copolymer Is Located in the Latex Particle?

Where the Acid Copolymer Is Located in the Latex Particle?

Emulsion Polymers Consulting and Education (EPCEd)
February 2, 2021
One Comment
Although often not appreciated, it is important to recognize is that how you conduct your process has a profound impact on where the acid groups reside and therefore on your final product properties.
Read More
Previous 1 2 … 17 18 19 20 21 22 23 24 25 … 48 49 Next
Manage My Account
  • eMagazine
  • Newsletters
  • Online Registration
  • Subscription Customer Service

More Videos

Popular Stories

Sherwin-Williams

Sherwin-Williams Opens Largest North American Plant

AkzoNobel, Nippon

AkzoNobel to Sell Southeast Asia Decorative Paints Business to Nippon Paint for $1.35 Billion

Mergers-and-Company-Strategies.jpg

BASF Confirms Exploratory Talks on Potential Evonik Takeover

Events

November 5, 2026

Advancing Polyester Powder Coatings: Breakthroughs in Flexibility and Low-Cure Performance

Join us to learn how to improve coating durability while keeping your manufacturing process efficient. Explore the latest advancements in polyester powder coating technology.

November 12, 2026

Premium Leveling, Broad Compatibility: A Cost-Effective Flow and Leveling Additive

This new workhorse additive is recommended in all types of coatings. This highly compatible, 100% active siloxane product prevents defects and maintains good defoamer synergy.

View All Submit An Event
PCI news now promo ad

Keep the info flowing with our eNewsletters!

Get the latest industry updates tailored your way.

JOIN TODAY!
  • RESOURCES
    • Advertise
    • Contact Us
    • Directories
    • Store
    • Want More
    • Manufacturing Division
  • SIGN UP TODAY
    • Create Account
    • eMagazine
    • Newsletters
    • Customer Service
    • Manage Preferences
  • SERVICES
    • Marketing Services
    • Reprints
    • Market Research
    • List Rental
    • Survey & Sample
  • STAY CONNECTED
    • LinkedIn
    • Facebook
    • Youtube
    • X (Twitter)
  • PRIVACY
    • PRIVACY POLICY
    • TERMS & CONDITIONS
    • DO NOT SELL MY PERSONAL INFORMATION
    • PRIVACY REQUEST
    • ACCESSIBILITY

Copyright ©2026. All Rights Reserved BNP Media, Inc. and BNP Media II, LLC.

Design, CMS, Hosting & Web Development :: ePublishing