This article reports on new UV-curable MA oligomers, present their properties as viscous liquids and their outstanding properties as cured MAs (thin films).
A new inorganic black pigment has been developed combining jetness and a neutral colour shade in reductions with an extraordinary IR-reflecting ability bridging the gap between existing products.