Painting & Coating Industry (PCI) logo Powder coating summit logo
search
cart
facebook twitter linkedin youtube
  • Sign In
  • Create Account
  • Sign Out
  • My Account
Painting & Coating Industry (PCI) logo Powder coating summit logo
  • NEWS
    • Latest News
    • PCI News Now
    • Market Trends & Reports
    • Finishing News
    • Price Alerts
    • Global Top 10/ PCI 25
  • PRODUCTS
    • Product News
    • Featured Products
    • Must See Products and Services
  • MATERIALS
    • Additives
    • Resins/Polymers
    • Pigments
    • Equipment
    • Distributors
  • TECHNOLOGIES
    • Adhesives
    • Architectural Coatings
    • Finishing Articles
    • Finishing Technologies
    • Finishing Equipment
    • Industrial Coatings
    • Nanotechnology
    • Powder Coatings
    • Solventborne
    • Special Purpose Coatings
    • Sustainability
    • UV Coatings
    • Waterborne
  • EVENTS
    • Coatings Trends & Technologies Summit
    • Paint and Coatings Academy
    • Webinars
    • Calendar of Events
    • Lifetime Achievement Award
  • DIRECTORIES
    • Buyer's Guide
    • Equipment Directory
    • Materials Directory
  • RESOURCES
    • Columns
      • Did you know?
      • Distribution Dive
      • Formulating With Mike
      • Innovation Insights
      • Powder Coating Perspectives
      • TiO2 Insider
    • Blogs
      • Editor's Viewpoint
      • Industry Insights
    • Coatings Supplier Handbook
    • COAT-IT! Podcast
    • Videos
    • PCI Store
    • eBooks
    • Sponsor Insights
  • EMAGAZINE
    • eMagazine
    • Archive Issues
    • Editorial Advisory Board
    • CONTACT
    • Advertise
  • JOIN!
Home » Topics » Industrial Coatings

Industrial Coatings
Industrial Coatings RSS Feed RSS

eoncoat

Excelling in Today’s Challenging Global Steel Marketplace

October 1, 2018
No Comments
How one steel manufacturer is addressing market obstacles and protecting its vital steel production assets from corrosion.
Read More
Coatings and New Treatments

Coatings and New Treatments Extend The Life of Plastic Injection Molds

Jeff Elliot
August 10, 2018
No Comments
Injection molders are turning to a variety of coatings to protect their investment and reduce maintenance and running costs. These coatings, applied to mold cavities as well as moving, sliding components within the mold, come in a variety of styles from carbonbased coatings, PVD and PACVD deposition to nitriding techniques that share one overriding goal: hardening the surface of the steel to protect it against all manner of abuse.
Read More
pci0818-EIG-483786639-lead-900.jpg

Chrome Plating and PVD Coating with Aluminum Target on Polymeric Substrate

in the Automotive and Home Appliance Industries
Emad Behdad Mohammad Janatian Javad Saheban Mohsen Darzi
August 7, 2018
No Comments
In this article special emphasis is given to PVD technology and its application for polymeric materials in the automotive and home appliance industries, highlighting cost reduction and improved quality around surface modification of parts.
Read More
Metal Design and Sleek Coatings Provide Air-Like Aesthetic for Renovated Boeing Facility

Metal Design and Sleek Coatings Provide Air-Like Aesthetic for Renovated Boeing Facility

August 1, 2018
No Comments
In an effort to streamline the production process and increase delivery time, plans were made to renovate the Charleston Boeing Delivery Center into a state-of-the-art aircraft paint facility in 2014.
Read More
sherwin williams

Transportation Center Presents Paragon of Sustainability

July 1, 2018
No Comments
Well known for its high-performance qualities and durability, including superior resistance to ultraviolet rays and exceptional dirt and stain resistance, Sherwin-Williams Coil Coating's Fluropon offers many valuable features.
Read More
pci0518-SinClair-671415012-900.jpg

Dissecting Orange Peel – A Process-Oriented Approach, Part II

Michael Bonner
June 1, 2018
No Comments

In this two-part series, we explore how this carefully crafted design of experiments (DOE) isolated and contrasted the impact and interaction of three key process variables: film build; atomization, and coating viscosity (as determined by temperature).


Read More
pci0518-Specialty-902258368-900.jpg

Metal Adhesion and Corrosion Resistance of Coatings

Greg Monaghan Nerissa Swaim Ben Estill Victoria Winston
May 8, 2018
No Comments

The improved adhesion, good corrosion resistance and good QUV gloss retention show that the hydrophobic resin in the hybrid polymer can be used to reduce the effects of high acid on corrosion and of styrene on QUV gloss retention.


Read More
pci0518-Cortec-178928369-900.jpg

Impact of Traditional vs New Biobased Rust-Preventive Temporary Coatings

Boris A. Miksic Ivana Radic Ivan Stojanović Eric Uutala
May 7, 2018
No Comments

Following the results from this study, biobased preventative is an excellent and environmentally acceptable alternative to petroleum-based products in temporary corrosion protection.


Read More
pci0418-Tosoh-538488098-900.jpg

Development of a Chemical-Resistant, Two-Component Polyurethane Coating System

Characterized by a Polycarbonate-Based Polyurethane Polyol
Kenji Horiguchi Takaki Jono Teppei Saito
April 11, 2018
One Comment

In this research, newly designed multifunctional polyol systems based on a polycarbonate structure and advanced polyisocyanate systems as crosslinkers were investigated in order to improve chemical resistance of coatings.


Read More
pci0418-Orion-908021140-900.jpg

Deep Black Coatings without Milling

Kai Krauss Carlos Hernandez Jennifer Kauffman
April 2, 2018
No Comments

To overcome the drawbacks of powdered carbon blacks, Orion Engineered Carbons is developing carbon black-based pigment preparations that facilitate, and in many cases eliminate, the dispersion step.


Read More
Previous 1 2 … 65 66 67 68 69 70 71 72 73 … 98 99 Next
Manage My Account
  • Join PCI
  • Subscription Customer Service

More Videos

Popular Stories

industry news

Dozens Treated After Toledo Chemical Release

AkzoNobel, Nippon

AkzoNobel to Sell Southeast Asia Decorative Paints Business to Nippon Paint for $1.35 Billion

Mergers and aquisitions

Evonik Declines BASF Negotiations

Events

November 5, 2026

Advancing Polyester Powder Coatings: Breakthroughs in Flexibility and Low-Cure Performance

Join us to learn how to improve coating durability while keeping your manufacturing process efficient. Explore the latest advancements in polyester powder coating technology.

November 12, 2026

Premium Leveling, Broad Compatibility: A Cost-Effective Flow and Leveling Additive

This new workhorse additive is recommended in all types of coatings. This highly compatible, 100% active siloxane product prevents defects and maintains good defoamer synergy.

View All Submit An Event
PCI news now promo ad

Keep the info flowing with our eNewsletters!

Get the latest industry updates tailored your way.

JOIN TODAY!
  • RESOURCES
    • Advertise
    • Contact Us
    • Directories
    • Store
    • Manufacturing Division
  • JOIN TODAY
    • Create Account
    • eMagazine
    • Newsletters
    • Customer Service
    • Manage Preferences
  • SERVICES
    • Marketing Services
    • Reprints
    • Market Research
    • List Rental
    • Survey & Sample
  • STAY CONNECTED
    • LinkedIn
    • Facebook
    • Youtube
    • X (Twitter)
  • PRIVACY
    • PRIVACY POLICY
    • TERMS & CONDITIONS
    • DO NOT SELL MY PERSONAL INFORMATION
    • PRIVACY REQUEST
    • ACCESSIBILITY

Copyright ©2026. All Rights Reserved BNP Media, Inc. and BNP Media II, LLC.

Design, CMS, Hosting & Web Development :: ePublishing